Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-7940/GY/EM Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Zone 3 | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-8032/GY Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Zone 3 | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-8086/YL Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Zone 3 | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-8087/BL Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Zone 3 | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-8088/RD Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Zone 3 | 350 - 370 °C | 662 - 698 °F | |
Lehmann & Voss LUVOCOM® 1500-0871 Polysulfone, with glass spheres Applications: Isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts, high continuous use temperature.Control disks, ca.. |
|||
Zone 3 | 350 - 370 °C | 662 - 698 °F | |
Lehmann & Voss LUVOCOM® 1503-7986 Polysuper sulfone, with glass fiber and PTFE Applications: Automotive industry, office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved friction and w.. |
|||
Zone 3 | 350 - 370 °C | 662 - 698 °F | |
Lehmann & Voss LUVOCOM® 1100-7725 VP Polyether sulfone, with glass fiber, lubricant modified Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Zone 3 | 350 - 370 °C | 662 - 698 °F | |
Lehmann & Voss LUVOCOM® 1100-7939/GY Polyether sulfone, unreinforced Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Zone 3 | 350 - 370 °C | 662 - 698 °F | |
Lehmann & Voss LUVOCOM® 1100-8194 Polyether sulfone, with glass fiber Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Zone 3 | 350 - 370 °C | 662 - 698 °F | |
Lehmann & Voss LUVOCOM® 1100-8301 Polyether sulfone, with carbon fiber, PTFE, lubricant modified Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.Strong, stiff parts.Dy.. |
|||
Zone 3 | 350 - 370 °C | 662 - 698 °F | |
Lehmann & Voss LUVOCOM® 1100-8325 Polyether sulfone, with glass fiber and PTFE Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.Improved friction and .. |
|||
Zone 3 | 350 - 370 °C | 662 - 698 °F | |
Lehmann & Voss LUVOCOM® 1100-8326 Polyether sulfone, with carbon fiber, PTFE, lubricant modified Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.Strong, stiff parts.Dy.. |
|||
Zone 3 | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-7223 Polyether imide, with PTFE Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Zone 3 | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-7227 Polyether imide, with carbon fiber and PTFE Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.Hig.. |
|||
Zone 3 | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-7743 Polyether imide, with PTFE Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Zone 3 | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-8133 Polyether imide, with carbon fiber, easy flowing Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.High dimensionally stable precision parts.Electrical.. |
|||
Zone 3 | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-8154/GY Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Zone 3 | 350 - 370 °C | 662 - 698 °F | |
Lehmann & Voss LUVOCOM® 1100/GF/20/EM/MR Polyether sulfone, with glass fiber, easy flowing, demolding aid Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Zone 3 | 350 - 370 °C | 662 - 698 °F | |
Lehmann & Voss LUVOCOM® 1100/GF/30/NAT Polyether sulfone, with glass fiber Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Zone 3 | 350 - 370 °C | 662 - 698 °F | |
Lehmann & Voss LUVOCOM® 1100-7337/WT Polyether sulfone, unreinforced Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Zone 3 | 350 - 370 °C | 662 - 698 °F | |
Lehmann & Voss LUVOCOM® 1100-7890 Polyether sulfone, with carbon fiber Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Zone 3 | 350 - 370 °C | 662 - 698 °F | |
Lehmann & Voss LUVOCOM® 1100-8049 Polyether sulfone, with glass fiber Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Zone 3 | 350 - 370 °C | 662 - 698 °F | |
Lehmann & Voss LUVOCOM® 1100-8166 Polyether sulfone, with glass fiber, easy flowing Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Zone 3 | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-7940/GY Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |