Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 200 °C | 392 °F | Recommended |
Nye Lubricants 802-1 (FG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | >= 200 °C | >= 392 °F | pending UL RTI |
Rogers Corporation Syron™ 7000 Thermoplastic Circuit Material SYRON™ 7000 thermoplastic circuit materials provide an excellent solution for printed circuit board applications used in demanding environmental conditions. SYRON 7000 is thermally stable, with a .. |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | |
Precision Polymer Engineering V60G Fluoroelastomer Compound Green Fluoroelastomer Rubber, 56-65 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out M2HK610, A1-10, B38, EF31, EO78, F15, Z1. Where Z1 = colour gr.. |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | |
Precision Polymer Engineering V60H Fluoroelastomer Compound Fluoroelastomer Rubber, 60 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Formulated using only those ingredients determined by the United States Federal Food and Drug Administra.. |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | |
Precision Polymer Engineering V70J Fluoroelastomer Compound Grey Fluoroelastomer Rubber, 65-75 °IRHD. Terpolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene. To meet ASTM D2000 line call-out M2HK710, A1-10, B38, EF31, EO78, Z2, wher.. |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | |
Precision Polymer Engineering V90B Fluoroelastomer Compound Fluoroelastomer Rubber, 85-95 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out:- M5HK910, A1-11, B38, EF31, EO78, F15, Z1. Where Z1 = compression s.. |
|||
Maximum Service Temperature, Air | 200 °C @Time >=1200 sec |
392 °F @Time >=0.333 hour |
|
Kazanorgsintez 271-274K Cable Composition Based on High Density Polyethylene Production Method: Gaseous-phase method. Application: Compositions are intended for cover insulating lapping, protective covers and cables.Information Provided by Kazanorgsintez |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | short term |
Lehmann & Voss LUVOCOM® 1100-8325 Polyether sulfone, with glass fiber and PTFE Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.Improved friction and .. |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | short term |
Lehmann & Voss LUVOCOM® 1100-7890 Polyether sulfone, with carbon fiber Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Maximum Service Temperature, Air | 200 - 220 °C | 392 - 428 °F | UL Temperature Rating |
Solvay Specialty Polymers Ryton® R-4-200NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-200NA and R-4-200BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and low maintenance molding using conventional molding equipmentFeat.. |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | Short peaks operation |
Polyram PlusTek PA320G3 Nylon 6.6 for Injection Molding, 15% Glass Fiber Reinforced, Flame Retardant 15% Glass fiber reinforced flame retardant Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Maximum Service Temperature, Air | >= 200 °C | >= 392 °F | Short peaks operation |
Polyram PlusTek PB320G6 Nylon 6, 30% Glass Fiber, Flame Retardant 30% glass-fiber reinforced, flame retardant polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | Short peaks operation |
Polyram PlusTek PA100 Nylon 6.6, General Purpose General purpose polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Maximum Service Temperature, Air | >= 200 °C | >= 392 °F | Short peaks operation |
Polyram PlusTek PA840G6 Nylon 6.6, 30% Glass Fiber 30% glass fiber reinforced, impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | |
Trelleborg S750 Silicone Rubber PropertiesExcellent resistance to heat (dry air), at +200°C continuous and +220°C intermittent.Remains flexible at low temperatures of -70°C.Resistant to ultra-violet light, ozone and weathering... |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | |
Dow Corning XIAMETER® PMCPPMX-200 5,000CS Silicone Fluid Is chemically equivalent to DOW CORNING® 200 FLUID 5,000CS. 100% active, high viscosity, polydimethylsiloxane polymer.Information provided by Dow Corning |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | Continuous use |
Daikin NEOFLON NP-40 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, transfer molding, compression molding.Applications: Films and s.. |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | Continuous |
Epoxy Technology EPO-TEK® 320-LV Optically Opaque Epoxy Material Description: A two component, optically opaque epoxy adhesive designed for semiconductor and PCB applications in optoelectronic instrumentation and assemblies. A lower viscosity version of.. |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | Continuous |
Epoxy Technology EPO-TEK® 377 High Temperature Epoxy Product Description: EPO TEK®377 is a two component, high Tg, fiber optic grade epoxy adhesive. It is well suited for semiconductor, medical and optical applications.Advantages & Application Notes:.. |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | Continuous |
Epoxy Technology EPO-TEK® EE149-6 Epoxy Material Description: A single component, silver-filled, B-stageable epoxy designed for semiconductor flip chip packaging or hybrid micro-electronic substrate attach or lid-sealing.Information Provi.. |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | ASTM D 3575 |
Eurofoam Siliconcell 411/PLT Platinic Silicone Foam Excellent thermal insulation and soundproofingInformation provided by Eurofoam s.r.l. |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | per UL Card E54153 |
Arlon 0.028" (0.7112 mm) Flexible Heater Silicone with Fiberglass Substrate (55586W028) 0.004 in. (0.1 mm) minimum uncured silicone on 0.006 in. (0.2 mm) minimum cured silicone on 0.018 in. (0.46 mm) nominal Prime Coated 162 Fiberglass; 0.003 in. (0.08 mm) polyethylene interleave; over.. |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | rated per UL card E54153 |
Arlon 51589R015 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of,.. |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | Recommended |
Nye Lubricants 783C (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | |
BASF Sicopal® Yellow L 1100 Color Additive Description: Weather-resistant inorganic bismuth vanadate pigment with high hiding powerChemical Structure: Bismuth vanadatSuitable for: Baking System, Waterborn systems, Acrylic-isocyanate systems,.. |
|||
Maximum Service Temperature, Air | 200 °C | 392 °F | |
BASF Ultramid® B3WG5 BK 00654 PA6 25% Glass Filled BK (Dry) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |