Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Spartech Korad® SP-2011 Cap/HIPS Polystyrene Sheet

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Spartech
Trade Name Korad®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech Korad® SP-2011 Cap/HIPS Polystyrene Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Polystyrene SheetKorad is a registered trademark of Polymer Extruded Products, Inc..Information provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 99
99
ASTM D785
Tensile Strength, Yield 24.1 MPa
3500 psi
ASTM D638
Tensile Modulus 1.86 GPa
270 ksi
ASTM D638
Flexural Yield Strength 48.3 MPa
7000 psi
ASTM D790
Flexural Modulus 2.14 GPa
310 ksi
ASTM D790
Izod Impact, Unnotched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Falling Dart Impact 9.60 J
7.08 ft-lb
73°F; ASTM D3029
Thermal Properties Metric English Comments
CTE, linear 81.0 µm/m-°C

@Temperature 20.0 °C
45.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
ASTM D648
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Gloss 86 %
86 %
Gardner; ASTM D2523