Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® AD4820 PC (Europe-Africa-Middle East) LEXAN AD4820 is a high viscosity grade exhibiting low dust attraction with a UV cut-off up to 400 nm and greater optical purity than standard resin. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
37.8 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® FXD9810 PC Copolymer Non-chlorinated, non-brominated Flame retardant PC-siloxane copolymer blend. Excellent processability, super high flow, good impact, UL rated V-0. Limited translucent colors. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HP2EU PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mol.. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® ML7682 PC Copolymer (Asia Pacific) Lexan ML7682 resin is a flame retardant polycarbonate blend featuring high flow, good processability, good impact, good heat resistance, and UV stability. It is of non-chlorine and non-bromine flame.. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® AD4820 PC (Asia Pacific) LEXAN AD4820 is a high viscosity grade exhibiting low dust attraction with a UV cut-off up to 400 nm and greater optical purity than standard resin. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
37.8 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® FXD9810U PC Copolymer (Asia Pacific) Polycarbonate with high flow, excellent processability, good impact and thermal properties, UV stabilized, non-Chlorine and non-Bromine flame retardant, UL rated V-0 and V-1. Available in limited di.. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL SE1GFN1 PPE+HIPS (Europe-Africa-Middle East) Noryl* SE1GFN1 is a 10% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non.. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL SE1GFN1 PPE+HIPS (Europe-Africa-Middle East) Noryl* SE1GFN1 is a 10% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non.. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL SE1GFN2 PPE+HIPS (Europe-Africa-Middle East) Noryl* SE1GFN2 is a 20% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non.. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature 150 - 200 °C |
37.8 µin/in-°F @Temperature 302 - 392 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® A-1133 L WH 015 Polyphthalamide (PPA), 33% Glass Fiber Formerly referred to as Amodel® PXM-13015. Amodel® A-1133 L resin is a 33% glass reinforced polyphthalamide (PPA) which is distinguished by its high-reflectivity white color. This grade featu.. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
37.8 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® X4870HH PC+PET Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st.. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
37.8 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® X4870HH PC+PET (Asia Pacific) Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st.. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics XYLEX HX7509HP PC+POLYESTER Medium flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), fo.. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics XYLEX X7509HP PC+POLYESTER PC+Polyester alloy. Houseware applications. USA/Europe Food contact. this grade will no longer be supported with biocompatibility information and should not be used for medical applications which r.. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics XYLEX X7509HP PC+POLYESTER (Asia Pacific) PC+Polyester alloy. Houseware applications. USA/Europe Food contact. this grade will no longer be supported with biocompatibility information and should not be used for medical applications which r.. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP DX06313 PC (Asia Pacific) Polycarbonate base, 30% glass fiber reinforced, impact modified material. Thinwall housing, mobile phone. Some light color grades may have lower impact data than nature and black grade. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP DX06313 PC (Asia Pacific) Polycarbonate base, 30% glass fiber reinforced, impact modified material. Thinwall housing, mobile phone. Some light color grades may have lower impact data than nature and black grade. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP DX06313I PC (Asia Pacific) DX06313I is 30% glass fiber reinforced, impact modified polycarbonate resin. High flow and good ductility. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL HH180 PPE+PS Noryl* HH180 is a high heat, unfilled modified polyphenylene ether resin with a Vicat B/120 temperature of 185 deg C. Noryl HH180 is only available in color 80365. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL HH180 PPE+PS (Europe-Africa-Middle East) Noryl* HH180 is a high heat, unfilled modified polyphenylene ether resin with a Vicat B/120 temperature of 185 deg C. Noryl HH180 is only available in color 80365. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to.. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to.. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
37.8 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® X5630 PC+PET (Asia Pacific) Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP WC006 PBT LNP* THERMOCOMP* WC006 is a compound based on PBT resin containing 30% Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP WC006 PBT LNP* THERMOCOMP* WC006 is a compound based on PBT resin containing 30% Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOTUF MF004AI PP (Asia Pacific) LNP* Thermotuf* MF004AI is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
37.8 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® X5630 PC+PET (Europe-Africa-Middle East) Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications |