Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 170 °C | 338 °F | Intermittent |
Nylacast PA6C Cast Nylon 6 Natural PA6 is the base to the other grades of material offered by Nylacast. It is available in Natural (off white) or Black colour. It is made by ionic polymerisation of e-caprolactam under anhydri.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | short term |
Polikim KESTOIL® Polyamide 6 + Lubricant Kestoil® is a self-lubricated, strong, wear resistant engineering plastic with a low coefficient of friction. Implicit in its nature, it has many properties that no other material has in combinatio.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | short period, no load (dry sample) |
Omnia Plastica Rilsan® PA6 GF - Akulon GF - at 50% RH Polyamide 6 reinforced with the addition of 30% glass fibre and graphite. The glass charge makes the material highly resistant to abrasion, compression and flexing. Akulon GF is particularly suitabl.. |
|||
Maximum Service Temperature, Air | 170 - 171 °C | 338 - 340 °F | Average value: 171 °C Grade Count:3 |
Overview of materials for Polyetherimide (PEI), 30% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 30% Glass Fiber". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Maximum Service Temperature, Air | 170 - 200 °C | 338 - 392 °F | Average value: 189 °C Grade Count:7 |
Overview of materials for Phenolic, Novolac, Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Flock Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
G-3 Fiberglass Phenolic Laminate Sheet This material is made from woven glass cloth and high-temperature phenolic resin. It has excellent flexural, compressive and impact strengths. Physical strength, resiliency, ease and versatility of .. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
Lehmann & Voss LUVOCOM® 1106-8032/GY Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
Lehmann & Voss LUVOCOM® 1106-8085/YL Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
Lehmann & Voss LUVOCOM® 1106-8086/YL Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | short term |
Lehmann & Voss LUVOCOM® 19/XCF/20 Polyamide 46, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | Intermittent |
Global EPP PA 6C Cast Polyamide 6 Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of .. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
Menzolit Menzolit® BMC 0400 Unsaturated Polyester UP BMC 0400 is a low profile DMC/BMC for automotive applications. It fulfills the requirements of the automotive industry regarding painted body panels including reduced C-emissions. For highest surfac.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
Lehmann & Voss LUVOCOM® 1106-8133 Polyether imide, with carbon fiber, easy flowing Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.High dimensionally stable precision parts.Electrical.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
Lehmann & Voss LUVOCOM® 1106-8217 Polyether imide, with PTFE, lubricant modified Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Control disks, cams, slidi.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
Lehmann & Voss LUVOCOM® 1106-8232 Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
Menzolit Menzolit® BMC 1400 Unsaturated Polyester UP BMC 1400 is a special BMC for the use on an engine. The glass content is set to a level that combines good mouldability with good strength and stiffness properties. The product has been developped f.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | <20000 hours; IEC 60216-P1 |
Hexion UP 802 Unsaturated Polyester Resin, High Surface Quality, Low Shrinkage, High Arc Resistance Polyester molding compound, inorganically filled, glass fiber reinforced, styrene free, high dimensional stability, very slight post shrinkage, good mechanical properties, increased electrical value.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
Sichuan Deyang Haton® 220 dtex Polyphenylene Sulfide Filament Excellent chemical stabilityInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Maximum Service Temperature, Air | 170 °C @Time >=1800 sec |
338 °F @Time >=0.500 hour |
Congo Red; BS 2782 |
Teknor Apex Sinvicomp SFE 3500 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Food Contact Acceptable; Non-Toxic Uses: Hose; Tubing Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
Chesterton 622 White Grease Description: Chesterton® 622 White Grease is a pure mineral oil grease with PTFE added designed for applications where a clean, nonstaining, food grade lubricant is required. It is a superior, mult.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | Long Term |
Ensinger TECATRON™ PPS Polyphenylene sulfide (PPS) TECATRON PPS is a high performance thermoplastic that combines good mechanical properties with excellent thermal and chemical resistance properties. There is no known solvent that dissolves TECATRON.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
BASF Ultradur® S 4090 G6X High Speed 30% Glass Filled PBT Description: Low-warpage, easy-flowing injection molding grade with 30 % glass fibers for technical parts, for which dimensional stability is very important, reduction of wall thickness (eg, e/e hou.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
BASF Ultradur® S 4090 GM11 5/5% Glass/Mineral Filled PBT Description: Is a PBT + ASA, injection-molding grades reinforced with 5% glass fiber/mineral, for laminar parts with high demands on dimensional stability and low warpage, e.g. lids, ventilation gri.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
ATG s.r.l. HNBR Hydrogenated Nitrile Butadiene Rubber |
|||
Maximum Service Temperature, Air | 170 °C @Time 10800 sec |
338 °F @Time 3.00 hour |
no distortion |
AlphaGary Evoprene™ LF 6156 Automotive Thermoplastic Elastomer Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
BASF Ultradur® S 4090 G6X 30% Glass Filled PBT Description: Is a PBT + ASA, low-warpage, free-flowing injection-molding grades with very good processing capabilities, containing 30% of glass fibers for industrial parts with high dimensional stab.. |
|||
Maximum Service Temperature, Air | 170 °C @Time >=Error in fixSigDigits: @digits must be between 1 a sec |
338 °F @Time >=Error in fixSigDigits: @digits must be between 1 a hour |
Congo Red; BS 2782 |
Teknor Apex Sinvicomp SFE 4000 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Food Contact Acceptable; Non-Toxic Uses: Hose; Tubing Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
Lehmann & Voss LUVOCOM® 1106-7940/GY Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |