Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 60.0 - 100 µm/m-°C @Temperature 20.0 °C |
33.3 - 55.6 µin/in-°F @Temperature 68.0 °F |
DN.53752 |
Polimersan Plastics POLIPA® (PA 6) Polyamide POLIPA® PA6 (POLYAMIDE) is produced by poly condensation of e-aminoacid and by the help of d-carbon acid and d-amine poly condensation. Its characteristics depend upon the numbers of the main struc.. |
|||
CTE, linear | 80.0 - 100 µm/m-°C | 44.4 - 55.6 µin/in-°F | Polykemi |
Polykemi AB POLYfill PP CQX8025 R2 Polypropylene, Mineral Reinforced, Scratch Resistant Information provided by Polykemi AB |
|||
CTE, linear | 50.0 - 100 µm/m-°C @Temperature 20.0 °C |
27.8 - 55.6 µin/in-°F @Temperature 68.0 °F |
Cured |
Resin Technology Group EN 239-2 Cationic UV Cure Epoxy Adhesive EN 239-2 is an epoxy-based, medium viscosity, cationic- curable adhesive/sealant. This product is activated by exposure to medium intensity UV radiation resulting in a high strength, chemical resist.. |
|||
CTE, linear | 23.0 - 100 µm/m-°C @Temperature >=162 °C |
12.8 - 55.6 µin/in-°F @Temperature >=324 °F |
Average value: 61.5 µm/m-°C Grade Count:1 |
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled". Each property range of values reported i.. |
|||
CTE, linear | 60.0 - 100 µm/m-°C @Temperature 20.0 °C |
33.3 - 55.6 µin/in-°F @Temperature 68.0 °F |
DN.53752 |
Polimersan Plastics POLIPA® (PA 6) Polyamide POLIPA® PA6 (POLYAMIDE) is produced by poly condensation of e-aminoacid and by the help of d-carbon acid and d-amine poly condensation. Its characteristics depend upon the numbers of the main struc.. |
|||
CTE, linear | 50.0 - 100 µm/m-°C | 27.8 - 55.6 µin/in-°F | Average value: 68.4 µm/m-°C Grade Count:25 |
Overview of materials for Polyphenylene Ether, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap.. |
|||
CTE, linear | 30.0 - 100 µm/m-°C | 16.7 - 55.6 µin/in-°F | Average value: 58.6 µm/m-°C Grade Count:15 |
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar.. |
|||
CTE, linear | 48.6 - 100 µm/m-°C | 27.0 - 55.6 µin/in-°F | Average value: 77.2 µm/m-°C Grade Count:10 |
Overview of materials for Polypropylene with 30% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are.. |
|||
CTE, linear | 42.0 - 100 µm/m-°C | 23.3 - 55.6 µin/in-°F | Average value: 59.5 µm/m-°C Grade Count:9 |
Overview of materials for Nylon 6, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ.. |
|||
CTE, linear | 10.0 - 100 µm/m-°C | 5.56 - 55.6 µin/in-°F | Average value: 70.9 µm/m-°C Grade Count:42 |
Overview of materials for Nylon 66, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum .. |
|||
CTE, linear | 10.0 - 100 µm/m-°C | 5.56 - 55.6 µin/in-°F | Average value: 63.3 µm/m-°C Grade Count:8 |
Overview of materials for Nylon 66, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Extruded". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
CTE, linear | 65.0 - 100 µm/m-°C | 36.1 - 55.6 µin/in-°F | ASTM D696 |
Guarniflon PTFE G455 Polytetrafluoroethylene 35% Carbographite PTFE G Special Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high w.. |
|||
CTE, linear | 80.0 - 100 µm/m-°C | 44.4 - 55.6 µin/in-°F | 25°C to 100°C; ASTM D696 |
Guarniflon FEP Fluorinated Ethylene Propylene Fluorinated thermoplastic material with excellent thermal, electrical and chemical inertness properties. Widely used for different industrial applications for its excellent chemical resistance up t.. |
|||
CTE, linear | 70.0 - 100 µm/m-°C @Temperature 20.0 - 100 °C |
38.9 - 55.6 µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
Schwartz Technical Plastics LAMIGAMID® 100 Polyamide 6, Extruded, Conditioned Application: machine parts under 80 mm diameter, hammer-heads, cup-shaped bearing shellsInformation provided by Schwartz Technical Plastics GmbH |
|||
CTE, linear | 70.0 - 100 µm/m-°C @Temperature 20.0 - 100 °C |
38.9 - 55.6 µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
Schwartz Technical Plastics LAMIGAMID® 100 Polyamide 6, Extruded, Dry Application: machine parts under 80 mm diameter, hammer-heads, cup-shaped bearing shellsInformation provided by Schwartz Technical Plastics GmbH |
|||
CTE, linear | 80.0 - 100 µm/m-°C @Temperature 20.0 - 100 °C |
44.4 - 55.6 µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
Schwartz Technical Plastics LAMIGAMID® 1200 Cast Polyamide 12, Dry Application: sprockets, chain-wheels, pulleys, wheels, slide and seal rings, curve disks, etc.Information provided by Schwartz Technical Plastics GmbH |
|||
CTE, linear | 80.0 - 100 µm/m-°C | 44.4 - 55.6 µin/in-°F | ISO 11359 |
Styrolution Luran® S KR2866C ASA / PC Luran S KR2866C is a blend of ASA and PC with a reduced content of PC. It is characterized by a medium impact toughness and heat resistance.Good heat resistanceMedium impact strengthInformation prov.. |
|||
CTE, linear | 80.0 - 100 µm/m-°C | 44.4 - 55.6 µin/in-°F | ISO 11359 |
Styrolution Novodur® BX13036 ABS + PMMA Novodur BX13036 is a new PMMA/ABS blend with high surface quality, enhanced scratch resistance and balanced mechanical propertiesInformation provided by Styrolution |
|||
CTE, linear | 80.0 - 100 µm/m-°C @Temperature -30.0 - 30.0 °C |
44.4 - 55.6 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics NORYL GTX GTX6011 PPE+PA6 (Asia Pacific) PA6 based unfilled GTX. High impact. |
|||
CTE, linear | 70.0 - 100 µm/m-°C @Temperature 20.0 °C |
38.9 - 55.6 µin/in-°F @Temperature 68.0 °F |
DIN 53752 |
Zell-Metall Engineering Plastics Zellamid 250 (PA6.6) Zellamid® 250 is noted for its high temperature resistance and high tensile strength. It is the hardest and most rigid type of extruded Nylon. Main characteristics are high resistance to fuels, oil.. |
|||
CTE, linear | 30.0 - 100 µm/m-°C | 16.7 - 55.6 µin/in-°F | Average value: 73.7 µm/m-°C Grade Count:34 |
Overview of materials for Nylon 6, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v.. |
|||
CTE, linear | 52.2 - 100 µm/m-°C | 29.0 - 55.6 µin/in-°F | Average value: 70.1 µm/m-°C Grade Count:4 |
Overview of materials for Nylon 66, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu.. |
|||
CTE, linear | 80.0 - 100 µm/m-°C | 44.4 - 55.6 µin/in-°F | Average value: 90.0 µm/m-°C Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum.. |
|||
CTE, linear | 100 - 100 µm/m-°C @Temperature -90.0 - -30.0 °C |
55.6 - 55.6 µin/in-°F @Temperature -130 - -22.0 °F |
Average value: 100 µm/m-°C Grade Count:1 |
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Crosslinkable". Each property range of values reported is minimum and .. |
|||
CTE, linear | 70.0 - 100 µm/m-°C | 38.9 - 55.6 µin/in-°F | Average value: 81.3 µm/m-°C Grade Count:16 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
CTE, linear | 10.0 - 100 µm/m-°C @Temperature -100 - 250 °C |
5.56 - 55.6 µin/in-°F @Temperature -148 - 482 °F |
Average value: 21.2 µm/m-°C Grade Count:23 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a.. |
|||
CTE, linear | 7.00 - 100 µm/m-°C @Temperature 55.0 - 250 °C |
3.89 - 55.6 µin/in-°F @Temperature 131 - 482 °F |
Average value: 20.4 µm/m-°C Grade Count:19 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |
|||
CTE, linear | 72.0 - 100 µm/m-°C | 40.0 - 55.6 µin/in-°F | Average value: 88.4 µm/m-°C Grade Count:7 |
Overview of materials for Acrylic, Gamma Radiation Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Gamma Radiation Resistant, Molded". Each property range of values reported is minimum and maxim.. |
|||
CTE, linear | 100 - 100 µm/m-°C @Temperature 100 - 100 °C |
55.6 - 55.6 µin/in-°F @Temperature 212 - 212 °F |
Average value: 100 µm/m-°C Grade Count:1 |
Overview of materials for Polypropylene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of.. |