Polymer Property : Die Temperature = 230 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Die Temperature 200 - 230 °C
392 - 446 °F
Extrusion Molding
LG Chemical AF360S ABS, TBBA-free Flame Retardant, Low Flow
Feature: Injection Molding, TBBA-free Flame Retardant, Low FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information ..
Die Temperature 190 - 230 °C
374 - 446 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1040D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Die Temperature 190 - 230 °C
374 - 446 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1045D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Die Temperature 190 - 230 °C
374 - 446 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1140D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical
Die Temperature 200 - 230 °C
392 - 446 °F
Extrusion Molding
LG Chemical MA210 ABS, Low Gloss
Feature: Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical
Die Temperature 200 - 230 °C
392 - 446 °F
Extrusion Molding
LG Chemical MA221 ABS, High Impact, Low Gloss
Feature: Injection Molding, Extrusion Molding, High Impact, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical
Die Temperature 220 - 230 °C
428 - 446 °F
6
Lubrizol Advanced Materials Pearlthane® ECO D12T55D Thermoplastic Polyurethane
Type: Pearlthane® ECO D12T55D is a high performance bio-based thermoplastic polyurethane. With ca. 29% bio-based content.Main Application : Extrusion/MouldingSpecial Features : Properties similar..
Die Temperature 220 - 230 °C
428 - 446 °F
TIP, 7
Lubrizol Advanced Materials Pearlthane® ECO D12T55D Thermoplastic Polyurethane
Type: Pearlthane® ECO D12T55D is a high performance bio-based thermoplastic polyurethane. With ca. 29% bio-based content.Main Application : Extrusion/MouldingSpecial Features : Properties similar..
Die Temperature 220 - 230 °C
428 - 446 °F
Solvay TECHNYL® C 442 Black V PA6, DRY
Description: Unreinforced polyamide PA6, high viscosity, with high flexibility and very high impact resistance even at low temperature, for extrusion.Available in: Europe Product Applications: It ha..
Die Temperature 210 - 230 °C
410 - 446 °F
Solvay TECHNYL® eXten D 437P PA6.10
Description: TECHNYL® eXten D 437P is a high viscosity, unfilled, plasticized, UV and heat stabilized PA6.10 for extrusion applications. Technyl® eXten D 437P is a partially biosourced materia..
Die Temperature 215 - 230 °C
419 - 446 °F
Solvay TECHNYL® C 536XT PA6, DRY
Description: TECHNYL® C 536XT is an unreinforced polyamide 6, high viscosity, for extrusion blow molding. This product is available in natural color.Benefits: The product offers a good processing..
Die Temperature 200 - 230 °C
392 - 446 °F
Borealis BB412E Polypropylene Block Copolymer for extrusion and injection
BB412E is a natural, medium molecular weight, medium melt flow rate polypropylene block copolymer with an optimal mechanical properties balance resulting in high stiffness and very good impact stren..
Die Temperature 200 - 230 °C
392 - 446 °F
Borealis BE50-7032 Polypropylene Homopolymer for Non-Pressure pipes and extruded sheets
BE50-7032 is a high molecular weight, low melt flow rate polypropylene homopolymer characterized by high stiffness, high heat distortion temperature and high resistance to thermal aging. The materia..
Die Temperature 200 - 230 °C
392 - 446 °F
Borealis BEC5012 Polypropylene Block Copolymer for Non-Pressure Pipes
BEC5012 is a high molecular weight, low flow rate polypropylene block copolymer with very high impact strength. Applications: BEC5012 is recommended for non-pressure pipes and fittings, structured..
Die Temperature 200 - 230 °C
392 - 446 °F
Borealis Beta (ß)-PP™ BE60-7032 Grey Polypropylene Homopolymer for Pressure Pipes, Fittings and Sheets
Beta(ß)-PP BE60-7032 is a high molecular weight, low melt flow rate polypropylene homopolymer with fine grained ß-modification crystalline structure leading to excellent impact strength even at lo..
Die Temperature 200 - 230 °C
392 - 446 °F
Borealis HA104E Polypropylene Homopolymer
HA104E is a natural high molecular weight, high melt flow rate polypropylene homopolymer characterized by well-balanced stiffness to impact strength ratio at increased processing properties. Applica..
Die Temperature 190 - 230 °C
374 - 446 °F
Hotmelt Coating Slot Die
EMS-Griltech Griltex® 6E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Die Temperature 190 - 230 °C
374 - 446 °F
Hotmelt Coating Slot Die
EMS-Griltech Griltex® D 1377E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Die Temperature 190 - 230 °C
374 - 446 °F
Hotmelt Coating Slot Die
EMS-Griltech Griltex® D 1439E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Die Temperature 180 - 230 °C
356 - 446 °F
Arkema Group LOTADER® 3200 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER 3200 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized under high pressure in an autoclave process. Due to its properties, LOTADER 3200 is used in pipeline ..
Die Temperature 200 - 230 °C
392 - 446 °F
Extrusion Molding
LG Chemical MA201 ABS, Low Gloss
Feature: Injection Molding, Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical