Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis BL1481 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Borealis
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis BL1481 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
BL1481 is a semi high molecular weight polyethylene comprising an extra ordinary ESCR and very good chemical resistance This product is intended for blow molding. This grade is available in granular form. Applications: containers from 1 liters up to 30 liters for storage and transport for dangerous goods, and containers intended for transport of dangerous goods according to UN regulations.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.948 g/cc
0.0342 lb/in³
ISO 1183
Environmental Stress Crack Resistance 300 hour
300 hour
Antarox 10%, F50; ASTM D1693-A
Melt Flow 7.0 g/10 min

@Load 21.6 kg,
Temperature 190 °C
7.0 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 62
62
ISO 868
Tensile Strength, Yield 24.0 MPa
3480 psi
50mm/min; ISO 527-2
Elongation at Yield 10 %
10 %
50mm/min; ISO 527-2
Tensile Modulus 1.00 GPa
145 ksi
1mm/min; ISO 527-2
Flexural Modulus 1.05 GPa
152 ksi
1mm/min; ISO 178
Charpy Impact, Notched 2.00 J/cm²

@Temperature -20.0 °C
9.52 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
2.50 J/cm²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 76.0 °C
169 °F
ISO 75-2
Processing Properties Metric English Comments
Middle Barrel Temperature 190 - 220 °C
374 - 428 °F
Die Temperature 180 - 220 °C
356 - 428 °F
Melt Temperature 180 - 220 °C
356 - 428 °F
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved