Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | |
Murtfeldt Murylon® A Nylon 66 This material combines the excellent properties of the Murylon® range with additional high tensile and compressive strength, increased wear resistance, and a lower level of moisture absorption than.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | |
Murtfeldt Murylon® B Nylon 6 Murylon® B natural has the best impact resistance of all Murylon materials. This material is especially suited for use in machine construction thanks to an excellent combination of mechanical prope.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | DIN.52612 |
Omnia Plastica Omniamid PA6 GHR HR - Dry Cast nylon 6 produced with the addition of graphite and a special lubricator which gives to this product better properties than natural PA6G. Whilst retaining the general features of OMNIAMID G it i.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | |
Quadrant EPP Ertalon® 6 SA PA 6, extruded (ISO Data) This material offers an optimal combination of mechanical strength, stiffness, toughness, mechanical damping properties and wear resistance. These properties, together with good electrical insulatin.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | |
Quadrant EPP Ertalon® 66 SA PA 66, extruded (ISO Data) Material with a higher mechanical strength, stiffness, heat and wear resistance than Ertalon 6 SA. It also has a better creep resistance but its impact strength and mechanical damping ability is red.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | |
Quadrant EPP Ertalon® LFX PA 6 + oil, cast (ISO Data) This internally lubricated cast nylon 6 is self-lubricating in the real meaning of the word. Ertalon LFX, especially developed for unlubricated, highly loaded and slow moving parts applications, yie.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | |
Quadrant EPP Nylatron® LFG PA 6 + oil, cast (ISO Data) Nylatron LFG (Lubricated Food Grade) is self-lubricating in the real meaning of the word, and has a FDA food contact compliant composition. The Nylatron LFG has been specially developed for non-lubr.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | DIN.52612 |
Omnia Plastica Akulon® PET Arnite Omnialite Arnite is a relatively new semi-crystalline polymer developed for technical applications. It is suitable for mechanical parts which require dimensional stability and a low friction coefficient. Omni.. |
|||
Thermal Conductivity | 0.280 - 1.10 W/m-K | 1.94 - 7.63 BTU-in/hr-ft²-°F | Average value: 0.500 W/m-K Grade Count:19 |
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor.. |
|||
Thermal Conductivity | 0.280 - 0.400 W/m-K | 1.94 - 2.78 BTU-in/hr-ft²-°F | Average value: 0.360 W/m-K Grade Count:3 |
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL V01550 PPE+HIPS (Europe-Africa-Middle East) NORYL V01550 is a 15 % short glass fibre reinforced, flame retardant material with a HDT/A of 130C according ISO 75. NORYL V01550 is V0 at 0.75 mm according UL94 and is halogen free according VDE/DI.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL V02570 PPE+HIPS (Asia Pacific) Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL V02570 PPE+HIPS (Europe-Africa-Middle East) Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM 2210 PEI (Europe-Africa-Middle East) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Ultem 2212 PEI (Europe-Africa-Middle East) 20% Milled glass filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Ultem 2412EPR PEI (Asia Pacific) 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the As.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire® AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This r.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Ultem PW2200 PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide (Tg 217°C). Product designed and certified for use in Potable Water
applications. KTW, WRAS, ACS certified. NSF61 and W270 pending. US FDA and.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL GFN3V PPE+HIPS (Europe-Africa-Middle East) NORYL GFN3V is a 30 % glass fibre reinforced material with a HDT/A of 145C according ISO 75. NORYL GFN3V has been approved for potable water applications up to 85C by the UK WFBS according BS 6920 i.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | DIN 52612 |
Zell-Metall Engineering Plastics Zellamid 1100 MO Improved sliding and self lubricating properties are achieved by the addition of molybdenum disulphide. UV-radiation resistance is enhanced.Color: blackApplications: For conveyor screws |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | DIN 52612 |
Zell-Metall Engineering Plastics Zellamid 1100 OIL at 50% RH Zellamid® 1100 OIL: A new type of cast nylon produced by addition of a special oil to the polymer structure. By laboratory test it was proven that this second generation oil filled product reduces .. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | DIN 52612 |
Zell-Metall Engineering Plastics Zellamid 1115 By special additives, impact strength and abrasion resistance are further improved. We particularly recommend this material for slipper pads for rolling mills.Color: IvoryApplications: slipper pads .. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | |
Chevron Phillips Xtel® XE3035NA Polyphenylene Sulfide Alloy Xtel® XE3035NA is a high performance, glass fiber reinforced, PPS based alloy developed to provide exceptionally high ductility and impact resistance along with good thermal stability.Information p.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | ASTM C 177 |
Adamas Adalon® 118 PTFE, 23/2% Carbon/Graphite Filled Information provided by Adamas, HPM |
|||
Thermal Conductivity | 0.280 - 0.360 W/m-K | 1.94 - 2.50 BTU-in/hr-ft²-°F | |
Arlon 0.008" (0.2032 mm) Thermabond® Uncured Silicone (99510N008) 0.008 in., ±0.001 (0.2 mm, ±0.03) uncured silicone on 0.003 in. (0.08 mm) nominal PTFE coated fiberglass; 0.001 in. (0.03 mm) FEP interleave; overall thickness 0.008 in ±0.001(0.2 mm ± 0.03). T.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | |
Arlon AD255A Glass, PTFE and Micro-Dispersed Ceramic Lower Loss and Improved Performance over Traditional AD Series.Information provided by Arlon Materials for Electronics (MED). |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® KR 4355 G7 BK 00564 35% Glass Filled PA6/6T (Conditioned) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | |
CENTROPLAST CENTROMID 6 GF 30 Polyamide 6 30% glass fiber The 30% glass fibre matrix adds very high strength and rigidity to this material. It has increased dimensional accuracy when hot. Can be used for rollers, belt pulleys and racks.Information provid.. |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | |
CENTROPLAST CENTROMID 6.6 FG Polyamide 6.6, Food Grade This material has good hardness, wear resistance, abrasion strength and impact strength.Information provided by CENTROPLAST Engineering Plastics GMBH |
|||
Thermal Conductivity | 0.280 W/m-K | 1.94 BTU-in/hr-ft²-°F | |
CENTROPLAST CENTROMID 6.6 Polyamide 6.6 This material has good hardness, wear resistance, abrasion strength and impact strength. It is used for bearing cages, sliding bearings and articulated joint blocks.Information provided by CENTROPL.. |