Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 266 - 282 °C | 510 - 540 °F | |
PlastiComp Complet® LGF30 - PA6 Nylon 6, 30% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 30% long glass fiber reinforcementInformation provided by PlastiComp, Inc.. |
|||
Middle Barrel Temperature | 266 - 282 °C | 510 - 540 °F | |
PlastiComp Complet® LGF40 - PA6 Nylon 6, 40% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 40% long glass fiber reinforcementInformation provided by PlastiComp, Inc.. |
|||
Middle Barrel Temperature | 266 - 282 °C | 510 - 540 °F | |
PlastiComp Complet® LGF60 - PA6 Nylon 6, 60% Long Glass Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 60% long glass reinforcementInformation provided by PlastiComp, Inc. |
|||
Middle Barrel Temperature | 266 - 288 °C | 510 - 550 °F | |
Polymer Resources PC-IM2 Polycarbonate, Impact Modified, Medium Flow Polycarbonate, Impact Modified, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided .. |
|||
Middle Barrel Temperature | 266 - 288 °C | 510 - 550 °F | |
Polymer Resources PC-IM2-UV Polycarbonate, Impact Modified, Medium Flow, UV-stabilized Polycarbonate, Impact Modified, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Middle Barrel Temperature | 266 - 288 °C | 510 - 550 °F | |
Polymer Resources PC-IM3 Polycarbonate, Impact Modified, High Flow Polycarbonate, Impact Modified, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Middle Barrel Temperature | 266 - 288 °C | 510 - 550 °F | |
Polymer Resources PC-IM4 Polycarbonate, Impact Modified, Easy Flow Polycarbonate, Impact Modified, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Middle Barrel Temperature | 266 - 277 °C | 510 - 530 °F | |
Ravago Manufacturing Americas Hylex® P1025G10 HB Polycarbonate, 10% Glass Reinforced Information provided by Ravago. |
|||
Middle Barrel Temperature | 266 - 293 °C | 510 - 560 °F | |
PTS Tristar® PC-05GFR 5% Glass Reinforced Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 266 - 277 °C | 510 - 530 °F | |
PTS Tristar® PC-10FR 12 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 266 - 277 °C | 510 - 530 °F | |
PTS Tristar® PC-10FR-(V) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 266 - 277 °C | 510 - 530 °F | |
PTS Tristar® PC-10FR-(VIM) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 266 - 277 °C | 510 - 530 °F | |
PTS Tristar® PC-10FRN (V) 15 MFI, 5VA, Flame Retardant, UV Stabilized Polycarbonate With Release ROHS Compliant.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 266 - 277 °C | 510 - 530 °F | |
PTS Tristar® PC-10FRNH 12 MFI Non-Bromine Non-Chlorine Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 266 - 277 °C | 510 - 530 °F | |
PTS Tristar® PC-10FRNH-V 12 MFI Non-Bromine Non-Chlorine Flame Retardant UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 266 - 293 °C | 510 - 560 °F | |
LTL Color Compounds ColorFast® NY2GF130 Nylon 66, 13% Glass-Filled 13% glass-filled nylon 6,6All information provided by LTL Color Compounders, Inc. |
|||
Middle Barrel Temperature | 266 - 293 °C | 510 - 560 °F | |
LTL Color Compounds ColorFast® NY2GF131 Nylon 66, 13% Glass-Filled, Impact Modified 13% glass-filled impact modified nylon 6,6All information provided by LTL Color Compounders, Inc. |
|||
Middle Barrel Temperature | 266 - 277 °C | 510 - 530 °F | |
MRC Polymers NAXALOYâ„¢ 770 GF10 ABS+PC Alloy, 10% Glass Fiber Filled Can be UV StabilizedInternal and external lubricant can be addedInformation provided by MRC Polymers Inc. |
|||
Middle Barrel Temperature | 266 - 277 °C | 510 - 530 °F | |
MRC Polymers NAXALOYâ„¢ 770 GF16 ABS+PC Alloy, 16% Glass Fiber Filled Can be UV StabilizedInternal and external lubricant can be addedInformation provided by MRC Polymers Inc. |
|||
Middle Barrel Temperature | 266 - 282 °C | 510 - 540 °F | |
MRC Polymers NAXELLâ„¢ PC110-919 General Purpose Polycarbonate, Medium High MFR Polycarbonate for colorable productsMFR can be modified between 10 to 40 g/10minCan be UV stabilizedInternal and external lubricant can be addedCan be clear to color matchedNot for products that req.. |
|||
Middle Barrel Temperature | 266 - 277 °C | 510 - 530 °F | |
MRC Polymers NAXELLâ„¢ PC210MR General Purpose Polycarbonate, Medium MFR, with Release Medium melt without impact modificationMFR can be modified between 10 to 40 g/10minCan be UV stabilizedInternal and external lubricant can be addedGenerally for black and gray colors onlyFR package .. |
|||
Middle Barrel Temperature | 266 °C | 510 °F | |
MTI ThermoStran® PA66-40C Long Carbon Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Middle Barrel Temperature | 266 °C | 510 °F | |
MTI ThermoStran® PA66-40G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Middle Barrel Temperature | 266 °C | 510 °F | |
MTI ThermoStran® PA66-50G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Middle Barrel Temperature | 266 - 277 °C | 510 - 530 °F | |
Samyang Trirex® PC-3025U 12 MFI UV Stabilized Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 266 - 277 °C | 510 - 530 °F | |
Wellman Wellamid® FR22F-N Flame Retardant Nylon 66, Lubricated Typical Applications: Electrical terminal blocks, electric fan switch housings, coil forms, multi-pin electrical connectors, electric fan switch housings, TV tuner components, automotive switch hous.. |
|||
Middle Barrel Temperature | 266 - 277 °C | 510 - 530 °F | |
Wellman Wellamid® FRGF25-66-N Flame Retardant Nylon 66, Lubricated, 25% Glass Fiber Typical Applications: Electrical terminal blocks, electric fan switch housings, coil forms, multi-pin electrical connectors, electric fan switch housings, TV tuner components, automotive switch hous.. |
|||
Middle Barrel Temperature | 266 - 277 °C | 510 - 530 °F | |
Entec Hylex® P1025G10NHFR Polycarbonate, 10% Glass Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Middle Barrel Temperature | 266 - 299 °C | 510 - 570 °F | |
Polymer Resources PPX/NY GP1 Modified PPO, General Purpose PPX/Nylon 6,6 Alloy
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Middle Barrel Temperature | 266 - 293 °C | 510 - 560 °F | |
LTL Color Compounds ColorFast® NY1GF330 Nylon 6, 33% Glass-Filled 33% glass-filled nylon 6All information provided by LTL Color Compounders, Inc. |