Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 70.0 µm/m-°C | 38.9 µin/in-°F | ASTM D-696 |
Plaskolite Optix® CP - 924 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
CTE, linear | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
ASTM D 696 |
Polimeri Europa Edistir N 2380 Polystyrene High molecular weight general purpose polystyrene combining high heat resistance and good mechanical strength. Suitable for direct gassing extrusion, for biaxially oriented films and sheets, for gla.. |
|||
CTE, linear | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
ISO 11359-2 |
Polycasa CAST PMMA QUINN CAST has an optical transparency of 93% light transmission for transparent sheets. It is significantly lighter and much more impact resistant than glass of equivalent thickness. QUINN CAST is .. |
|||
CTE, linear | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Covestro Apec® DP9-9371 High-Heat Polycarbonate, General Purpose
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
CTE, linear | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Covestro Apec® DP9-9373 High-Heat Polycarbonate, General Purpose, UV-Stabilized
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
CTE, linear | 70.0 µm/m-°C | 38.9 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 50/TF/15/BK-1 Polycarbonate, with PTFE, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
CTE, linear | 70.0 µm/m-°C | 38.9 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 50/TF/15/GY77 Polycarbonate, with PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
CTE, linear | 70.0 µm/m-°C | 38.9 µin/in-°F | ASTM D696 |
Kolon KOPA® KN3322V0Y Flame Retardant Nylon 66 Halogen free, Impact -resistantApplications A variety of connectorsInformation provided by API-Kolon. |
|||
CTE, linear | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
DIN 53752; ASTM D696 |
Kolon KOPA® KN3322VO Flame Retardant Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
CTE, linear | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
DIN 53752; ASTM D696 |
Kolon KOPA® KN331F General Purpose Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
CTE, linear | 70.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
38.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
LyondellBasell Astryn BA36GC Polypropylene Copolymer Key Features: conventional melt flow, medium modulus, UV-stabilized polypropylene copolymer, moderate stiffness, good impact resistance, low foggingApplications: seat valances, passenger assist hand.. |
|||
CTE, linear | 70.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
38.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics NORYL SE100P PPE+HIPS (Asia Pacific) |
|||
CTE, linear | 70.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
38.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics NORYL TPN9221 PPE+PS (Asia Pacific) Transparent Noryl grade with 90dc and V-2 FR |
|||
CTE, linear | 70.0 - 80.0 µm/m-°C @Temperature 20.0 - 100 °C |
38.9 - 44.4 µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
Schwartz Technical Plastics LAMIGAMID® 300 Cast Polyamide 6, Dry Application: slippers and center blocks for heavy rolling mills, outrigger floatsInformation provided by Schwartz Technical Plastics GmbH |
|||
CTE, linear | 70.0 µm/m-°C | 38.9 µin/in-°F | ISO 11359 |
Styrolution Luran® HH-120 Alpha-Methylstyrene Acrylonitrile Luran HH-120 is a grade of AMSAN with high heat resistance and improved mechanical strength. It is suitable for injection molding and extrusion applications and can be used as a modifier for high he.. |
|||
CTE, linear | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
Teijin Panlite® AD-5503 Optical Use Polycarbonate Resin High fluidity grade for optical media that provides low optical distortion moldings. Impurities in pellets are severely controlled, and resulting high quality is obtaining good reputation.Applicatio.. |
|||
CTE, linear | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
Teijin Panlite® L-1225Z100 Transparent and Weather Resistant grade Polycarbonate Resin Conforms to SAE regulations. It is an injection molding grade that has slightly high fluidity, weather resistance and mold release property and is bluish-tinted to exhibit clear colorApplications:Co.. |
|||
CTE, linear | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
Teijin Panlite® L-1225ZL100 Transparent and Weather Resistant grade Polycarbonate Resin Conforms to SAE regulations. It is a thin wall injection molding grade as it has high fluidity, weather resistance and mold release property and is bluish-tinted to exhibit clear color.Applications:.. |
|||
CTE, linear | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
Teijin Panlite® L-1250Y Standard (mold release/ice color grade) Polycarbonate Resin Standard injection molding grade that has an improved mold release property and is bluish-tinted to exhibit clear color.Applications:Components of mechanical, electric, electronic, medical, safety a.. |
|||
CTE, linear | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
Teijin Panlite® LN-1250G Flame Resistant, Translucent Polycarbonate Resin Flame retardant and mold release grade with normal fluidity, which is suitable for injection molding applications.Applications:Electric, electronic and business machine components that need flame re.. |
|||
CTE, linear | 70.0 µm/m-°C | 38.9 µin/in-°F | ISO 11359 |
Styrolution Novodur® H950 ABS Novodur H950 is a very high heat injection molding grade with high gloss surface appearanceInformation provided by Styrolution |
|||
CTE, linear | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Lubrizol Isoplast® 202LGF40 Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
CTE, linear | 70.0 µm/m-°C @Temperature 40.0 - 130 °C |
38.9 µin/in-°F @Temperature 104 - 266 °F |
TMA; ASTM E831 |
Plenco 1500 Polyester, Granular, Transfer Molded PLENCO 01500 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance, and low post shrinkage characteristics. UL recognized under compon.. |
|||
CTE, linear | 70.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
38.9 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duracon® TR-20 Acetal Co-polymer (POM), Mineral filling, Mineral filling, High rigidity, Low warpage DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
CTE, linear | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
|
Tra-Con Tra-Bond 2230 Color Keyed, High Temperature Epoxy Adhesive TRA-BOND 2230 is a clear, low viscosity, high temperature, two-part epoxy adhesive that changes colors during the curing process to indicate cure status. The unmixed components are light yellow; the.. |
|||
CTE, linear | 70.0 - 80.0 µm/m-°C | 38.9 - 44.4 µin/in-°F | |
Hippe PET Polyethylene Terephthalate Linear, saturated polyesters are thermoplastics which are used where good dimensional accuracy, high creep resistance and good sliding and wear behavior are required. Partially crystallized PET pos.. |
|||
CTE, linear | 70.0 µm/m-°C @Temperature 20.0 °C |
38.9 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Altuglas® GR 7E LIL Acrylic ALTUGLAS GR 7E LIL is an injection molding grade with excellent balance between mechanical, thermal and optical properties.Key features : easy processing and demolding improved chemical resistance .. |
|||
CTE, linear | 70.0 µm/m-°C | 38.9 µin/in-°F | ASTM E831 |
Addiplast Addinyl B2 Nylon 6 Unreinforced, medium viscosityInformation provided by Addiplast. |