Techmer ES Plaslube® NY-1/SI/2 WT PA66

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Techmer ES
Trade Name Plaslube®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Plaslube® NY-1/SI/2 WT PA66.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Water Absorption 1.0 %
1.0 %
24 Hrs; ASTM D570
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 119
119
ASTM D785
Tensile Strength at Break 74.5 MPa
10800 psi
ASTM D638
Elongation at Break 4.5 %
4.5 %
ASTM D638
Flexural Strength 100 MPa
14500 psi
ASTM D790
Flexural Modulus 2.76 GPa
400 ksi
ASTM D790
Compressive Strength 89.6 MPa
13000 psi
ASTM D695
Izod Impact, Notched 0.801 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 81.0 µm/m-°C

@Temperature 20.0 °C
45.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 79.4 °C
175 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.59 mm
HB

@Thickness 0.0625 in