Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 190 - 220 °C | 374 - 428 °F | Start Point: 205°C |
Kingfa FW-650 Flame Retardant ABS Features:Weather resistanceSuper high impact resistanceApplications:Injection moldingSwitchSocketInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
LG Chemical AT-553 Transparent ABS, Permanent Antistatic, Natural and Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical KEYFLEX BT GN7142F Ester Type TPE Description: Extrusion Molding, TPC-ET, Halogen Free Flame Retardant, Low ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetInformation provided by LG Chemical |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
LG Chemical KEYFLEX TO-1075A Thermoplastic Olefin for Injection Molding, 75A Hardness KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber .. |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
LG Chemical KEYFLEX TO-1175A Thermoplastic Olefin for Extrusion, 75A Hardness KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber .. |
|||
Middle Barrel Temperature | 180 - 220 °C | 356 - 428 °F | Injection Molding |
LG Chemical KEYFLEX TO1192A Olefin Type TPE Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0, 9010-79-1, 64742-54-7, 1333-86-4 and 9002-88-4Information provided by LG Chemical |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical MP211 ABS, Low Gloss, Metal Plating Feature: Injection Molding, High Flow, Metal PlatingApplication: Decorative Parts (Home Appliance Door Handle Etc)CAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical |
|||
Middle Barrel Temperature | 180 - 220 °C | 356 - 428 °F | Extrusion |
Inno-Comp INNOPOL® CS 1-7120 AP 20% Talc Filled Polypropylene Homopolymer INNOPOL® CS 1-7120 is a 20 % talc-filled polypropylene homopolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 1-7120 is recommended for extrusion of sheet.. |
|||
Middle Barrel Temperature | 180 - 220 °C | 356 - 428 °F | Extrusion |
Inno-Comp INNOPOL® CS 2-7120 20% Talc Filled Polypropylene Copolymer INNOPOL® CS 2-7120 is a 20 % talc-filled polypropylene block-copolymer compound /PP-B TD20 (ISO 1043)/. This grade is available in natural and custom colored form.INNOPOL® CS 2-7120 is recomme.. |
|||
Middle Barrel Temperature | 180 - 220 °C | 356 - 428 °F | Extrusion |
Inno-Comp INNOPOL® CS 3-8000 FR Flame Retardant Polypropylene Blend INNOPOL® CS 3-8000 FR is a flame retarded polypropylene compound based on a specific blend of polypropylene homo polymer and copolymer. This grade is available in natural and custom colored form... |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
LG Chemical TR-558 Transparent ABS, Humidity Resistance, Natural and Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Middle Barrel Temperature | 190 - 220 °C | 374 - 428 °F | Start Point: 205°C |
Kingfa FRABS V-0 Flame Retardant ABS Features:UL 94 V-0 @ 1.5-3.0mmHigh toughnessFor extrusion moldingApplications:PlateElectric and electronic cabinetPCB boardInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
LG Chemical TR-558AI Transparent ABS, High Stiffness, Ice Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
LG Chemical TR-558NS Transparent ABS, Antistatic, Natural and Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
Samsung Cheil Industries Starex® MP-0160RD Metal Plating Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
Samsung Cheil Industries Starex® SD-0160 Super High Impact Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 170 - 220 °C | 338 - 428 °F | |
Sumitomo Chemical ESPOLEX® 4675 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Middle Barrel Temperature | 170 - 220 °C | 338 - 428 °F | |
Sumitomo Chemical ESPOLEX® WT525 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
Borealis BA202E Polypropylene Block Copolymer for Non-Pressure Pipes BA202E is a high molecular weight, low melt flow rate polypropylene block copolymer with very high impact strength. Applications: BA202E is recommended for non-pressure pipes & fittings, thin-walled.. |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
Borealis BA204E Polypropylene Block Copolymer for Non-Pressure Pipes BA204E is a high molecular weight, low melt flow rate polypropylene block copolymer with very high impact strength. Applications: BA204E is recommended for non-pressure pipes & fittings, thin-walle.. |
|||
Middle Barrel Temperature | 190 - 220 °C | 374 - 428 °F | |
Borealis BB125MO Polypropylene Copolymer BB125MO is a heterophasic copolymer. This grade is a low melt flow rate grade intended for blow molding and sheet extrusion, and features extremely good process ability with improved melt strength a.. |
|||
Middle Barrel Temperature | 190 - 220 °C | 374 - 428 °F | |
Borealis BL1481 High Density Polyethylene BL1481 is a semi high molecular weight polyethylene comprising an extra ordinary ESCR and very good chemical resistance This product is intended for blow molding. This grade is available in granular.. |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | cylinder |
Borealis Borcoat™ MA115E Syntactic Polypropylene for Steel Pipe Coating Borcoat™ MA115E is a highly filled polypropylene compound and is self colored. Applications: Borcoat™ MA115E is recommended as heavy weight coating for special applications used in steel pipe coa.. |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
Arkema Group KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. Low melt shrinkage, graphite powder filled. High stability in harsh thermal, chemical and ultraviolet environments. High toug.. |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
Arkema Group KYNAR® 6000 HD Polyvinylidene Fluoride - Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Middle Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
Arkema Group KYNAR® 9000 HD Polyvinylidene Fluoride - Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Middle Barrel Temperature | 180 - 220 °C | 356 - 428 °F | Injection Molding |
LG Chemical KEYFLEX TO1088AV Olefin Type TPE Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0Information provided by LG Chemical |