Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 20.0 - 40.0 µm/m-°C @Temperature 50.0 - 150 °C |
11.1 - 22.2 µin/in-°F @Temperature 122 - 302 °F |
ISO 11359-2 |
Raschig Group 4552 Silicone Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to +/- 300°C continuously, excellent electrical properties, good mechanical strength, very good dimensional stabi.. |
|||
CTE, linear | 15.0 - 40.0 µm/m-°C | 8.33 - 22.2 µin/in-°F | Average value: 21.9 µm/m-°C Grade Count:9 |
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35.. |
|||
CTE, linear | 20.0 - 40.0 µm/m-°C | 11.1 - 22.2 µin/in-°F | Average value: 30.5 µm/m-°C Grade Count:15 |
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a.. |
|||
CTE, linear | 18.0 - 40.0 µm/m-°C | 10.0 - 22.2 µin/in-°F | Average value: 28.8 µm/m-°C Grade Count:9 |
Overview of materials for Polycarbonate, Carbon + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + PTFE Filled". Each property range of values reported is minimum and maximum valu.. |
|||
CTE, linear | 20.0 - 40.0 µm/m-°C @Temperature 50.0 - 150 °C |
11.1 - 22.2 µin/in-°F @Temperature 122 - 302 °F |
Average value: 30.0 µm/m-°C Grade Count:2 |
Overview of materials for Silicone, Molded, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
CTE, linear | 15.0 - 40.0 µm/m-°C | 8.33 - 22.2 µin/in-°F | Average value: 29.4 µm/m-°C Grade Count:11 |
Overview of materials for Phenolic, Novolac, Fabric Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Fabric Filled". Each property range of values reported is minimum and maximum values .. |
|||
CTE, linear | 30.0 - 40.0 µm/m-°C @Temperature 20.0 - 100 °C |
16.7 - 22.2 µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
Schwartz Technical Plastics LAMINEX® 2101 Cotton Fabric, Phenolic Resin Impregnated Application: bearing segments and prismatic bearingsInformation provided by Schwartz Technical Plastics GmbH |
|||
CTE, linear | 30.0 - 40.0 µm/m-°C @Temperature 20.0 - 100 °C |
16.7 - 22.2 µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
Schwartz Technical Plastics LAMINEX® 2141 Cotton Fabric, Phenolic Resin Impregnated, MoS2 Filled Application: bearing segments and prismatic bearingsInformation provided by Schwartz Technical Plastics GmbH |
|||
CTE, linear | 35.0 - 40.0 µm/m-°C | 19.4 - 22.2 µin/in-°F | |
Master Bond EP42HT-2Med Epoxy Meets USP Class VI Requirements Description: Master Bond Polymer System EP42HT-2Med is a room temperature curable two component epoxy, adhesive, sealant, coating and casting material featuring high temperature resistance along wit.. |
|||
CTE, linear | 35.0 - 40.0 µm/m-°C | 19.4 - 22.2 µin/in-°F | |
Master Bond EP42HT-2ND-2Med Heat Resistant, Medical Grade Non-Drip Epoxy Master Bond Polymer System EP42HT-2ND2MED (Black) is a room temperature curable two component epoxy adhesive and sealant featuring high temperature resistance along with outstanding chemical resista.. |
|||
CTE, linear | 35.0 - 40.0 µm/m-°C | 19.4 - 22.2 µin/in-°F | |
Master Bond EP45HTND-2 Chemically Resistant, Non-Drip Epoxy Description: Master Bond EP45HTND-2 is a two component epoxy system for high performance bonding, sealing and coating. It is used for applications requiring solid temperature resistance and capable .. |
|||
CTE, linear | 35.0 - 40.0 µm/m-°C | 19.4 - 22.2 µin/in-°F | |
Master Bond EP42-2LV Epoxy Resists Heat and Chemicals Description: Master Bond Polymer System EP42-2LV is a low viscosity room temperature curable two component epoxy, adhesive, sealant, coating and casting material featuring outstanding chemical resis.. |
|||
CTE, linear | 35.0 - 40.0 µm/m-°C | 19.4 - 22.2 µin/in-°F | |
Master Bond EP42HT-2 Epoxy Adhesive Resists Sterilization Description: Master Bond Polymer System EP42HT-2 is a room temperature curable, two component epoxy adhesive, sealant, coating and casting material featuring high temperature resistance along with o.. |
|||
CTE, linear | 35.0 - 40.0 µm/m-°C | 19.4 - 22.2 µin/in-°F | |
Master Bond EP42HT-2FG Two Component Epoxy Adhesive for Food Applications Master Bond Polymer System EP42HT-2FG is a room temperature setting, two component epoxy adhesive, sealant and coating specially formulated for food applications. It has been independently tested an.. |
|||
CTE, linear | 35.0 - 40.0 µm/m-°C | 19.4 - 22.2 µin/in-°F | |
Master Bond Supreme 11AOHTLO Epoxy Passes NASA Low Outgassing Tests Description: Master Bond Supreme 11AOHTLO is a two component epoxy resin system for high performance bonding and sealing. Although, it is formulated to cure at room temperature, the best cure schedu.. |
|||
CTE, linear | 35.0 - 40.0 µm/m-°C | 19.4 - 22.2 µin/in-°F | ASTM D696 |
Unitika PT-3020 Characteristics: Dimensional accuracy (planarity) Heat resistance Creep resistance and elasticity RigidityInformation provided by Unitika Ltd. |
|||
CTE, linear | 30.0 - 40.0 µm/m-°C @Temperature 20.0 °C |
16.7 - 22.2 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
E-Polymers TEKAMID® TA210M40 , 40% Mineral Filled PA66, DAM 40% Mineral filled, Heat resistance, PlatableInformation provided by E-Polymers Co. Ltd. |
|||
CTE, linear | 20.0 - 40.0 µm/m-°C | 11.1 - 22.2 µin/in-°F | Average value: 27.7 µm/m-°C Grade Count:14 |
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an.. |
|||
CTE, linear | 30.0 - 40.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
16.7 - 22.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics NORYL PX2944 PPE+HIPS (Asia Pacific) PPE/PS, GF20%, high heat, non-FR |
|||
CTE, linear | 35.0 - 40.0 µm/m-°C | 19.4 - 22.2 µin/in-°F | |
Master Bond EP42HT-2LO Low Outgassing, Heat Resistant Two Component Epoxy Master Bond Polymer System EP42HT-2LO is a room temperature curable two component epoxy, adhesive, sealant, coating and casting material featuring high temperature resistance along with outstanding .. |
|||
CTE, linear | 32.0 - 40.0 µm/m-°C @Temperature 100 - 300 °C |
17.8 - 22.2 µin/in-°F @Temperature 212 - 572 °F |
Average value: 37.4 µm/m-°C Grade Count:27 |
Overview of materials for Polyimide, Thermoset Film This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Thermoset Film". Each property range of values reported is minimum and maximum values of appr.. |