Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.400 W/m-K | 2.78 BTU-in/hr-ft²-°F | ISO 52612 |
Murtfeldt Material ”S”® 8000 Polyethylene Material ”S”® 8000 improves on the already impressive material properties of Original Material ”S”®. The self lubricating character of this material makes it ideally suited for use in sliding.. |
|||
Thermal Conductivity | 0.400 W/m-K | 2.78 BTU-in/hr-ft²-°F | ISO 52612 |
Murtfeldt Muralen® Black Antistatic Polyethylene, Conductive Muralen® is based on high molecular weight polyethylene (PE-HMW) and is ideally suited for use in applications that require the generally impressive material properties of polyethylene. Because of.. |
|||
Thermal Conductivity | 0.400 W/m-K | 2.78 BTU-in/hr-ft²-°F | ISO 52612 |
Murtfeldt Original Material ”S”® Green Polyethylene Material ”S”® is based on virgin, ultrahigh molecular weight low pressure polyethylene and significantly exceeds the requirements of DIN 16972. In particular, Material ”S”® green has excellen.. |
|||
Thermal Conductivity | 0.400 W/m-K | 2.78 BTU-in/hr-ft²-°F | ISO 52612 |
Murtfeldt Original Material ”S”® plus + Bright ESD Polyethylene, Conductive Material ”S”® plus+ Bright ESD is a light plastic with high conductivity and a voltage-dissipating effect on earthed components. This material is ideal for use in applications where a high value.. |
|||
Thermal Conductivity | 0.400 W/m-K | 2.78 BTU-in/hr-ft²-°F | ISO 52612 |
Murtfeldt Original Material ”S”® plus + LF ESD Polyethylene, Low Friction Conductive This material is electrically conductive and has half the sliding friction coefficient of the Original Material ”S”® enabling voltage to be dissipated at maximum speed with the same maximum frict.. |
|||
Thermal Conductivity | 0.400 W/m-K | 2.78 BTU-in/hr-ft²-°F | DIN.52612 |
Omnia Plastica PE 1000 - Polyethylene 1000 Polyethylene with a molecular weight of ± 1000,000 with excellent impact strength. PE 1000 is less rigid and has a higher shock resistance than the low molecular weight polyethylene and it is there.. |
|||
Thermal Conductivity | 0.400 W/m-K | 2.78 BTU-in/hr-ft²-°F | |
Quadrant EPP Cestilene™ HD 1000 R Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Thermal Conductivity | 0.400 W/m-K | 2.78 BTU-in/hr-ft²-°F | |
Quadrant EPP TIVAR® Dryslide PE-UHMW + internal lubricant + other additives (ISO Data) Thanks to the lubricant built into a PE-UHMW matrix with higher molecular weight, TIVAR DrySlide offers a lower coefficient of friction and enhanced wear and abrasion resistance than TIVAR 1000. The.. |
|||
Thermal Conductivity | 0.400 W/m-K | 2.78 BTU-in/hr-ft²-°F | |
Quadrant EPP TIVAR® MD PE-UHMW + metal detectable additive (ISO Data) This PE-UHMW grade with extremely high degree of polymerisation contains a metal detectable additive which does hardly affect the inherent PE-UHMW key properties. TIVAR MD presents excellent toughne.. |
|||
Thermal Conductivity | 0.400 - 0.600 W/m-K | 2.78 - 4.16 BTU-in/hr-ft²-°F | ASTM E1461 |
Raschig Group 4554 Silicone Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to 300°C, exceptional electrical properties, good mechanical strength, very good dimensional stability. Processi.. |
|||
Thermal Conductivity | 0.400 - 0.600 W/m-K | 2.78 - 4.16 BTU-in/hr-ft²-°F | ASTM E1461 |
Raschig Group DECAL® 1760 Phenolic Glass-fiber reinforced phenolic molding compound. Very good electrical properties, good chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals an.. |
|||
Thermal Conductivity | 0.400 - 0.600 W/m-K | 2.78 - 4.16 BTU-in/hr-ft²-°F | ASTM E1461 |
Raschig Group EPOXIDUR® 3585 EP Epoxy, Molded, Glass Fiber Filler Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures, excel.. |
|||
Thermal Conductivity | 0.400 - 0.500 W/m-K | 2.78 - 3.47 BTU-in/hr-ft²-°F | ASTM E1461 |
Raschig Group MELOPLAS® 3025 MF Cellulose-reinforced and inorganically filled MF molding compound in white and colored shades. High surface hardness, good UV and heat stability, very good resistance to chemicals - also to foodstu.. |
|||
Thermal Conductivity | 0.400 W/m-K | 2.78 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1301-7578 PPS, linear, with glass fiber and PTFE, improved wear resistance Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Thermal Conductivity | 0.400 W/m-K | 2.78 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1850/GF/30/TF/15/BK PBT, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Thermal Conductivity | 0.400 W/m-K | 2.78 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1-0784 Polyamide 66, with glass fiber and carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Thermal Conductivity | 0.400 W/m-K | 2.78 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1105-0779/WT PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High chemical resistance parts, hydrolysis resistance, non flammable.H.. |
|||
Thermal Conductivity | 0.400 W/m-K | 2.78 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1105-0923/GY2 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera.. |
|||
Thermal Conductivity | 0.400 W/m-K | 2.78 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1105-7128 PEEK, with glass fiber, low-warpage Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts.Not flammable.High continuos use temperature.High.. |
|||
Thermal Conductivity | 0.400 W/m-K | 2.78 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1105-0858 PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera.. |
|||
Thermal Conductivity | 0.400 W/m-K @Temperature 100 °C |
2.78 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1461 |
Plenco 7100 Phenolic, Nodular, Injection Molded PLENCO 07100 is an organic fiber reinforced phenolic molding compound, with improved mechanical strength properties and an industrial finish. 07100 is densified for easy handling and good pourabilit.. |
|||
Thermal Conductivity | 0.400 W/m-K @Temperature 121 °C |
2.78 BTU-in/hr-ft²-°F @Temperature 250 °F |
|
Tra-Con Tra-Bond Ablebond 933-1.5 Moisture Resistant Encapsulant TRA-BOND 933-1.5 electrically insulating epoxy encapsulant is formulated to provide a smooth crown over the device of wire bonds. This encapsulant provides protection from thermal and mechanical sho.. |
|||
Thermal Conductivity | 0.400 W/m-K | 2.78 BTU-in/hr-ft²-°F | DIN 52612 |
Total 3802 YCF MDPE pipe grade FINATHENE® 3802 Y CF is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Y CF is a yellow cadmi.. |
|||
Thermal Conductivity | 0.400 W/m-K | 2.78 BTU-in/hr-ft²-°F | |
Trelleborg Emerson & Cuming Stycast® 2057FR/11 Two-Component Epoxy Flame Retardant Encapsulant Features and Typical ApplicationsProvide flame resistance down to 1/8 of an inch. These products also offer various other features such as thermal shock protection, low viscosity, and thermal conduc.. |
|||
Thermal Conductivity | 0.400 W/m-K | 2.78 BTU-in/hr-ft²-°F | Product Property; ASTM E 1530 |
Arlon Thermabond® 48991A010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Generation IIa Thermabond® NP electrically insulating electronic adhesive. Bonds without primer.Design/Construction: Liner: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style .. |
|||
Thermal Conductivity | 0.400 W/m-K | 2.78 BTU-in/hr-ft²-°F | Silicone Property; ASTM E 1530 |
Arlon Thermabond® 48991A015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Thermabond® G2pr - electrically insulating electronic adhesive. Bonds without primer.Design/Construction: Liner: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1080 Fiberg.. |
|||
Thermal Conductivity | 0.400 W/m-K | 2.78 BTU-in/hr-ft²-°F | Average value: 0.400 W/m-K Grade Count:7 |
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max.. |
|||
Thermal Conductivity | 0.400 W/m-K @Temperature 80.0 °C |
2.78 BTU-in/hr-ft²-°F @Temperature 176 °F |
Z Direction; ASTM C518 |
Rogers Corporation 2929 Bondply Unreinforced, Hydrocarbon based Thin Film Adhesive System Low dielectric constant and loss tangentIdeal for multi-layer bondingCompatible with traditional processing methodsCompatible with a broad range of material types including PTFE compositesReliable t.. |