| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Hot Ball Pressure Test | <= 125 °C | <= 257 °F | IEC 60695-10-2 |
|
SABIC Innovative Plastics Cycoloy® C1200 PC+ABS (Europe-Africa-Middle East)
CYCOLOY C1200 is a PC+ABS blend developed to serve extremely demanding applications in a variety of markets while maintaining good processing properties. The combination of superior heat resistance ..
|
|||
| Hot Ball Pressure Test | <= 125 °C | <= 257 °F | IEC 60695-10-2 |
|
SABIC Innovative Plastics Cycoloy® C3100 PC+ABS (Europe-Africa-Middle East)
C3100 is blow moulding/extrusion grade offering low temperature ductility, high heat resistance and high meltstrength.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Hot Ball Pressure Test | <= 125 °C | <= 257 °F | IEC 60695-10-2 |
|
SABIC Innovative Plastics Lexan® FST9436 PC Copolymer
Medium viscosity opaque, low smoke, and OSU 65/65 compliant PC Copolymer
|
|||
| Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 598-1 |
|
LG Chemical Lupoy 1200-10 Polycarbonate Resin
Description: LUPOY PC 1200-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
|
|||
| Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 598-1 |
|
LG Chemical Lupoy 1201-18 Polycarbonate Resin
Description: LUPOY PC 1201-18 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
|
|||
| Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 598-1 |
|
LG Chemical Lupoy 1301-10 Polycarbonate Resin
Description: LUPOY PC 1301-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
|
|||
| Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 598-1 |
|
LG Chemical Lupoy 1301-12 Polycarbonate Resin
Description: LUPOY PC 1301-12 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
|
|||
| Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 598-1 |
|
LG Chemical Lupoy 1301V-10 Polycarbonate Resin
Description: LUPOY PC 1301V-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength..
|
|||
| Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 598-1 |
|
LG Chemical Lupoy 1302-07 Polycarbonate Resin
Description: LUPOY PC 1302-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
|
|||
| Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 598-1 |
|
LG Chemical Lupoy 1303EP-22 Polycarbonate Resin
Description: LUPOY PC 1303EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
|
|||
| Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 598-1 |
|
LG Chemical Lupoy 3010-22 Polycarbonate Resin
Description: LUPOY PC 3010-22 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character..
|
|||
| Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 598-1 |
|
LG Chemical Lupoy 3030-15 Polycarbonate Resin
Description: LUPOY PC 3030-15 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character..
|
|||
| Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 598-1 |
|
LG Chemical Lupoy NF1009F 15 Polycarbonate Resin
Description: LUPOY NF 1009F15, eco-friendly UL94 V0/2.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpare..
|
|||
| Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 598-1 |
|
LG Chemical Lupoy 1201HP-22 Polycarbonate Resin
Description: LUPOY PC 1201HP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
|
|||
| Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 598-1 |
|
LG Chemical Lupoy 1302HP-22 Polycarbonate Resin
Description: LUPOY PC 1302HP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
|
|||
| Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 598-1 |
|
LG Chemical Lupoy 1303EP-30 Polycarbonate Resin
Description: LUPOY PC 1303EP-30 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
|
|||
| Hot Ball Pressure Test | 125 °C | 257 °F | IEC 60695-10-2 |
|
SABIC Innovative Plastics NORYL PX9406P PPE+PS (Europe-Africa-Middle East) |
|||
| Hot Ball Pressure Test | <= 125 °C | <= 257 °F | IEC 60695-10-2 |
|
SABIC Innovative Plastics NORYL V01525 PPE+HIPS
Noryl* V01525 is a 15% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
|
|||
| Hot Ball Pressure Test | 125 °C | 257 °F | IEC 60335-1 |
|
Styron CALIBREâ„¢ 201-10 Polycarbonate Resin
Overview: CALIBREâ„¢ 201-10 is produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. It provides excellent impact resistance, heat distortion resi..
|
|||
| Hot Ball Pressure Test | 125 °C | 257 °F | IEC 60335-1 |
|
Styron CALIBREâ„¢ 201-15 Polycarbonate Resin
Overview: CALIBREâ„¢ 201-15 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc..
|
|||
| Hot Ball Pressure Test | 125 °C | 257 °F | IEC 60335-1 |
|
Styron CALIBREâ„¢ 201-6 Polycarbonate Resin
Overview: CALIBREâ„¢ 201-6 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistance..
|
|||
| Hot Ball Pressure Test | 125 °C | 257 °F | IEC 60335-1 |
|
Styron CALIBREâ„¢ 301-15 Polycarbonate Resin
Overview: CALIBREâ„¢ 300-115 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity. The CALIBREâ„¢ 300-10 series products are available in 4 ..
|
|||
| Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 60335-1 |
|
Styron CALIBREâ„¢ 301EP-22 Polycarbonate Resin
Overview: CALIBREâ„¢ 300EP-22 Series are polycarbonate resins that offer exceptional impact resistance, heat distortion resistance and optical clarity for injection molding applications. Their hi..
|
|||
| Hot Ball Pressure Test | 125 °C | 257 °F | IEC 60335-1 |
|
Styron CALIBREâ„¢ 701-15 Polycarbonate Resin
Overview: CALIBREâ„¢ 701-15 Series resins are formulated and produced to supply both clarity and enhanced ignition resistance. They do so while maintaining excellent physical properties and proce..
|
|||
| Hot Ball Pressure Test | 125 °C | 257 °F | IEC 60335-1 |
|
Styron CALIBREâ„¢ 703-15 Polycarbonate Resin
Overview: CALIBREâ„¢ 701-15 Series resins are formulated and produced to supply both clarity and enhanced ignition resistance. They do so while maintaining excellent physical properties and proce..
|
|||
| Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 60335-1 |
|
Styron EMERGEâ„¢ 4702-15 Polycarbonate
EMERGEâ„¢ PC 4702-15 advanced resin is formulated with 20% glass fiber and a proprietary flame retardant package. It provides good ignition resistance, rigidity, dimension stability and heat res..
|
|||
| Hot Ball Pressure Test | 125 °C | 257 °F | IEC 60335-1 |
|
Styron CALIBREâ„¢ 302V-10 Polycarbonate Resin
Overview: CALIBREâ„¢ 300V Polycarbonate resins offer exceptional impact resistance, heat distortion resistance, optical clarity and meets UL94 V-2 rating. CALIBRE 300V series products are availab..
|
|||
| Hot Ball Pressure Test | 125 °C | 257 °F | I.E.C. 335-1 |
|
Cossa Polimeri ESTABLEND 4501 V0/D Flame Retardant PC - ABS
PC - ABS BlendFlame retardant class V0, PBDE and antimony free, with halogens, high impact resistance, very high thermal resistance, high gloss, good processabilityInformation provided by Cossa Poli..
|
|||
| Hot Ball Pressure Test | >= 125 °C | >= 257 °F | BS 3456, IEC 335 |
|
EPICHEM Epicarb PC BLACK IQ Polycarbonate
Characteristics: good fluidity, good impact, industrial quality
|
|||
| Hot Ball Pressure Test | >= 125 °C | >= 257 °F | BS 3456, IEC 335 |
|
EPICHEM Epilon PC UVR Polycarbonate, High Impact
Characteristics: high fluidity, high impact, UV resistant
|
|||