Arlon 0.008" (0.2032 mm) Thermabond® Uncured Silicone (99510N008)

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Elastomer, for Thermal Management
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 0.008" (0.2032 mm) Thermabond® Uncured Silicone (99510N008).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
0.008 in., ±0.001 (0.2 mm, ±0.03) uncured silicone on 0.003 in. (0.08 mm) nominal PTFE coated fiberglass; 0.001 in. (0.03 mm) FEP interleave; overall thickness 0.008 in ±0.001(0.2 mm ± 0.03). The shelf life is defined as the duration of time for which the product will meet the physical requirements outlined below. It does not guarantee the product’s usefulness in all applications. Color: Natural. Weight: 305.2 g/m² ± 33.9 (9.0 oz./yd.² ± 1.0). Shelf Life: 6 months . Thermal Impendence is 0.7°C/W, ±0.07 °C/W.Information provided by the manufacturer, Arlon Silicone Technologies Division.
Mechanical Properties Metric English Comments
Hardness, Shore A >= 50
>= 50
Tensile Strength, Ultimate 4.68 - 5.72 MPa
679 - 830 psi
Elongation at Break 250 - 300 %
250 - 300 %
Shear Modulus <= 0.000700 GPa
<= 0.102 ksi
Adhesive Bond Strength >= 2.80 MPa
>= 406 psi
lap shear strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.280 - 0.360 W/m-K
1.94 - 2.50 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -73.3 °C
-99.9 °F
Electrical Properties Metric English Comments
Dielectric Strength 14.0 kV/mm
356 kV/in
2.8 kV minimum
Processing Properties Metric English Comments
Processing Temperature 176.6 °C
349.9 °F
curing temp.