Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 30.0 - 103 µm/m-°C | 16.7 - 57.0 µin/in-°F | Average value: 58.5 µm/m-°C Grade Count:30 |
Overview of materials for Nylon 6, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ.. |
|||
CTE, linear | 30.0 µm/m-°C @Temperature 20.0 °C |
16.7 µin/in-°F @Temperature 68.0 °F |
DIN 53752; ASTM D696 |
Kolon KOPA® KN333HB640BL Multi Reinforced Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
CTE, linear | 30.0 µm/m-°C | 16.7 µin/in-°F | ASTM D696 |
Gromax PBT 4130-201D 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
CTE, linear | 30.0 µm/m-°C | 16.7 µin/in-°F | ASTM D696 |
Gromax PBT 5130-104 30% Glass Fiber Filled CCP Halogen-free PBT, Black. PBT flame-retarded glass fiber 30% reinforced injection molding gradeCharacteristics:Excellent electrical property Excellent temperature resistance, high heat distortion.. |
|||
CTE, linear | 30.0 µm/m-°C | 16.7 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1105/GF/20/EM PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch.. |
|||
CTE, linear | 30.0 µm/m-°C | 16.7 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1301-0915 PPS, linear, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
CTE, linear | 30.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
16.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics Valox® AB9530 ABS+PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear | 30.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
16.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics Valox® PDR4908 PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear | 30.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
16.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics Valox® VIC4311 PBT VALOX VIC4311 is a 30% glass filled, impact modified PBT with excellent epoxy adhesion. Automotive underhood applications such as ignition coil housings. |
|||
CTE, linear | 30.0 µm/m-°C @Temperature 20.0 °C |
16.7 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
Teijin Multilon DN-1530B Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy Halogen-free flame retardant PC/ABS polymer alloy, and is also antimony-free. It has improved stiffness through the addition of 30 % filler. Improved stiffness and high fluidity realizes a thin wall.. |
|||
CTE, linear | 30.0 µm/m-°C | 16.7 µin/in-°F | ASTM D696 |
Samyang Tribit® 1500G15K PBT, Reinforced Impact Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1500G15K is a reinforced, impact grade.Appl.. |
|||
CTE, linear | 30.0 µm/m-°C @Temperature 20.0 °C |
16.7 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Toyobo VYLOPET® EMC133 Injection Molding Polyester Resin, Hydrolysis Resistant Applications: Electric rice cooker partsBathroom appliancesFeatures: Good hydrolysis resistanceInformation provided by Toyobo. |
|||
CTE, linear | 30.0 µm/m-°C | 16.7 µin/in-°F | ASTM-D696 |
Toyobo VYLOPET® EMC320R Polyester Resin VYLOPET® is a polyester resin developed specifically for injection molding. Polyester resins have excellent heat resistance, rigidity, chemical resistance, and electric properties. Grade EMC320R ha.. |
|||
CTE, linear | 30.0 µm/m-°C | 16.7 µin/in-°F | Below Tg |
Tra-Con Tra-Bond 933-2 Moisture Resistant Chip Encapsulant TRA-BOND 933-2 one component, highly filled, electrically insulating epoxy encapsulant is designed for encapsulating microelectronic chips. This epoxy provides excellent environmental and mechanical.. |
|||
CTE, linear | 30.0 - 35.0 µm/m-°C | 16.7 - 19.4 µin/in-°F | |
Master Bond Supreme 11AO Electrically Isolating Adhesive and Sealant Description: Master Bond Polymer System SURPEME 11AO is a two component epoxy resin system for high performance bonding and sealing formulated to cure at room temperature or more rapidly at elevated.. |
|||
CTE, linear | 30.0 µm/m-°C @Temperature 20.0 °C |
16.7 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Toyobo VYLOPET® EMC330 Injection Molding Polyester Resin, Hydrolysis Resistant Applications: Electric rice cooker partsBathroom appliancesFeatures: Good hydrolysis resistanceInformation provided by Toyobo. |
|||
CTE, linear | 30.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
16.7 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 53752 |
CP-Polymer-Technik Wellamid® 6000/42 GV 15 HWCP 15% Glass Fiber Nylon 6, Polymer Modified, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
CTE, linear | 30.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
16.7 µin/in-°F @Temperature 73.4 - 176 °F |
53752-A |
BASF Elastollan R 3001 15% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
CTE, linear | 30.0 - 50.0 µm/m-°C @Temperature 20.0 °C |
16.7 - 27.8 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance BIF-11 Bonded (Composite) Magnetic Material |
|||
CTE, linear | 30.0 µm/m-°C @Temperature 20.0 °C |
16.7 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Chang Chun Plastic PBT4830 Fire Retardant & 30% Glass Fiber Enforced Grade PBT Information provided by Dowell Trading Company Ltd. |
|||
CTE, linear | 30.0 µm/m-°C | 16.7 µin/in-°F | VDE 0304T1 |
Bulk Molding Compounds tetra-DUR F 4001 Bulk Molding Compound UL-Licensed, Abrasion resistance, free of fiber glass.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipati.. |
|||
CTE, linear | 30.0 µm/m-°C @Temperature 20.0 °C |
16.7 µin/in-°F @Temperature 68.0 °F |
Dry; ASTM D696 |
Asahi Kasei Leona® 90G33 33% Glass Filled Nylon 66 Enhanced strength and stiffness; with 33% GF. Superior fluidity and appearance.Applications:Automotive parts Information provided by Asahi Kasei |
|||
CTE, linear | 30.0 µm/m-°C | 16.7 µin/in-°F | ASTM D696 |
Gromax CCP PBT 3030-200HR 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
CTE, linear | 30.0 µm/m-°C | 16.7 µin/in-°F | ASTM E831 |
Addiplast Addinyl B2 V30 Nylon 6, 30% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||
CTE, linear | 30.0 µm/m-°C | 16.7 µin/in-°F | ASTM E831 |
Addiplast Addinyl B2 ZV30 Nylon 6, 30% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |
|||
CTE, linear | 30.0 µm/m-°C @Temperature 20.0 °C |
16.7 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
LATI LARIL 13 G/30-V1 30% Glass Fiber Reinforced Polyphenylene Oxide (PPOm) (UL94V-1)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
CTE, linear | 30.0 µm/m-°C | 16.7 µin/in-°F | ASTM D696 |
Samyang Tripet® 2500G45 Polyethylene Terephthalate, 45% Glass Fiber Reinforced TRIPET® has excellent heat resistance, good surface, chemical resistance and high electrical performance.Applications:Coil BobbinConnectorMotor HousingLamp HousingRelay BaseIron bodyAll information.. |