Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 23.0 µm/m-°C

@Temperature 0.000 - 100 °C
12.8 µin/in-°F

@Temperature 32.0 - 212 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® A-1133 NL WH 505 Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1133 NL resin is a 33% glass reinforced polyphthalamide (PPA) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatibilit..
CTE, linear, Parallel to Flow 23.0 µm/m-°C

@Temperature 0.000 - 100 °C
12.8 µin/in-°F

@Temperature 32.0 - 212 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® A-4122 NL WH 905 Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-4122 NL resin is a 22% glass reinforced, high-reflectivity white grade of polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhi..
CTE, linear, Parallel to Flow 23.0 µm/m-°C

@Temperature 0.000 - 100 °C
12.8 µin/in-°F

@Temperature 32.0 - 212 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0..
CTE, linear, Parallel to Flow 23.0 µm/m-°C

@Temperature >=162 °C
12.8 µin/in-°F

@Temperature >=324 °F
Above Tg; ISO 11359
Victrex® ST™ ST45GL30 Polyetherketoneetherketoneketone (PEKEKK), 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, c..
CTE, linear, Parallel to Flow 23.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
12.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP OFL36XXC PPS - Linear
LNP* LUBRICOMP* OFL36XXC is a compound based on PPS - Linear resin containing 30% Glass Fiber, 15% PTFE. Added features of this grade are: Wear Resistant.
CTE, linear, Parallel to Flow 23.0 µm/m-°C

@Temperature 0.000 - 100 °C
12.8 µin/in-°F

@Temperature 32.0 - 212 °F
2
Solvay Specialty Polymers Amodel® A-1133 NL WH 505 Polyphthalamide (PPA), 33% Glass Fiber
Amodel® A-1133 NL resin is a 33% glass reinforced polyphthalamide (PPA) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatib..
CTE, linear, Parallel to Flow 23.0 µm/m-°C

@Temperature 0.000 - 100 °C
12.8 µin/in-°F

@Temperature 32.0 - 212 °F
2
Solvay Specialty Polymers Amodel® A-4122 NL WH 905 Polyphthalamide (PPA), 22% Glass Fiber
Amodel® A-4122 NL resin is a 22% glass reinforced, high-reflectivity white grade of polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material ..
CTE, linear, Parallel to Flow 23.0 µm/m-°C

@Temperature 0.000 - 100 °C
12.8 µin/in-°F

@Temperature 32.0 - 212 °F
2
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater th..
CTE, linear, Parallel to Flow 23.0 µm/m-°C

@Temperature -40.0 - 150 °C
12.8 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics Valox® IQNH4550 PBT
Valox* iQNH4550 resin is a glass filled, non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% ..
CTE, linear, Parallel to Flow 23.0 µm/m-°C

@Temperature -40.0 - 150 °C
12.8 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics Valox® IQNH4550 PBT (Asia Pacific)
Valox* iQNH4550 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% based on EPEAT..
CTE, linear, Parallel to Flow 23.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
12.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® VIC4311 PBT
VALOX VIC4311 is a 30% glass filled, impact modified PBT with excellent epoxy adhesion. Automotive underhood applications such as ignition coil housings.
CTE, linear, Parallel to Flow 23.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
12.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® VIC4311 PBT
VALOX VIC4311 is a 30% glass filled, impact modified PBT with excellent epoxy adhesion. Automotive underhood applications such as ignition coil housings.
CTE, linear, Parallel to Flow 23.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
12.8 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Xenoy® 6380U PBT+PET (Asia Pacific)
XENOY 6380U is a 30% glass reinforced, UV stabilized grade, that combines high stiffness with improved ductility. The combination of mechanical properties at high and low temperatures and chemical r..
CTE, linear, Parallel to Flow 23.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
12.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL GFN3 PPE+HIPS (Asia Pacific)
PPE+PS blend. 30% Glass reinforced.FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Suitable for fluid engineering applications including pump ..
CTE, linear, Parallel to Flow 23.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
12.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL GTX GTX8720 PPE+PA
Noryl GTX* GTX8720 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-..
CTE, linear, Parallel to Flow 23.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
12.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL GTX GTX8720 PPE+PA
Noryl GTX* GTX8720 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-..
CTE, linear, Parallel to Flow 23.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
12.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL GTX GTX8720 PPE+PA (Asia Pacific)
Noryl GTX* GTX8720 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-..
CTE, linear, Parallel to Flow 23.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
12.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL GTX GTX8720 PPE+PA (Asia Pacific)
Noryl GTX* GTX8720 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-..
CTE, linear, Parallel to Flow 23.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
12.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL GTX GTX8720 PPE+PA (Europe-Africa-Middle East)
Noryl GTX* GTX8720 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-..
CTE, linear, Parallel to Flow 23.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
12.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL GTX GTX8720 PPE+PA (Europe-Africa-Middle East)
Noryl GTX* GTX8720 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-..
CTE, linear, Parallel to Flow 23.0 µm/m-°C

@Temperature -40.0 - 150 °C
12.8 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics Valox® IQNH4550 PBT (Europe-Africa-Middle East)
Valox* iQNH4550 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% based on EPEAT..
CTE, linear, Parallel to Flow 23.0 µm/m-°C

@Temperature 180 °C
12.8 µin/in-°F

@Temperature 356 °F
DIN 53752
BASF Ultrason® E 2010 G4 MR SW 15102 20% Glass Filled PESU
Information provided by BASF
CTE, linear, Parallel to Flow 23.0 µm/m-°C

@Temperature 140 - 180 °C
12.8 µin/in-°F

@Temperature 284 - 356 °F
ISO 180/A
BASF Ultrason E 2010 G4 20% Glass Filled PES
Ultrason E 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength.
CTE, linear, Parallel to Flow 23.0 µm/m-°C

@Temperature 0.000 - 100 °C
12.8 µin/in-°F

@Temperature 32.0 - 212 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® A-1240 L Polyphthalamide (PPA)  (discontinued **)
Amodel A-1240 L is a 40% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten..
Copyright © lookpolymers.com All Rights Reserved