Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 81.0 µm/m-°C @Temperature -40.0 - 149 °C |
45.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP Ertalyte® TX Internally Lubricated Semi-Crystalline Polyester (ASTM Product Data Sheet) |
|||
CTE, linear | 81.0 µm/m-°C @Temperature 20.0 °C |
45.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
PolyOne Edgetek® PS-1000 Polybutylene Terephthalate (PBT)
(discontinued **) Description/Features:UL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
CTE, linear | 81.0 µm/m-°C @Temperature -40.0 - 300 °C |
45.0 µin/in-°F @Temperature -40.0 - 572 °F |
ASTM E831 |
Quadrant EPP Semitron® CMP LL5 Polyester (ASTM Product Data Sheet) Enhanced semi-crystalline polyester product for extended service in CMP retaining rings. Superior performance, especially in oxide processes, and cost effective relative to standard ring materials. .. |
|||
CTE, linear | 81.0 µm/m-°C @Temperature 20.0 °C |
45.0 µin/in-°F @Temperature 68.0 °F |
ASTM data |
BASF Capron® 1202CQ Nylon 6 (Dry)
(discontinued **) Capron 1202CQ is a blended low viscosity, polyamide 6 injection molding homopolymer, possessing a modified crystalline structure for increased property performance and faster cycles. It is also ava.. |
|||
CTE, linear | 81.0 µm/m-°C @Temperature 20.0 °C |
45.0 µin/in-°F @Temperature 68.0 °F |
ASTM data |
BASF Capron® 8203C Nylon 6 (Dry)
(discontinued **) Capron 8203C is a high viscosity, nylon 6 extrusion compound, possessing a modified crystalline structure for increased property performance and faster set up for tubing and cable applications. It.. |
|||
CTE, linear | 81.0 µm/m-°C | 45.0 µin/in-°F | ASTM-D696 |
Ineos ABS Lustran® ABS 248FC Medical & Food Contact Grade Lustran® ABS 248FC resin is a high-gloss, medium-impact grade of ABS (acrylonitrile butadiene styrene). This injection molding grade offers a good balance of physical properties and has been desi.. |
|||
CTE, linear | 81.0 µm/m-°C | 45.0 µin/in-°F | ASTM-D696 |
Ineos ABS Lustran® ABS 349 Lustran® ABS 349 is a high-gloss, medium-impact injection molding resin that has been specially formulated for excellent surface lubricity using internal additives. |
|||
CTE, linear | 81.0 µm/m-°C @Temperature 20.0 °C |
45.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Acrylloy 7 Acrylic Sheet Description: Acrylic SheetInformation provided by Spartech. |
|||
CTE, linear | 81.0 µm/m-°C @Temperature 20.0 °C |
45.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Korad® SP-2011 Cap/HIPS Polystyrene Sheet Description: Polystyrene SheetKorad is a registered trademark of Polymer Extruded Products, Inc..Information provided by Spartech. |
|||
CTE, linear | 81.0 µm/m-°C @Temperature 20.0 °C |
45.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Litho SP-2090 Polystyrene Sheet Description: Polystyrene SheetInformation provided by Spartech. |
|||
CTE, linear | 81.0 µm/m-°C @Temperature 20.0 °C |
45.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Royalite R522 PVC Alloy Aircraft Grade Sheet Description: Aircraft Grade SheetInformation provided by Spartech. |
|||
CTE, linear | 81.0 µm/m-°C @Temperature 20.0 °C |
45.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Royalite R60 PVC/Acrylic Aircraft Grade Sheet Description: Aircraft Grade SheetInformation provided by Spartech. |
|||
CTE, linear | 81.0 µm/m-°C @Temperature 20.0 °C |
45.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Royalite R722 PVC Alloy Aircraft Grade Sheet Description: Aircraft Grade SheetInformation provided by Spartech. |
|||
CTE, linear | 81.0 µm/m-°C @Temperature 20.0 °C |
45.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech SP-2010 HIPS Polystyrene Sheet Description: Polystyrene SheetInformation provided by Spartech. |
|||
CTE, linear | 81.0 µm/m-°C @Temperature 20.0 °C |
45.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech SP-2050 Glossy HIPS Polystyrene Sheet Description: Polystyrene SheetInformation provided by Spartech. |
|||
CTE, linear | 81.0 µm/m-°C @Temperature 20.0 °C |
45.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Tuf-Glas Impact Modified Acrylic Sign Grade Sheet Description: Sign Grade SheetInformation provided by Spartech. |
|||
CTE, linear | 81.0 µm/m-°C @Temperature 20.0 °C |
45.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Techmer ES Plaslube® NY-1/SI/2 WT PA66 |
|||
CTE, linear | 81.0 - 110 µm/m-°C @Temperature 20.0 °C |
45.0 - 61.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Westlake Plastics Pomalux® Acetal Copolymer For Medical Applications Medical grade Pomalux is made from acetal copolymer resin which allows machined products the ability to retain dimensional integrity, maintain stability in water and most chemicals at elevated tempe.. |
|||
CTE, linear | 81.0 µm/m-°C @Temperature 20.0 °C |
45.0 µin/in-°F @Temperature 68.0 °F |
ASTM D1525 |
Lubrizol Isoplast® 101 Engineering Thermoplastic Polyurethane Resin ISOPLAST® 101 is an engineering thermoplastic polyurethane resin.Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product li.. |
|||
CTE, linear | 81.0 µm/m-°C @Temperature 20.0 °C |
45.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Ensinger Tecamid® 6/6 Nylon (PA66) Type 6/6 is a general purpose standard grade nylon. Extruded in natural and black. (Weather Resistant Black Grade is also available.)Information provided by Ensinger, Inc. |
|||
CTE, linear | 81.0 µm/m-°C @Temperature 20.0 °C |
45.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Cast Nylons Nycast® 6MPB Plasticized Nylon 6 A plasticized Type 6 material, NYCAST® 6MPB is formulated for use as pile driver caps or cushion pads. Data provided by the manufacturer, Cast Nylons Limited.The data below are average values prese.. |
|||
CTE, linear | 81.0 µm/m-°C @Temperature 20.0 °C |
45.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Cast Nylons Nycast® 6MPY Plasticized Nylon 6 A plasticized Type 6 material, NYCAST® 6MPY is formulated for use as pile driver caps or cushion pads. Data provided by the manufacturer, Cast Nylons Limited.The data below are average values prese.. |
|||
CTE, linear | 81.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
45.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM Test |
BASF Ultramid® 8202C HS BK-102 PA6 (Dry) Ultramid 8202C HS BK-102 is a heat stabilized, low viscosity, pigmented black, PA6, injection molding homopolymer possessing a modified crystalline structure for increased property performance and f.. |
|||
CTE, linear | 81.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
45.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM Test |
BASF Ultramid® 8202C PA6 (Dry) Ultramid 8202C is a modified crystalline and low viscosity, nylon 6 injection molding homopolymer. It is also available in heat stabilized (Ultamid 8202C HS) and/or pigmented versions. Its unique .. |
|||
CTE, linear | 81.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
45.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM Test |
BASF Ultramid® 8202CQ PA6 (Dry) Ultramid 8202CQ is a low viscosity, PA6 injection molding homopolymer, possessing a modified crystalline structure or increased property performance and faster cycles. It is also available in pigme.. |
|||
CTE, linear | 81.0 µm/m-°C @Temperature 20.0 °C |
45.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Cast Nylons Nycast® XHA Heat Stabilized Nylon 6 Heat stabilized Cast Nylon 6 adds up to 20 degrees F higher continuous operation temperature for those applications that require additional temperature resistance beyond the standard resistance. Dat.. |
|||
CTE, linear | 81.0 µm/m-°C @Temperature 20.0 °C |
45.0 µin/in-°F @Temperature 68.0 °F |
ASTM data |
BASF Capron® 8202C HS Nylon 6 (Dry)
(discontinued **) Capron 8202C HS is a heat stabilized, low viscosity, polyamide 6 injection molding homopolymer possessing a modified crystalline structure for increased property performance and faster cycles. It i.. |
|||
CTE, linear | 81.0 µm/m-°C @Temperature 20.0 °C |
45.0 µin/in-°F @Temperature 68.0 °F |
ASTM data |
BASF Capron® 8203C HS Blend Nylon 6 (Dry)
(discontinued **) Capron 8203C HS Blend is a heat stabilized, high viscosity nylon 6 extrusion compound possessing a modified crystalline structure for increased strength, stiffness and heat distortion temperature. .. |
|||
CTE, linear | 81.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
45.0 µin/in-°F @Temperature -40.0 - 180 °F |
|
Ascend Performance Materials VYDYNE® 21SP Nylon, General Purpose 1.4% Deformation under 14 MPa (2000 psi) load.Typical property data. VYDYNE is a registered trademark of Solutia Inc. |