Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | |
Resinlab® EP1112 Clear Electronic Grade Epoxy Encapsulant Resinlab™ EP 1112 Clear is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexib.. |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | ISO 8302 |
Polimeri Europa Edistir RT 441M Polystyrene High impact polystyrene combining high toughness and high stiffness with good flowability for easy processing. Designed for injection moulding of technical parts, housings and covers.
Especially rec.. |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | ASTM C 177 |
Polimeri Europa Sinkral® E 332 ABS Resin Sinkral E 332 is a medium heat injection molding grade offering good flow and good impact resistance together with an excellent thermal stability during processing. Designation: Thermoplastic ISO 2.. |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | ASTM C 177 |
Polimeri Europa Sinkral® F 332 ABS Resin Sinkral F 332 is a general purpose injection molding grade which combines excellent thermal stability during processing with a good balance between flow and impact characteristics. Designation: Ther.. |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | ASTM E 1530 |
SABIC Innovative Plastics LNP COLORCOMP D1000FH PC (Asia Pacific) LNP COLORCOMP* D1000FH is a compound based on Polycarbonate resin containing Unfilled Custom Color. Added features of this material include: Low Extractible. |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | ASTM C 177 |
Polimeri Europa Sinkral® D 232/M3 ABS Resin
(discontinued **) Special low gloss extrusion/ co-extrusion grade, with good flow. Designation: Thermoplastic ISO 2580-ABS 1, EGN, 105-08-09-15Applications: Sinkral D 232-M3 is widely used in the extrusion / co-extr.. |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | DOM 52612 |
Manifattura Cattaneo PVC U Polyvinyl Chloride Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | DIN 52612 |
Isoflon PVDF Polyvinyl Dichloride Fluoropolymer Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | DIN 52612-1 |
Styrolution Luran® 378 P Crystal Clear Transparent SAN Description: Easy-flow grade with enhanced resistance to chemicals.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | DIN 52612-1 |
Styrolution Luran® HD 20 SAN Luran HD 20 is an easy-flow grade of SAN especially designed for the medical market. It is suitable for moldings with very thin walls and / or adverse flow length to wall ratio. It features very goo.. |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | DIN 52612-1 |
Styrolution Luran® HH-120 Alpha-Methylstyrene Acrylonitrile Luran HH-120 is a grade of AMSAN with high heat resistance and improved mechanical strength. It is suitable for injection molding and extrusion applications and can be used as a modifier for high he.. |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | DIN 52612-1 |
Styrolution Luran® S 776 S Colored ASA Description: Injection molding grade with good toughness and strength. Uses include parts for garden equipment, parts for office chairs and antennas.Information provided by STYROLUTION, which is a j.. |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | DIN 52612-1 |
Styrolution Luran® S KR 2863 C Colored ASA+PC Description: Grade with very high heat resistance for automotive interiors and exteriors as well as electrical parts.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | DIN 52612-1 |
Styrolution Luran® S KR 2864 C Colored ASA+PC Description: Easy flowing injection molding grade with heat resistance for parts with thin walls and/or with adverse flowpath/wall thickness ratios.Applications: Mobile phone housings.Information pr.. |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | DIN 52612-1 |
Styrolution PS 165 N/L GPPS Styrolution PS 165N/L is a high molecular weight, good flowing grade, often blended with high impact extrusion grades.High molecular weightGood flow characteristicsAppropriate for blending with HIPS.. |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | DIN 52612-1 |
Styrolution Terluran® HI-12 ABS Terluran HI-12 is an injection molding grade of ABS with a very high toughness and easy flow.Very high toughnessEasy flowingUL 94 HB (1.6 & 3.2 mm)Information provided by Styrolution |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | DIN 52612-1 |
Styrolution Terluran® SP-6 ABS Description: High impact grade, suitable for extrusion.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 307A4000015 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 360E0096914 Cellulose Acetate Propionate, Natural, Trsp Applications:ProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 360E3V45512 Propionate Water Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 380A3V32818 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 383A2R30010 Cellulose Acetate Propionate, Natural, Trsp Applications:Oral HygienePlastics for hygiene feminine productsRecreationalToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughne.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 485E3720008 Cellulose Acetate Butyrate, Clear, Trsp Applications:Toys/Sporting goodsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties including toughness, hardness, strength, surface gloss, clarity,.. |
|||
Thermal Conductivity | 0.170 - 0.330 W/m-K | 1.18 - 2.29 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Tenite 550E3V45510 Cellulose Acetate Butyrate, Water Clear, Trsp Applications:AppliancesConsumer-Personal careProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gl.. |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | Melt |
Covestro Bayblend® FR 3030 Polycarbonate + ABS, Flame Retardant Grade Flame retardant extrusion gradeVicat/B 120 temperature = 115 °Cgood extrusion and vacuum-forming behaviourUL-listing 94 V-0 (1.5 mm)halogen-free according to DIN VDE 0472-815glow wire temperature (.. |
|||
Thermal Conductivity | 0.170 - 0.190 W/m-K | 1.18 - 1.32 BTU-in/hr-ft²-°F | ASTM D433 |
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | |
CENTROPLAST CENTROLEN PPS Polypropylene flame resistant This material is a low density, easily machined plastic that can be welded and is flame resistant. Applications include exhaust systems for heating systems, and apparatus engineering.Information pr.. |
|||
Thermal Conductivity | 0.170 - 0.190 W/m-K | 1.18 - 1.32 BTU-in/hr-ft²-°F | ASTM D433 |
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Thermal Conductivity | 0.170 - 0.190 W/m-K | 1.18 - 1.32 BTU-in/hr-ft²-°F | ASTM D433 |
Arkema Group KYNAR® 460 Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Broad molecular weight distribution, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, .. |
|||
Thermal Conductivity | 0.170 - 0.190 W/m-K @Temperature 50.0 - 200 °C |
1.18 - 1.32 BTU-in/hr-ft²-°F @Temperature 122 - 392 °F |
Average value: 0.180 W/m-K Grade Count:4 |
Overview of materials for Thermoset Fluoroelastomer This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Fluoroelastomer". Each property range of values reported is minimum and maximum values of appr.. |