Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 225 - 245 °C | 437 - 473 °F | Tubular (Blown) Film |
Honeywell Aegis™ HCA95YP Nylon 6/6,6 Extrusion Grade Copolymer
(discontinued **) Description: Aegis HCA95YP is a lubricated medium viscosity, nylon 6/6,6 film extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.. |
|||
Middle Barrel Temperature | 225 - 245 °C | 437 - 473 °F | Tubular (Blown) Film |
Honeywell Aegis™ HCA115ZP Nylon 6/6,6 Extrusion Grade Copolymer
(discontinued **) Description: Aegis HCA115ZP is a high viscosity, nylon 6/6,6 extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500. It possess.. |
|||
Middle Barrel Temperature | 225 - 245 °C | 437 - 473 °F | Injection Molding |
LG Chemical KEYFLEX BT 1068D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Middle Barrel Temperature | 225 - 245 °C | 437 - 473 °F | Injection Molding |
LG Chemical KEYFLEX BT 3047D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Medium ModulusApplication: Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Middle Barrel Temperature | 230 - 245 °C | 446 - 473 °F | |
LG Chemical LUMAX GP-5106F General Purpose PBT, 10% Polymer Alloy, Weather Resistant, Flame Retardant LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Middle Barrel Temperature | 230 - 245 °C | 446 - 473 °F | Injection Molding |
LG Chemical LUMAX GP5106FI PBT+ABS+GF10%, Flame Retardant Description: Injection Molding Grade, PBT+ABS+GF10%, Flame Retardant, Impact Modified, Dimensional StabilityApplication: E&E (Switch)CAS: 9003-56-9, 68928-70-1, 65997-17-3, 24968-12-5, 9003-54-7 an.. |
|||
Middle Barrel Temperature | 230 - 245 °C | 446 - 473 °F | |
LG Chemical LUMAX GP-5200 General Purpose PBT, 20 % Polymer Alloy LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Middle Barrel Temperature | 230 - 245 °C | 446 - 473 °F | Injection Molding |
LG Chemical LUMAX GP5200B PBT+ABS+GF20% Description: Injection Molding Grade, PBT+ABS+GF20%, General PurposeApplication: E&E (Speaker Frame)CAS: 9003-56-9, 65997-17-3, 24968-12-5 and 9003-54-7Information provided by LG Chemical |
|||
Middle Barrel Temperature | 230 - 245 °C | 446 - 473 °F | |
LG Chemical LUMAX HF-5306F High Flow PBT, 30% Polymer Alloy, Weather Resistant, Flame Retardant LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Middle Barrel Temperature | 230 - 245 °C | 446 - 473 °F | |
LG Chemical LUMAX HR-5306F Heat Resistant PBT, 30% Polymer Alloy, Weather Resistant, Flame Retardant LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Middle Barrel Temperature | 215 - 245 °C | 419 - 473 °F | Injection Molding |
LG Chemical LUMID GP1300AP PA6, Plasticized Feature: Injection Molding, PA6, PlasticizedApplication: Automotive PartsInformation provided by LG Chemical |
|||
Middle Barrel Temperature | 235 - 245 °C | 455 - 473 °F | Injection Molding |
LG Chemical Lupox® GP1000M PBT Description: Injection Molding, PBT, High Flow, High ImpactApplication: Automotive (Connector)CAS No. 155123-66-3 and 24968-12-5Information provided by LG Chemical |
|||
Middle Barrel Temperature | 235 - 245 °C | 455 - 473 °F | Injection Molding |
LG Chemical Lupox® GP1006FD PBT Description: Injection Molding, PBT, Flame Retardant, High ImpactApplication: IT/OA, Automotive (Connector)CAS No. 68928-70-1, 155123-66-3, 24968-12-5 and 1309-64-4Information provided by LG Chemica.. |
|||
Middle Barrel Temperature | 205 - 245 °C | 401 - 473 °F | |
Sumitomo Chemical ESPOLEX® 4832 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Middle Barrel Temperature | 205 - 245 °C | 401 - 473 °F | |
Sumitomo Chemical ESPOLEX® 4855 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Middle Barrel Temperature | 200 - 245 °C | 392 - 473 °F | |
Sumitomo Chemical ESPOLEX® 901 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Middle Barrel Temperature | 200 - 245 °C | 392 - 473 °F | |
Sumitomo Chemical ESPOLEX® 903 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Middle Barrel Temperature | 200 - 245 °C | 392 - 473 °F | |
Sumitomo Chemical ESPOLEX® 907 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Middle Barrel Temperature | 200 - 245 °C | 392 - 473 °F | |
Sumitomo Chemical ESPOLEX® UT412A Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Middle Barrel Temperature | 205 - 245 °C | 401 - 473 °F | |
Sumitomo Chemical ESPOLEX® WT361 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Middle Barrel Temperature | 205 - 245 °C | 401 - 473 °F | |
Sumitomo Chemical ESPOLEX® WT485 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Middle Barrel Temperature | 200 - 245 °C | 392 - 473 °F | |
Sumitomo Chemical ESPOLEX® WT487X Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Middle Barrel Temperature | 200 - 245 °C | 392 - 473 °F | |
Sumitomo Chemical ESPOLEX® WT521 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Middle Barrel Temperature | 175 - 245 °C | 347 - 473 °F | |
Equate EMDA-8920 HDPE Injection Molding Resin EMDA-8920 is a high density copolymer polyethylene resin designed for injection molding applications which require excellent toughness and gloss.Applications: EMDA-8920 is a high density copolymer p.. |
|||
Middle Barrel Temperature | 235 - 245 °C | 455 - 473 °F | |
Beijing Chemical Industry KAIFA® HN201-G20 PA6 Resin 20% glass fiber reinforced, thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Middle Barrel Temperature | 235 - 245 °C | 455 - 473 °F | |
Beijing Chemical Industry KAIFA® HN301-G10 PA6 Resin 10% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Middle Barrel Temperature | 235 - 245 °C | 455 - 473 °F | |
Beijing Chemical Industry KAIFA® HN301-G20 PA6 Resin 20% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Middle Barrel Temperature | 225 - 245 °C | 437 - 473 °F | Cylinder Temperature |
Asia International Enterprise (Hong Kong) 3010F Polybutylene terephthalate Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Middle Barrel Temperature | 225 - 245 °C | 437 - 473 °F | Cylinder Temperature |
Asia International Enterprise (Hong Kong) 3010FW Polybutylene terephthalate Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Middle Barrel Temperature | 225 - 245 °C | 437 - 473 °F | |
Beijing Chemical Industry KAIFA® 301-G0 PBT Resin Flame retardant, folding enduranceInformation provided by Beijing Chemical Industry Research Institute (Group) |