Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 75.0 °C @Time 21600 - 57600 sec |
167 °F @Time 6.00 - 16.0 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1-1120 Polyamide 66, with PTFE, lubricant modified, high viscosity Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Drying Temperature | 75.0 °C @Time 21600 - 57600 sec |
167 °F @Time 6.00 - 16.0 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1-7390 Polyamide 66, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Drying Temperature | 75.0 °C @Time 21600 - 57600 sec |
167 °F @Time 6.00 - 16.0 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1-7882 Polyamide 66, with carbon fiber and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Electrically conductive, suita.. |
|||
Drying Temperature | 75.0 °C @Time 21600 - 57600 sec |
167 °F @Time 6.00 - 16.0 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1-8218 Polyamide 66, with carbon fiber, toughness-modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; impact resistance.Reduced moment of inertia compared with metal parts.Elec.. |
|||
Drying Temperature | 75.0 °C @Time 21600 - 57600 sec |
167 °F @Time 6.00 - 16.0 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1-8501 Polyamide 66, with glass fiber, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.dynamic st.. |
|||
Drying Temperature | 75.0 °C @Time 36000 - 57600 sec |
167 °F @Time 10.0 - 16.0 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 3/TF/20/BK Polyamide 6, with PTFE Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce.. |
|||
Drying Temperature | 75.0 °C @Time 36000 - 57600 sec |
167 °F @Time 10.0 - 16.0 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 3-7088-2 Polyamide 6, with carbon fiber and glass fiber, low-warpage, heat stabilized Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressElectrically conductive, suitable for continuous discharging of staticall.. |
|||
Drying Temperature | 75.0 °C @Time 21600 - 36000 sec |
167 °F @Time 6.00 - 10.0 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 6-7834 Polyamide 12, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Dynamic stressed parts.Low waterabsorbtion, for dimensional stable precision parts.Isotropic sh.. |
|||
Drying Temperature | 75.0 °C @Time 21600 - 36000 sec |
167 °F @Time 6.00 - 10.0 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 6-8512 Polyamide 12, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Especially suitable at dynamic.. |
|||
Drying Temperature | 75.0 °C @Time 7200 - 28800 sec |
167 °F @Time 2.00 - 8.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 80/TF/18/SI/2/BK Polyacetal-copolymer, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Drying Temperature | 75.0 °C @Time 7200 - 28800 sec |
167 °F @Time 2.00 - 8.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 80-7580/BK Polyacetal-copolymer, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Drying Temperature | 75.0 °C @Time 7200 - 28800 sec |
167 °F @Time 2.00 - 8.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 80-7653 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Antistatic.No change of electric potential at bearings in case of separation of charge caused b.. |
|||
Drying Temperature | 75.0 °C @Time 7200 - 28800 sec |
167 °F @Time 2.00 - 8.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 80-7655/RD Polyacetal-copolymer, with aramid reinforcement and PTFE, toughness-modified, high viscosity Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Drying Temperature | 75.0 °C @Time 7200 - 28800 sec |
167 °F @Time 2.00 - 8.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 80-7705 Polyacetal-copolymer, with carbon fiber, aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Suitable for discharging of st.. |
|||
Drying Temperature | 75.0 °C @Time 7200 - 28800 sec |
167 °F @Time 2.00 - 8.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 80-7713 Polyacetal-copolymer, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Drying Temperature | 75.0 °C @Time 7200 - 28800 sec |
167 °F @Time 2.00 - 8.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 80-8470 Polyacetal-copolymer, unreinforced Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Isotropic shrinkage characteristics.Strong, stiff parts.Impact resistance.Control disks, cams, .. |
|||
Drying Temperature | 75.0 °C @Time 21600 - 57600 sec |
167 °F @Time 6.00 - 16.0 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1/CF/20 Polyamide 66, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Drying Temperature | 75.0 °C @Time 21600 - 57600 sec |
167 °F @Time 6.00 - 16.0 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1/CF/30/TF/13/SI/2/BK Polyamide 66, with carbon fiber, PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh.. |
|||
Drying Temperature | 75.0 °C @Time 21600 - 57600 sec |
167 °F @Time 6.00 - 16.0 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1-0867 Polyamide 66, with aramid reinforcement and PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage, isotropic shrinka.. |
|||
Drying Temperature | 75.0 °C @Time 21600 - 57600 sec |
167 °F @Time 6.00 - 16.0 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1-0889-2 Polyamide 66, with carbon fiber and glass fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically .. |
|||
Drying Temperature | 75.0 °C @Time 21600 - 57600 sec |
167 °F @Time 6.00 - 16.0 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1-0935 Polyamide 66, with glass fiber and PTFE, 8-mm-granulate Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Drying Temperature | 75.0 °C @Time 21600 - 57600 sec |
167 °F @Time 6.00 - 16.0 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1-0936 Polyamide 66, with glass fiber and PTFE, 8-mm-granulate Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Drying Temperature | 75.0 °C @Time 21600 - 57600 sec |
167 °F @Time 6.00 - 16.0 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® G Polyamide 66, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Isotropic shrinkage characteristics.Control disks, cams, sliding ele.. |
|||
Drying Temperature | 75.0 °C @Time 21600 - 57600 sec |
167 °F @Time 6.00 - 16.0 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® GS-H/2 Polyamide 66, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Isotropic shrinkage characteristics.Control disks, cams, sliding ele.. |
|||
Drying Temperature | 75.0 °C @Time 21600 - 57600 sec |
167 °F @Time 6.00 - 16.0 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® NSB 90 BK Polyamide 66, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Drying Temperature | 75.0 °C @Time 21600 - 57600 sec |
167 °F @Time 6.00 - 16.0 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® PA66/TF/40 Polyamide 66, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Drying Temperature | 75.0 °C @Time 21600 - 57600 sec |
167 °F @Time 6.00 - 16.0 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1-0890 Polyamide 66, with carbon fiber, low-warpage, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Stiff parts, low coefficient of expansion, low viscose, anisotropic.Reduced moment of inertia c.. |
|||
Drying Temperature | 75.0 °C @Time 21600 - 57600 sec |
167 °F @Time 6.00 - 16.0 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1-7233-1 Polyamide 66, with glass fiber, PTFE, lubricant modified, silicone-free Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Bearings, .. |