Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ensinger TECATRON™ PPS Polyphenylene sulfide (PPS)

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS)
Manufacturer Ensinger
Trade Name TECATRON™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger TECATRON™ PPS Polyphenylene sulfide (PPS).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
TECATRON PPS is a high performance thermoplastic that combines good mechanical properties with excellent thermal and chemical resistance properties. There is no known solvent that dissolves TECATRON PPS at temperatures below 392°F. Its low ionic impurities make it an excellent choice for applications where high purity is a concern. TECATRON GF40 is a glass reinforced material that offers extremely high strength along with excellent chemical resistance properties. TECATRON PVX is a bearing grade PPS that is suitable for high load applications.Information Provided by Ensinger Industries, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Density 1.35 g/cc
0.0488 lb/in³
ASTM D792
Water Absorption at Saturation 0.020 %

@Temperature 22.8 °C,
Time 86400 sec
0.020 %

@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 104
104
ASTM D785
Tensile Strength, Yield 60.0 MPa

@Temperature 22.8 °C
8700 psi

@Temperature 73.0 °F
ASTM D638
Elongation at Break 4.0 %

@Temperature 22.8 °C
4.0 %

@Temperature 73.0 °F
ASTM D638
Tensile Modulus 3.31 GPa
480 ksi
ASTM D638
Flexural Strength 120 MPa

@Temperature 22.8 °C
17400 psi

@Temperature 73.0 °F
ASTM D790
Flexural Modulus 3.00 GPa

@Temperature 22.8 °C
435 ksi

@Temperature 73.0 °F
ASTM D790
Izod Impact, Notched 0.267 J/cm

@Temperature 22.8 °C
0.500 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Coefficient of Friction, Dynamic 0.24

@Pressure 0.276 MPa
0.24

@Pressure 40.0 psi
50 fpm; ASTM D3702
K Factor (Wear Factor) 5.4e-8

@Pressure 0.276 MPa
5.4e-8

@Pressure 40.0 psi
(in<sup>3</sup>/hr)x(1/PV), 50 fpm, Against Steel; ASTM D3702
Thermal Properties Metric English Comments
CTE, linear 72.0 µm/m-°C
40.0 µin/in-°F
ASTM D696
Thermal Conductivity 0.300 W/m-K
2.08 BTU-in/hr-ft²-°F
Melting Point 282 °C
540 °F
ASTM D2133
Maximum Service Temperature, Air 170 °C
338 °F
Long Term
Deflection Temperature at 0.46 MPa (66 psi) 204 °C
400 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
220 °F
ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Dielectric Constant 3.0

@Frequency 60.0 Hz,
Temperature 22.8 °C
3.0

@Frequency 60.0 Hz,
Temperature 73.0 °F
50% RH; ASTM D150
Dissipation Factor 0.00010

@Frequency 60.0 Hz,
Temperature 22.8 °C
0.00010

@Frequency 60.0 Hz,
Temperature 73.0 °F
ASTM D150