Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 83.0 µm/m-°C @Thickness 2.00 mm, Temperature -125 - 20.0 °C |
46.1 µin/in-°F @Thickness 0.0787 in, Temperature -193 - 68.0 °F |
ASTM E831-06 |
NeXolve Clear Optionox® Polyimide Film/Coating Highly UV durable with excellent weatherability and stability to ozone.Optinox® films and coatings are highly UV durable and exhibit excellent weathering durability, including very high stability .. |
|||
CTE, linear | 83.0 µm/m-°C | 46.1 µin/in-°F | ASTM D696 |
Samyang Triloy® 410 PC/PET alloy
(discontinued **) Characteristics:Impact resistantHeat resistantDimensional stabilityProcessabilityGood flowApplications:O/A partRear view mirror housingRice cooker baseAll information provided by Samyang |
|||
CTE, linear | 83.0 µm/m-°C | 46.1 µin/in-°F | ASTM D696 |
Samyang Triloy® 410N PC/PET alloy, Flame Retardant
(discontinued **) Characteristics:Impact resistantHeat resistantDimensional stabilityProcessabilityFlame retardantApplications:O/A partRear view mirror housingRice cooker baseAll information provided by Samyang |
|||
CTE, linear | 83.0 µm/m-°C @Temperature 20.0 °C |
46.1 µin/in-°F @Temperature 68.0 °F |
Injection molded sample; ASTM D696 |
Ineos ABS Lustran® 356 Extrusion, Low-Gloss
(discontinued **) Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with |
|||
CTE, linear | 83.0 - 135 µm/m-°C | 46.1 - 75.0 µin/in-°F | Average value: 98.9 µm/m-°C Grade Count:10 |
Overview of materials for Fluorinated Ethylene Propylene (FEP), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Fluorinated Ethylene Propylene (FEP), Molded/Extruded". Each property range of values reported is minimu.. |
|||
CTE, linear | 83.0 µm/m-°C @Temperature 20.0 °C |
46.1 µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
BASF Capron® 8200 NL Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
CTE, linear | 83.0 µm/m-°C @Temperature 20.0 °C |
46.1 µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
BASF Capron® 8202 NL Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
CTE, linear | 83.0 µm/m-°C @Temperature 20.0 °C |
46.1 µin/in-°F @Temperature 68.0 °F |
ASTM data |
BASF Capron® 8202 HS BK-102 Nylon 6 (Dry)
(discontinued **) Capron 8202 HS BK-102 is an unfilled, heat stabilized, pigmented black, low viscosity, general purpose nylon 6 exhibiting excellent fluidity for filling thin sections. It possesses the combination.. |
|||
CTE, linear | 83.0 µm/m-°C @Temperature 20.0 °C |
46.1 µin/in-°F @Temperature 68.0 °F |
ASTM data |
BASF Capron® 8202 NL Nylon 6 (Dry)
(discontinued **) Capron 8202 NL is an unfilled, low viscosity, non-lubricated nylon 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is available in natural, heat sta.. |
|||
CTE, linear | 83.0 µm/m-°C | 46.1 µin/in-°F | ASTM D696 |
Samyang Triloy® 120H PC/ABS alloy Characteristics:Impact resistantChemical resistantDimensional stabilityProcessabilityGood flowApplications:Automotive bumperAutomotive outdoor handleAll information provided by Samyang |
|||
CTE, linear | 83.0 µm/m-°C | 46.1 µin/in-°F | ASTM D696 |
Samyang Triloy® 130 PC/PBT alloy Characteristics:Impact resistantChemical resistantDimensional stabilityProcessabilityGood flowApplications:Automotive bumperAutomotive outdoor handleAll information provided by Samyang |
|||
CTE, linear | 83.0 µm/m-°C | 46.1 µin/in-°F | ASTM D696 |
Samyang Triloy® 170 PC/PBT alloy Characteristics:Impact resistantChemical resistantDimensional stabilityProcessabilityFlame retardantApplications:Automotive bumperAutomotive outdoor handleAll information provided by Samyang |
|||
CTE, linear | 83.0 µm/m-°C | 46.1 µin/in-°F | ASTM D696 |
Samyang Triloy® 200NH PC/ABS alloy, Flame Retardant Non-halogenCharacteristics:Impact resistantDimensional stabilityProcessabilityApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information provided by Samyang |
|||
CTE, linear | 83.0 µm/m-°C | 46.1 µin/in-°F | ASTM D696 |
Samyang Triloy® 210NH PC/ABS alloy, Flame Retardant Non-halogenCharacteristics:Impact resistantHeat resistantFlame retardantDimensional stabilityProcessabilityApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information pro.. |
|||
CTE, linear | 83.0 µm/m-°C | 46.1 µin/in-°F | ASTM D696 |
Samyang Triloy® 210NHF Polymer Alloy, Flame Retardancy (Non-Halogen) Excellent impact, formability and weather resistance.210NHF is a flame retardant (non-halogen) grade.Applications: LCD TV Rear Cover (high flow)Information provided by Samyang. |
|||
CTE, linear | 83.0 µm/m-°C | 46.1 µin/in-°F | ASTM D696 |
Samyang Triloy® 230NH PC/ABS alloy, Flame Retardant Non-halogenCharacteristics:Impact resistantHeat resistantFlame retardantDimensional stabilityProcessabilityApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information pro.. |
|||
CTE, linear | 83.0 µm/m-°C | 46.1 µin/in-°F | Absolute Drying; ASTM-D696 |
Toyobo GLAMIDE® T-803 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
CTE, linear | 83.0 - 105 µm/m-°C @Temperature 23.0 - 60.0 °C |
46.1 - 58.3 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
Daikin NEOFLON NP-101 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: High speed wire and cable coatings.Information pro.. |
|||
CTE, linear | 83.0 - 105 µm/m-°C @Temperature 23.0 - 60.0 °C |
46.1 - 58.3 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
Daikin NEOFLON NP-120 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, cable jacketing, tubes.. |
|||
CTE, linear | 83.0 - 105 µm/m-°C @Temperature 23.0 - 60.0 °C |
46.1 - 58.3 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
Daikin NEOFLON NP-21 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Suited to high speed extrusion .. |
|||
CTE, linear | 83.0 - 105 µm/m-°C @Temperature 23.0 - 60.0 °C |
46.1 - 58.3 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
Daikin NEOFLON NP-30 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, tubes, cable jacketing.. |
|||
CTE, linear | 83.0 - 105 µm/m-°C @Temperature 23.0 - 60.0 °C |
46.1 - 58.3 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
Daikin NEOFLON NP-20 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Wire and cable coatings, films,.. |
|||
CTE, linear | 83.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
46.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM Test |
BASF Ultramid® 8202 HS BK-102 PA6 (Dry) Ultramid 8202 HS BK-102 is an unfilled, heat stabilized, pigmented black, low viscosity, general purpose injection molding PA6 exhibiting excellent fluidity for filling thin sections. It possesses .. |
|||
CTE, linear | 83.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
46.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM Test |
BASF Ultramid® 8202 HS PA6 (Dry) Ultramid 8202 HS is a heat stabilized, low viscosity, general purpose nylon 6 injection molding homopolymer. It possesses the combination of strength and toughness and has excellent chemical and ab.. |
|||
CTE, linear | 83.0 µm/m-°C | 46.1 µin/in-°F | ASTM E831 |
BASF Ultramid® 8202 L Intermediate PA6 (Dry) Description: Ultramid 8202 L-Intermediate is an unreinforced, low viscosity, non-lubricated PA6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is avai.. |
|||
CTE, linear | 83.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
46.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM Test |
BASF Ultramid® 8202 PA6 (Dry) Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ult.. |
|||
CTE, linear | 83.0 µm/m-°C | 46.1 µin/in-°F | ASTM D696 |
Samyang Triloy® 450N Polymer Alloy, Blow Molding Excellent impact, formability and weather resistance.450N is a blow molding grade.Applications: ConnectorsInformation provided by Samyang. |
|||
CTE, linear | 83.0 µm/m-°C | 46.1 µin/in-°F | ASTM D696 |
Samyang Triloy® S460G15 Polymer Alloy, Reinforced Excellent impact, formability and weather resistance.220 is a reinforced grade.Applications: LCD Panel Frame - for dimensional stabilityInformation provided by Samyang. |
|||
CTE, linear | 83.0 µm/m-°C | 46.1 µin/in-°F | ASTM D696 |
Samyang Triloy® 200N PC/ABS alloy, Flame Retardant Characteristics:Impact resistantFlame retardantApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information provided by Samyang |