Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants 436 (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants 438 (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants 570H-10 (NT) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants UniFlor 8511E (853-2EP) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants UniFlor 8512 (842) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants UniFlor 8520 (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants UniFlor 8521 (841-1) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants UniFlor 8521R (841RP-1) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants UniFlor 8911 (891-1) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants UniFlor 8971 (898-1) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | |
Precision Polymer Engineering V90D Fluoroelastomer Compound Fluoroelastomer Rubber, 86-93 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Meets Aerospace Specifications DTD5612A and DTD5543B Grade 90. ASTM designation = FKM. ISO designatio.. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | |
Precision Polymer Engineering V97B Fluoroelastomer Compound Fluoroelastomer Rubber, 90-98 °IRHD. Terpolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene. To meet ASTM D2000 line call-out M3HK914, A1-10, B37, B38, EF31, EO78, Z1. Wher.. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | |
LATI Larton GCE/650 PPS, Glass/Mineral Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa .. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | |
LATI Larton K/30 PPS, 30% Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Ball pressure temperature; IEC Method |
Toyobo VYLOPET® EMC130-20 Injection Molding Polyester Resin, Flame Resistant Applications: Relay partsFeatures: Excellent arc resistanceFlame resistanceInformation provided by Toyobo. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Ball pressure temperature; IEC Method |
Toyobo VYLOPET® EMC132-01 Injection Molding Polyester Resin, Flame Resistant Applications: Relay partsFeatures: Excellent arc resistanceFlame resistanceInformation provided by Toyobo. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Ball pressure temperature; IEC Method |
Toyobo VYLOPET® EMC132-02 Injection Molding Polyester Resin, Flame Resistant Applications: Relay partsFeatures: Excellent arc resistanceFlame resistanceInformation provided by Toyobo. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Ball pressure temperature; IEC Method |
Toyobo VYLOPET® EMC133 Injection Molding Polyester Resin, Hydrolysis Resistant Applications: Electric rice cooker partsBathroom appliancesFeatures: Good hydrolysis resistanceInformation provided by Toyobo. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Ball pressure temperature; IEC Method |
Toyobo VYLOPET® EMC341 Injection Molding Polyester Resin, Hydrolysis Resistant Applications: Electric rice cooker partsBathroom appliancesFeatures: Good hydrolysis resistanceInformation provided by Toyobo. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Heat Resistance; ASTM D570D |
Plenco 6343 Phenolic, Granular, Compression Molded PLENCO 06343 is a mica reinforced phenolic molding compound, offering for a low power factor, low electrical losses, and good electrical properties after long exposures to high humidity. UL recogniz.. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Ball pressure temperature; IEC Method |
Toyobo VYLOPET® EMC330 Injection Molding Polyester Resin, Hydrolysis Resistant Applications: Electric rice cooker partsBathroom appliancesFeatures: Good hydrolysis resistanceInformation provided by Toyobo. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Ball pressure temperature; IEC Method |
Toyobo VYLOPET® EMC532 Injection Molding Polyester Resin, Glass Reinforced Applications: Auto-partsFeatures: Ultrasonic weldabilityGlass fiber reinforcementInformation provided by Toyobo. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Continuous |
Epoxy Technology EPO-TEK® 353ND-T1 High Temperature Thixotropic Epoxy Material Description: A two component, thixotropic and high temperature epoxy designed for fiber optic, electronics and medical applications. It is a more viscous alternative to EPO-TEK® 353ND-T.I.. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Continuous |
Epoxy Technology EPO-TEK® H27D Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H27D is a two component, silver-filled epoxy adhesive designed for semiconductor and hybrid-microelectronic packaging applications.Advantages & Application Notes: Rheo.. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Intermittent |
Epoxy Technology EPO-TEK® OG178 UV Cure Optical Epoxy Material Description: A single component, UV/visible shifted light curable epoxy, designed for adhesive, sealing, coating and encapsulating applications found in semiconductor, electro-optics, fiber.. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Continuous |
Epoxy Technology EPO-TEK® P1011 Electrically Conductive Modified Polyimide Product Description: EPO-TEK® P-1011 is a single component, modified polyimide, silver-filled adhesive designed for chip bonding in microelectronic and optoelectronic applications.Advantages & Appl.. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Intermittent |
Epoxy Technology EPO-TEK® T7109-18 Electrically Insulating Epoxy Paste Material Description: A flexible, electrically insulating epoxy paste designed for low stress and heat dissipation applications. Alternative to EPO-TEK® T7109-17.Information Provided by Epoxy Tec.. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Continuous |
Epoxy Technology EPO-TEK® U300-2 Two Component Epoxy Material Description: A two component epoxy designed for capillary underfill of semiconductor chips and SMDs. Long potlife, high Tg, and optical clarity are a few of its traits. NASA approved lo.. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Recommended |
Nye Lubricants UniFlor 8917 (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 225 °C | 437 °F | Heat Resistance; ASTM D570D |
Plenco 7552 Phenolic, Nodular, Transfer Molded PLENCO 07552 is a glass fiber reinforced novolac phenolic molding compound, exhibiting superior dimensional stability, good impact strength, and good electrical properties. Type ASTM 5948 MFH. UL re.. |