Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 260 - 270 °C | 500 - 518 °F | hopper |
Nilit Nilamid A H2 FR HF2 Unfilled, Flame Retardant PA66/6 Co-Polymer Description: Nilamid A H2 FR HF2 is an unfilled, flame retardant NYLON 66/6 co-polymer that does not contain halogen or red phosphorous. This product combines excellent flow characteristics and extr.. |
|||
Zone 1 | 240 - 270 °C | 464 - 518 °F | hopper |
Nilit Nilamon B3 H7 GK 35 15% Glass Fiber, 25% Mineral Reinforced PA6 Description: Nilamon B3 H7 GK 35 provides a combination between low warpage and high stiffness, while retaining a good impact strength. It has a high heat aging resistance, so that it is suitable fo.. |
|||
Zone 1 | 240 - 270 °C | 464 - 518 °F | hopper |
Nilit Nilamid B3 H G10 50% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G10 is a product that combines outstanding strength and stiffness with good moldability and good impact strength. It is widely used for structural applications.Key characte.. |
|||
Zone 1 | 240 - 270 °C | 464 - 518 °F | hopper |
Nilit Nilamid B3 H G3 15% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 6. These products combine good overall mechanical performance and impact strength with ease of processing. Key cha.. |
|||
Zone 1 | 250 - 270 °C | 482 - 518 °F | |
Lehmann & Voss LUVOCOM® 3/CF/10/BK Polyamide 6, with carbon fiber Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressElectrically conductive, suitable.. |
|||
Zone 1 | 250 - 270 °C | 482 - 518 °F | |
Lehmann & Voss LUVOCOM® 3/CF/12/EG Polyamide 6, with carbon fiber, high viscosity Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressElectrically conductive, suitable.. |
|||
Zone 1 | 250 - 270 °C | 482 - 518 °F | |
Lehmann & Voss LUVOCOM® 3/CF/30/EG Polyamide 6, with carbon fiber, extrusion grade Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressElectrically conductive, suitable.. |
|||
Zone 1 | 250 - 270 °C | 482 - 518 °F | |
Lehmann & Voss LUVOCOM® 3-7088-1 Polyamide 6, with carbon fiber and glass fiber, low-warpage Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressElectrically conductive, suitable for continuous discharging of staticall.. |
|||
Zone 1 | 250 - 270 °C | 482 - 518 °F | |
Lehmann & Voss LUVOCOM® 3-7088-2 Polyamide 6, with carbon fiber and glass fiber, low-warpage, heat stabilized Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressElectrically conductive, suitable for continuous discharging of staticall.. |
|||
Zone 1 | 250 - 270 °C | 482 - 518 °F | |
Lehmann & Voss LUVOCOM® 3-7234-1 Polyamide 6, with carbon fiber, electrically conducting Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressAntistatic.Handles, levers, rollers, body parts.Information provided by L.. |
|||
Zone 1 | 250 - 270 °C | 482 - 518 °F | |
Lehmann & Voss LUVOCOM® 3-7281/PL/HI/BK Polyamide 6, with PTFE, toughness-modified Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce.. |
|||
Zone 1 | 250 - 270 °C | 482 - 518 °F | |
Lehmann & Voss LUVOCOM® 3-7723/ EG Polyamide 6, with carbon fiber, high viscosity Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressAntistatic.Handles, levers, rolle.. |
|||
Zone 1 | 250 - 270 °C | 482 - 518 °F | |
Lehmann & Voss LUVOCOM® 3-8266/BL Polyamide 6, unreinforced Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce.. |
|||
Zone 1 | 250 - 270 °C | 482 - 518 °F | |
Lehmann & Voss LUVOCOM® 3-8351 Polyamide 6, with carbon fiber Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated el.. |
|||
Zone 1 | 240 - 270 °C | 464 - 518 °F | |
Lehmann & Voss LUVOCOM® 7-0755 Polyamide 610, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.Improved friction and wear behaviou.. |
|||
Zone 1 | 250 - 270 °C | 482 - 518 °F | |
Lehmann & Voss Nylatron® MR 2007 Polyamide 6, with mineral filler Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Low warpage.Isotropic shrinkage characteristics.Information provided by Lehmann & Voss & Co.KG |
|||
Zone 1 | 260 - 270 °C | 500 - 518 °F | |
Eurostar Staramide A28N PA66, Nucleated, Injection Molding Staramide A28K is an Unreinforced and Heat Stabilized, Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 260 - 270 °C | 500 - 518 °F | |
Eurostar Staramide A40 PA66, Extrusion Staramide A40 is Unreinforced, High Viscosity Polyamide 66, Extrusion ResinInformation provided by Eurostar. |
|||
Zone 1 | 260 - 270 °C | 500 - 518 °F | |
Eurostar Starflam A28UL PA66, Flame Retardant, Injection Molding Staramide A28UL is Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 260 - 270 °C | 500 - 518 °F | |
Eurostar Starflam AFR200B PA66, Flame Retardant, Injection Molding Staramide AFR200B is an Unfilled, Flame Retardant Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 260 - 270 °C | 500 - 518 °F | |
Eurostar Starflam AFR450B PA66, 25% Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR450B is a Flame Retardant, 25% Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 260 - 270 °C | 500 - 518 °F | |
Eurostar Starflam AFR682A1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding Starflam AFR682A1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 260 - 270 °C | 500 - 518 °F | |
Eurostar Starflam AFR682B1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding Starflam AFR682B1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 260 - 270 °C | 500 - 518 °F | |
Eurostar Starflam RFK517E PA66, Glass/Mineral Fiber Reinforced, Flame Retardant, Injection Molding Starflam RFK517E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Mineral Filled, Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 260 - 270 °C | 500 - 518 °F | |
Eurostar Staramide R1000HI620 PA66, Impact Modified, Injection Molded Staramide R1000HI620 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as R1000HI010)Information provided by Eurostar. |
|||
Zone 1 | 260 - 270 °C | 500 - 518 °F | |
Eurostar Starflam AFR450B1 PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR450B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |