Material Notes:
Nylatron LFG (Lubricated Food Grade) is self-lubricating in the real meaning of the word, and has a FDA food contact compliant composition. The Nylatron LFG has been specially developed for non-lubricated, highly loaded and slowly moving parts in food contact applications. Compared to standard cast nylons, it offers lower maintenance costs and longer service life. High mechanical strength, stiffness, hardness and toughness Good fatigue resistance High mechanical damping ability Good sliding properties Excellent wear resistance Good electrical insulating properties Good resistance to high energy radiation (gamma- and X-rays) Good machinability
Physical Properties Metric English Comments
Density 1.135 g/cc
0.04100 lb/in³
ISO 1183-1
Moisture Absorption at Equilibrium 2.0 %
2.0 %
50% RH
Water Absorption at Saturation 6.3 %
6.3 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 82
82
ISO 2039-2
Hardness, Shore D 76
76
Ball Indentation Hardness 145 MPa
21000 psi
ISO 2039-1
Tensile Strength 73.0 MPa
10600 psi
at Yield; ISO 527-1/-2
Elongation at Break 25 %
25 %
ISO 527-1/-2
Elongation at Yield 5.0 %
5.0 %
ISO 527-1/-2
Tensile Modulus 3.00 GPa
435 ksi
ISO 527-1/-2
Flexural Strength 107 MPa
15500 psi
Flexural Modulus 3.00 GPa
435 ksi
Compressive Strength 31.0 MPa

@Strain 1 %
4500 psi

@Strain 1 %
ISO 604
58.0 MPa

@Strain 2 %
8410 psi

@Strain 2 %
ISO 604
85.0 MPa

@Strain 5 %
12300 psi

@Strain 5 %
ISO 604
K Factor (ISO) 6.0 µm/km
6.0 µm/km
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
ISO 179-1/1eU
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.22 - 0.35
0.22 - 0.35
Limiting Pressure Velocity 0.0800 MPa-m/sec
2280 psi-ft/min
at 1 m/s unlubricated
0.130 MPa-m/sec
3710 psi-ft/min
at 0.1 m/s unlubricated
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C

@Temperature 23.0 - 100 °C
50.0 µin/in-°F

@Temperature 73.4 - 212 °F
Thermal Conductivity 0.280 W/m-K
1.94 BTU-in/hr-ft²-°F
Melting Point 215 °C
419 °F
DSC, 10°C/min.; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 °C
194 °F
Continuous; 20,000 h
105 °C
221 °F
Continuous; 5,000 h
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity >= 1.0e+14 ohm-cm
>= 1.0e+14 ohm-cm
IEC 60093
Surface Resistivity per Square >= 1.0e+13 ohm
>= 1.0e+13 ohm
IEC 60093
Dielectric Constant 3.5

@Frequency >=100000 Hz
3.5

@Frequency >=100000 Hz
IEC 60250
Dielectric Strength 22.0 kV/mm
559 kV/in
Dissipation Factor 0.015

@Frequency 100000 Hz
0.015

@Frequency 100000 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112
Compliance Properties Metric English Comments
3A-Dairy No
No
European Food 1935/2004 No
No
FDA Yes
Yes
natural and blue
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Unacceptable
Unacceptable
Acids, Weak Limited
Limited
Alcohols Limited
Limited
Alkalies, Strong (pH 11-14) Unacceptable
Unacceptable
Alkalies, Weak Limited
Limited
Chlorinated Solvents Limited
Limited
Continuous Sunlight Limited
Limited
Hot Water / Steam Limited
Limited
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Acceptable
Acceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Acceptable
Acceptable