Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.500 - 0.700 W/m-K | 3.47 - 4.86 BTU-in/hr-ft²-°F | ASTM E1461 |
Raschig Group 3536 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed.. |
|||
Thermal Conductivity | 0.500 - 0.600 W/m-K | 3.47 - 4.16 BTU-in/hr-ft²-°F | DIN 52 612 |
Raschig Group AMPLA® 7250 melamine-modified polyester Cellulose reinforced melamine-modified Polyester molding compound. Very good electrical values, excellent heat resistance, excellent surface quality, low post shrinkage. This product meets the allow.. |
|||
Thermal Conductivity | 0.500 W/m-K | 3.47 BTU-in/hr-ft²-°F | |
Resinlab® EP1295 Black Medium Viscosity, Halogen Free, Flame Retardant Epoxy Casting Resin Resinlab™ EP1295 Black is a medium viscosity, halogen free, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (.. |
|||
Thermal Conductivity | 0.500 W/m-K | 3.47 BTU-in/hr-ft²-°F | |
Resinlab® EP1340 Medium Viscosity, Flame Retardant Epoxy Casting Resin System Resinlab™ EP1340 is a medium viscosity, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File# E186034) for U.. |
|||
Thermal Conductivity | 0.500 W/m-K @Temperature 80.0 °C |
3.47 BTU-in/hr-ft²-°F @Temperature 176 °F |
ASTM C518 |
Rogers Corporation RO3035 Ceramic-Filled PTFE Composite, High Frequency Circuit Material Features and Benefits:Low dielectric lossExcellent mechanical properties versus temperature - reliable stripline and multi-layer board constructions.Uniform mechanical properties- ideal for multi-la.. |
|||
Thermal Conductivity | 0.500 - 0.600 W/m-K | 3.47 - 4.16 BTU-in/hr-ft²-°F | ASTM E1461 |
Raschig Group RALUPOL® 8601 UP Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic moulding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical stren.. |
|||
Thermal Conductivity | 0.500 - 0.600 W/m-K | 3.47 - 4.16 BTU-in/hr-ft²-°F | ASTM E1461 |
Raschig Group RALUPOL® 8602 UP Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic molding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical streng.. |
|||
Thermal Conductivity | 0.500 W/m-K | 3.47 BTU-in/hr-ft²-°F | HOT-DISK || 60x60x3 mm |
Lehmann & Voss LUVOCOM® 1106-7843 Polyether imide, with glass fiber, PTFE, lubricant modified, easy flowing Applications: Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Information provided by Lehmann & Voss & Co.KG |
|||
Thermal Conductivity | 0.500 W/m-K | 3.47 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 7/CF/30/BK Polyamide 610, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Especially suitable at dynamic.. |
|||
Thermal Conductivity | 0.500 W/m-K | 3.47 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 8-7190 High impact polyamide, with carbon fiber, toughness-modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Especially suitable at dynamic.. |
|||
Thermal Conductivity | >= 0.500 W/m-K | >= 3.47 BTU-in/hr-ft²-°F | DIN 52612 |
Fluorseals PTFE Unfilled Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials. |
|||
Thermal Conductivity | 0.500 W/m-K | 3.47 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1/XCF/20 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Thermal Conductivity | 0.500 W/m-K | 3.47 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1/XCF/30 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Thermal Conductivity | 0.500 W/m-K | 3.47 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1/XCF/25 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Thermal Conductivity | 0.500 W/m-K @Temperature 90.0 °C |
3.47 BTU-in/hr-ft²-°F @Temperature 194 °F |
|
Schott Glass 8650 Sealing Glass Sealing glass for molybdenum, free from Na and K, of high lead content Implosion diodesInformation provided by SCHOTT AG. |
|||
Thermal Conductivity | 0.500 - 7.00 W/m-K | 3.47 - 48.6 BTU-in/hr-ft²-°F | |
Goodfellow Potassium Aluminosilicate (Muscovite Mica) Mica is a naturally occurring mineral and as such its exact composition varies between grades, as will its properties. Ruby Mica is the highest grade of Muscovite Mica. The name comes from the Latin.. |
|||
Thermal Conductivity | 0.500 W/m-K @Temperature 121 °C |
3.47 BTU-in/hr-ft²-°F @Temperature 250 °F |
|
Tra-Con Tra-Bond 77-2LTC Low Temperature Cure SMD Adhesive TRA-BOND 77-2LTC one component, solvent-free, insulative epoxy adhesive is designed to cure at temperatures as low as 80°C. This adhesive is specifically designed for attaching surface mounted devi.. |
|||
Thermal Conductivity | 0.500 W/m-K | 3.47 BTU-in/hr-ft²-°F | |
Tra-Con Tra-Cast 3103 General Purpose Epoxy Casting Compound TRA-CAST 3103 is a low viscosity two-part formulation recommended for general purpose electrical potting and encapsulating application where the combination of good mechanical thermal and electrical.. |
|||
Thermal Conductivity | 0.500 W/m-K @Temperature 100 °C |
3.47 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1461 |
Plenco 4311 Phenolic, Granular, Compression Molded PLENCO 04311 is a heat resistant, mineral filled phenolic molding compound offering excellent processability, mechanical strength, and improved cold powder pourability characteristics. UL recognized.. |
|||
Thermal Conductivity | 0.500 W/m-K | 3.47 BTU-in/hr-ft²-°F | MIL STD 883D |
CoorsTek Epoxy Seal 216 (ES-216) B-staged epoxy lids ES-216 is available for applications where high strength and moisture resistance are required. It displays fillet formation characteristics and, after cure, is highly temperature and moisture resist.. |
|||
Thermal Conductivity | 0.500 W/m-K @Temperature 100 °C |
3.47 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1225 |
Arlon CLTE-P Pre-Preg Bonding Layer Arlon's CLTE-P Prepreg Bonding Layer is a ceramic filled PTFE coated glass stock that is used as a bonding ply for CLTE, CLTE-X or CLTE-AT laminates. CLTE-P is a pre-preg material that consists of .. |
|||
Thermal Conductivity | 0.500 - 0.600 W/m-K | 3.47 - 4.16 BTU-in/hr-ft²-°F | ASTM E1461 |
Raschig Group MELOPLAS® 180 MF Wood flour-reinforced, phenol-modified MF molding compound (MPF) in dark colors. High surface hardness, good mechanical strength and electrical properties, good heat resistance. Self-extinguishing .. |
|||
Thermal Conductivity | 0.500 W/m-K | 3.47 BTU-in/hr-ft²-°F | ISO 8302 |
Solvay Specialty Polymers Primef® 4002 40% GF PPS, High Fluidity Grade
(discontinued **) Used for injection molding of high performance parts. |
|||
Thermal Conductivity | 0.500 W/m-K | 3.47 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1105-7251 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera.. |
|||
Thermal Conductivity | 0.500 W/m-K | 3.47 BTU-in/hr-ft²-°F | |
Resinlab® EP1240RC Flame Retardant Epoxy Casting Resin Resinlab™ EP1240RC is a medium viscosity, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File# E186034, Pro.. |