Samyang Tripet® 2500G45 Polyethylene Terephthalate, 45% Glass Fiber Reinforced

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), 50% Glass Reinforced
Manufacturer Samyang
Trade Name Tripet®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samyang Tripet® 2500G45 Polyethylene Terephthalate, 45% Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
TRIPET® has excellent heat resistance, good surface, chemical resistance and high electrical performance.Applications:Coil BobbinConnectorMotor HousingLamp HousingRelay BaseIron bodyAll information provided by Samyang
Physical Properties Metric English Comments
Specific Gravity 1.70 g/cc
1.70 g/cc
ASTM D792
Water Absorption 0.10 %

@Time 86400 sec
0.10 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm

@Thickness 3.00 mm
0.0020 - 0.0040 in/in

@Thickness 0.118 in
ASTM D955
Melt Flow 28 g/10 min

@Load 5.00 kg,
Temperature 265 °C
28 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 119
119
ASTM D785
Tensile Strength, Yield 191 MPa
27700 psi
ASTM D638
Elongation at Break 6.0 %
6.0 %
ASTM D638
Flexural Yield Strength 279 MPa
40500 psi
ASTM D790
Flexural Modulus 9.32 GPa
1350 ksi
ASTM D790
Izod Impact, Unnotched 0.932 J/cm

@Thickness 3.17 mm
1.74 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 30.0 µm/m-°C
16.7 µin/in-°F
ASTM D696
Melting Point 255 °C
491 °F
Deflection Temperature at 0.46 MPa (66 psi) 250 °C
482 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 230 °C
446 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.59 mm
HB

@Thickness 0.0625 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Constant 3.9

@Frequency 1.00e+6 Hz
3.9

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 25.0 kV/mm
635 kV/in
ASTM D149
Dissipation Factor 0.016

@Frequency 1.00e+6 Hz
0.016

@Frequency 1.00e+6 Hz
ASTM D150
Arc Resistance 125 sec
125 sec
ASTM D495