Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 30.0 - 100 MPa @Time 2.00 - 10.0 sec |
4350 - 14500 psi @Time 0.000556 - 0.00278 hour |
|
Gromax 1140LH TPE Product Description: 1140LH is Low modulus grade with nominal Durometer hardness of 40D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like inject.. |
|||
Injection Pressure | 30.0 - 100 MPa @Time 2.00 - 10.0 sec |
4350 - 14500 psi @Time 0.000556 - 0.00278 hour |
|
Gromax 1155LL TPE 1155LL is medium modulus grade with nominal Durometer hardness of 55D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like injection molding and ex.. |
|||
Injection Pressure | 30.0 - 100 MPa @Time 2.00 - 10.0 sec |
4350 - 14500 psi @Time 0.000556 - 0.00278 hour |
|
Gromax 1163LL TPE 163LL is medium modulus grade with nominal Durometer hardness of 63D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like injection molding and ext.. |
|||
Injection Pressure | 30.0 - 100 MPa @Time 2.00 - 10.0 sec |
4350 - 14500 psi @Time 0.000556 - 0.00278 hour |
|
Gromax 1172LL TPE 1172LL is high modulus grade with nominal Durometer hardness of 72D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like blow molding grade. Charac.. |
|||
Injection Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis Nepol™ GB601HP Polypropylene, 30% Long Glass Fiber Reinforced w/BJ356MO Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat.. |
|||
Injection Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis Nepol™ GB601HP Polypropylene, 40% Long Glass Fiber Reinforced w/BJ356MO Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat.. |
|||
Injection Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis Nepol™ GB601HP Polypropylene, 40% Long Glass Fiber Reinforced w/HK060AE Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat.. |
|||
Injection Pressure | 30.0 - 90.0 MPa | 4350 - 13100 psi | |
Zhejiang Juner JEPP2056 PP For Automotive Parts Applications: BumpersInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Injection Pressure | 30.0 - 80.0 MPa | 4350 - 11600 psi | |
Zhejiang Juner JEPPB003 High Glossy PP Applications: Electric Rice CookerInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Injection Pressure | 30.0 - 70.0 MPa | 4350 - 10200 psi | |
Zhejiang Juner JEPPB006 High Glossy PP Applications: Electric Rice CookerInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Injection Pressure | 30.0 - 55.0 MPa | 4350 - 7980 psi | |
Toyobo GLAMIDE® T-400G15 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Injection Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Toyobo GLAMIDE® T-402 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Injection Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Toyobo GLAMIDE® T-521 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Injection Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Toyobo GLAMIDE® T-602G30 MXD66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Injection Pressure | 30.0 - 40.0 MPa | 4350 - 5800 psi | |
Toyobo GLAMIDE® T-656E Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Injection Pressure | 30.0 - 40.0 MPa | 4350 - 5800 psi | |
Toyobo GLAMIDE® T-662 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Injection Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Toyobo GLAMIDE® T-663G30 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Injection Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Toyobo GLAMIDE® T-663G50 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Injection Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Toyobo GLAMIDE® T-665C30 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Injection Pressure | 30.0 - 90.0 MPa | 4350 - 13100 psi | |
Zhejiang Juner PP430R Weatherability PP Series Applications: Air Conditioning SystemInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Injection Pressure | 30.0 - 70.0 MPa | 4350 - 10200 psi | |
Toyobo GLAMIDE® TY-181GC Nylon/Elastomer GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Injection Pressure | 30.0 - 40.0 MPa | 4350 - 5800 psi | |
Toyobo GLAMIDE® TY-502NZ 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Injection Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Toyobo GLAMIDE® TY-835TC Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Injection Pressure | 30.0 - 40.0 MPa | 4350 - 5800 psi | (DAM) |
Toyobo T-661 Nylon 66, Standard Grade (Conditioned) Features: Non-reinforced, Standard GradeInformation provided by Toyobo. |
|||
Injection Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Borealis Nepol™ GB601HP Polypropylene, 20% Long Glass Fiber Reinforced w/BJ356MO Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat.. |
|||
Injection Pressure | 30.0 - 60.0 MPa | 4350 - 8700 psi | |
Toyobo GLAMIDE® NB-1700 Nylon/Olefin GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Injection Pressure | 30.0 - 40.0 MPa | 4350 - 5800 psi | |
Toyobo GLAMIDE® T-802 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Injection Pressure | 30.0 - 40.0 MPa | 4350 - 5800 psi | |
Toyobo T-661 Nylon 66, Standard Grade (DAM) Features: Non-reinforced, Standard GradeInformation provided by Toyobo. |
|||
Injection Pressure | 30.0 MPa | 4350 psi | Recommended Molding Pressure. |
Asahi Glass Fluon® G307 PTFE Granular Powder Fluon®PTFE granular powders (molding powders) are used for the production of sheets, rods, billets and other general moldings.Information provided by Asahi Glass Company, Inc. |
|||
Injection Pressure | 30.0 MPa | 4350 psi | Recommended Molding Pressure. |
Asahi Glass Fluon® G350 PTFE Granular Powder Fluon®PTFE granular powders (molding powders) are used for the production of sheets, rods, billets and other general moldings.Information provided by Asahi Glass Company, Inc. |