Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 60.0 - 70.0 MPa | 8700 - 10200 psi | |
Plastcom PLASTALEN® EH 91 N Polyethylene HDPE regrind for injection molding. General use in all industry branches. Delivered in blue ( approx. RAL 5015) mode.Information Provided by Plastcom spol. s r.o. |
|||
Injection Pressure | 60.0 - 70.0 MPa | 8700 - 10200 psi | |
Plastcom PLASTALEN® PH 91 SD Polypropylene Modified homopolymer PP for injection molding. General use in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Plastcom spol. s r.o. |
|||
Injection Pressure | 60.0 - 70.0 MPa | 8700 - 10200 psi | |
Plastcom PLASTALEN® PQ 81 N 003 Polypropylene with improved impact strength PP copolymer regranulate for injection molding, impact modified. General use in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Plastcom spol.. |
|||
Injection Pressure | 60.0 - 70.0 MPa | 8700 - 10200 psi | |
Plastcom SLOVALEN PH 51 N PP, basic type FeaturesModified homopolymer PP for injection moulding. General use in all industry branches - packing material, garden flowerpots, toys, furniture industry, hinges, fasteners, clamps, office chairs.. |
|||
Injection Pressure | 40.0 - 70.0 MPa | 5800 - 10200 psi | |
Polykemi AB POLYfill PP CIP1001F Polypropylene Information provided by Polykemi AB |
|||
Injection Pressure | 40.0 - 70.0 MPa | 5800 - 10200 psi | |
Polykemi AB POLYfill PP CIP15015 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Injection Pressure | 40.0 - 70.0 MPa | 5800 - 10200 psi | |
Polykemi AB POLYfill PP CIP15015 UV Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Injection Pressure | 40.0 - 70.0 MPa | 5800 - 10200 psi | |
Polykemi AB POLYfill PP CIP16020FCS Polypropylene, Fast Cycle Information provided by Polykemi AB |
|||
Injection Pressure | 40.0 - 70.0 MPa | 5800 - 10200 psi | |
Polykemi AB POLYfill PP CIP6020F Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Injection Pressure | 40.0 - 70.0 MPa | 5800 - 10200 psi | |
Polykemi AB POLYfill PP CMX8030 VT Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Injection Pressure | 40.0 - 70.0 MPa | 5800 - 10200 psi | |
Polykemi AB POLYfill PP CPX10030 UV Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Injection Pressure | 40.0 - 70.0 MPa | 5800 - 10200 psi | |
Polykemi AB POLYfill PP CQX10030 RT Polypropylene, Mineral Reinforced, Scratch Resistant Information provided by Polykemi AB |
|||
Injection Pressure | 40.0 - 70.0 MPa | 5800 - 10200 psi | |
Polykemi AB POLYfill PP CQX10030E10 F Polypropylene, Mineral Reinforced, Elastomer Modified Information provided by Polykemi AB |
|||
Injection Pressure | 40.0 - 70.0 MPa | 5800 - 10200 psi | |
Polykemi AB POLYfill PP CQX10030E10 Polypropylene, Mineral Reinforced, Elastomer Modified Information provided by Polykemi AB |
|||
Injection Pressure | 50.0 - 70.0 MPa | 7250 - 10200 psi | |
Polykemi AB POLYfill PP CQX15015 R3 UV Polypropylene, Mineral Reinforced, Scratch Resistant Information provided by Polykemi AB |
|||
Injection Pressure | 40.0 - 70.0 MPa | 5800 - 10200 psi | |
Polykemi AB POLYfill PP CQX30030 RTX Polypropylene, Mineral Reinforced, Scratch Resistant Information provided by Polykemi AB |
|||
Injection Pressure | 40.0 - 70.0 MPa | 5800 - 10200 psi | |
Polykemi AB POLYfill PP CQX8025 R2 Polypropylene, Mineral Reinforced, Scratch Resistant Information provided by Polykemi AB |
|||
Injection Pressure | 40.0 - 70.0 MPa | 5800 - 10200 psi | |
Polykemi AB POLYfill PPC T4020 E20 Polypropylene Copolymer, Mineral Reinforced, Modified Information provided by Polykemi AB |
|||
Injection Pressure | 40.0 - 70.0 MPa | 5800 - 10200 psi | |
Polykemi AB POLYfill PPC TS6020 E20 Polypropylene Copolymer, Mineral Reinforced, Elastomer Modified Information provided by Polykemi AB |
|||
Injection Pressure | 60.0 - 70.0 MPa | 8700 - 10200 psi | |
Plastcom SLOVALEN PC 53 N Polypropylene Copolymer, UV Stabilization FeaturesModified copolymer PP for injection moulding, with the ability of modeling the melt flow rate within the interval 5 - 20 g/10 min. Can be used for simple small as well as for large complica.. |
|||
Injection Pressure | 60.0 - 70.0 MPa | 8700 - 10200 psi | |
Plastcom SLOVALEN PQ 91 N Polypropylene Homopolymer, Modified with Elastomer, Impacted FeaturesHomopolymer PP modified with elastomer. The addition of thermoplastic elastomer causes increased toughness, possible alternative to PP copolymers. General application in all industry branc.. |
|||
Injection Pressure | 40.0 - 70.0 MPa | 5800 - 10200 psi | |
Polykemi AB POLYfill PP CIP6015F VTUV Polypropylene, Mineral Reinforced, Heat and UV Stabilized Information provided by Polykemi AB |
|||
Injection Pressure | 40.0 - 70.0 MPa | 5800 - 10200 psi | |
Polykemi AB POLYfill PPC 200 E20 Polypropylene Copolymer, Elastomer Modified Information provided by Polykemi AB |
|||
Injection Pressure | 30.0 - 70.0 MPa | 4350 - 10200 psi | |
Zhejiang Juner JEPP263 Weatherability PP Series Applications: Air Conditioning SystemInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Injection Pressure | 30.0 - 70.0 MPa | 4350 - 10200 psi | |
Zhejiang Juner JEPPB006 High Glossy PP Applications: Electric Rice CookerInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Injection Pressure | 30.0 - 70.0 MPa | 4350 - 10200 psi | |
Toyobo GLAMIDE® TY-791GT 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Injection Pressure | 60.0 - 70.0 MPa | 8700 - 10200 psi | |
Plastcom SLOVALEN PQ 51 N Polypropylene Homopolymer, Modified with Elastomer, Impacted FeaturesHomopolymer PP modified with elastomer. The addition of thermoplastic elastomer causes increased toughness, possible alternative to PP copolymers. General application in all industry branc.. |
|||
Injection Pressure | 60.0 - 70.0 MPa | 8700 - 10200 psi | |
Plastcom SLOVALEN PQ 53 N PP, imp. strength FeaturesPP modified with natural caoutchouc. The addition of thermoplastic caoutchouc causes increased toughness. General application in all industry branches. Delivered in natural mode and in the f.. |