Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT4500-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Automotive componentsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT4900-746UV Thermoplastic Polyolefin, UV Stabilized, CD7 Dark Slate Solid Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products G13P100-559UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (GM WPP 646H) Charcoal Metallic Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products GC10P250-00 10% Glass Fiber Reinforced Polypropylene Copolymer, Non-UV Stabilized, Chemically Coupled, Natural Applications: Component housingsStorage binsBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP514-438 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 167 Ebony Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP514-489 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 101E Lite Oak Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP520-01 12% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Black Applications: Interior trimCenter consolesGlove box binsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP521-00UV 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Natural Applications: Interior trimIP structural componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products T10P250-01 10% Talc Reinforced Polypropylene Copolymer, General Purpose Black Applications: Wire troughFan shroudsElectrical housingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products T12P600-01BG 12% Talc Reinforced Polypropylene Copolymer, General Purpose Black, Blow Molding Grade Applications: Flipper panelClose out panelSeat backsLoad floorInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP522-286 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, ZUCA Medium Graphite Applications: ConsolesClose out panelInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP522-473 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, ZU5A Dark Graphite Applications: ConsolesClose out panelInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-60/10/CC/30/E NATL Polypropylene Homopolymer, 10% FiberGlass and 30% Calcium Carbonate Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-60/15/E Polypropylene Homopolymer, 15% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-60/20 Polypropylene Homopolymer, 20% Glass Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-60/30 Polypropylene Homopolymer, 30% Glass Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-60/30/E Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-60/30/E/HF Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled, improved flow Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-60/30/FR Polypropylene Homopolymer, 30% Glass Fiber Reinforced, Flame Retardant Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-60/40/E/EX Polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled, high viscosity Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® PP-60/CC/40 Polypropylene Homopolymer, 40% Calcium Carbonate Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® PP-60/TC/13 BL8860 Polypropylene Homopolymer, 13% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® PP-61/TC/20/UV Polypropylene Copolymer, 20% Talc, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® PP-68/TC/20 Polypropylene Copolymer, 20% Talc Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-60/15/MI/20 Polypropylene Homopolymer, 35% Glass/mica Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® PP-60/CC/20 Polypropylene Homopolymer, 20% Calcium Carbonate Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 193 - 227 °C | 380 - 440 °F | |
CTC SunPro® SP 200 P 3085 Polypropylene Copolymer SunPro® SP 200 P 3085 is a general purpose, medium flow, polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Certifications: GM.PP... |
|||
Middle Barrel Temperature | 193 - 227 °C | 380 - 440 °F | |
CTC SunPro® SP 200 P 5000 Polypropylene Copolymer SunPro® SP 200 P 5000 is a general purpose, medium flow, polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Certifications: MS DB5.. |
|||
Middle Barrel Temperature | 193 - 227 °C | 380 - 440 °F | |
CTC X-PRO CTC PP2020 Polypropylene Impact Copolymer X-PRO PP 2020 is an impact, polypropylene copolymer. It has automotive and industrial general purpose applications.Data provided by Composite Technologies (CTC). |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-68/30/E/UV Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled, UV Stabilized Information provided by FIBERFIL Engineered Plastics |