Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eurofoam Siliconcell 411/PLT Platinic Silicone Foam

Category Polymer , Thermoset , Silicone , Silicone Foam
Manufacturer Eurofoam s.r.l.
Trade Name Siliconcell
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurofoam Siliconcell 411/PLT Platinic Silicone Foam.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Excellent thermal insulation and soundproofingInformation provided by Eurofoam s.r.l.
Physical Properties Metric English Comments
Density 0.400 - 0.440 g/cc
0.0145 - 0.0159 lb/in³
ISO 845-88
Water Absorption <= 5.0 %
<= 5.0 %
ASTM D 1056
Mechanical Properties Metric English Comments
Hardness, Shore OO 50 - 60
50 - 60
ASTM D 2240
Tensile Strength 0.150 MPa
21.8 psi
ASTM D 412
Elongation at Break >= 300 %
>= 300 %
ASTM D 412
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
ASTM D 3575
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
ASTM D 3575
Shrinkage <= 5.0 %

@Temperature 70.0 °C,
Time 605000 sec
<= 5.0 %

@Temperature 158 °F,
Time 168 hour
Linear; ASTM D 1204
Compliance Properties Metric English Comments
European Food 1935/2004 Yes
Yes
EU 90/128/EC
FDA Yes
Yes
FDA N.177.2600
Descriptive Properties Value Comments
Cellular Structure Closed
Color White
Declaration of Heavy Metal Absence Conform
RoHS2002/95/EC
UL Flammability HF-1