Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 7552 Phenolic, Nodular, Transfer Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Glass Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 7552 Phenolic, Nodular, Transfer Molded.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PLENCO 07552 is a glass fiber reinforced novolac phenolic molding compound, exhibiting superior dimensional stability, good impact strength, and good electrical properties. Type ASTM 5948 MFH. UL recognized under component file E40654.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.710 g/cc
0.0257 lb/in³
ASTM D1895
Density 1.78 g/cc
0.0643 lb/in³
ASTM D792
Water Absorption 0.090 %
0.090 %
ASTM D570
Linear Mold Shrinkage 0.00143 cm/cm
0.00143 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 78
78
ASTM D785
Tensile Strength, Ultimate 57.0 MPa
8270 psi
ASTM D638
Elongation at Break 0.60 %
0.60 %
ASTM D638
Tensile Modulus 13.1 GPa
1900 ksi
ASTM D638
Flexural Strength 102 MPa
14800 psi
ASTM D790
Flexural Modulus 12.8 GPa
1860 ksi
ASTM D790
Compressive Strength 168 MPa
24400 psi
ASTM D695
Izod Impact, Notched 0.570 J/cm
1.07 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.620 J/cm²
2.95 ft-lb/in²
ASTM D256
Impact 227
227
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 42.0 µm/m-°C

@Temperature 40.0 - 130 °C
23.3 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Maximum Service Temperature, Air 225 °C
437 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 280 °C
536 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Oxygen Index 46 %
46 %
ASTM D2863
Shrinkage 0.070 %
0.070 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 1.30e+12 ohm-cm
1.30e+12 ohm-cm
ASTM D247
Dielectric Constant 5.0
5.0
ASTM D150
Dielectric Strength 14.3 kV/mm
363 kV/in
Short Time; ASTM D149
Dissipation Factor 0.033
0.033
ASTM D150
Arc Resistance 184 sec
184 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638