| Category | Polymer , Thermoset , Epoxy |
| Manufacturer | Epoxy Technology |
| Trade Name | EPO-TEK® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Epoxy Technology EPO-TEK® T7109-18 Electrically Insulating Epoxy Paste.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.07 g/cc | 1.07 g/cc | Part B |
| 1.86 g/cc | 1.86 g/cc | Part A | |
| Particle Size | <= 20 µm | <= 20 µm | |
| Viscosity | 6500 - 10700 cP @Temperature 23.0 °C |
6500 - 10700 cP @Temperature 73.4 °F |
20 rpm |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 69 | 69 | |
| Tensile Modulus | 0.009873 GPa | 1.432 ksi | Storage |
| Shear Strength | 1.50 MPa | 218 psi | Lap |
| >= 2.34 MPa | >= 340 psi | Die |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 68.0 µm/m-°C | 37.8 µin/in-°F | Below Tg |
| 200 µm/m-°C | 111 µin/in-°F | Above Tg | |
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | |
| Maximum Service Temperature, Air | 125 °C | 257 °F | Continuous |
| 225 °C | 437 °F | Intermittent | |
| Minimum Service Temperature, Air | -55.0 °C | -67.0 °F | Continuous |
| -55.0 °C | -67.0 °F | Intermittent | |
| Glass Transition Temp, Tg | >= 5.00 °C | >= 41.0 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min |
| Decomposition Temperature | 294 °C | 561 °F | Degradation Temperature |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 5.00e+9 ohm-cm | >= 5.00e+9 ohm-cm | |
| Dielectric Constant | 5.63 @Frequency 1000 Hz |
5.63 @Frequency 1000 Hz |
|
| Dissipation Factor | 0.070 @Frequency 1000 Hz |
0.070 @Frequency 1000 Hz |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 120 min @Temperature 80.0 °C |
2.00 hour @Temperature 176 °F |
Minimum |
| 2880 min @Temperature 23.0 °C |
48.0 hour @Temperature 73.4 °F |
Minimum | |
| Pot Life | 90 min | 90 min | |
| Shelf Life | 6.00 Month @Temperature 25.0 °C |
6.00 Month @Temperature 77.0 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Clear | Part B |
| Gray | Part A | |
| Consistency | Smooth flowing paste | |
| Mix Ratio By Weight | 10:2 | |
| Number of Components | Two | |
| Thixotropic Index | 2.2 | |
| Weight Loss | 0.5% | 200°C |
| 1.18% | 250°C | |
| 4.51% | 300°C |