Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 40.0 - 50.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
22.2 - 27.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics Lexan® BFL2015 PC (Asia Pacific) Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only |
|||
CTE, linear | 40.0 µm/m-°C | 22.2 µin/in-°F | |
Resinlab® EP1340 Medium Viscosity, Flame Retardant Epoxy Casting Resin System Resinlab™ EP1340 is a medium viscosity, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File# E186034) for U.. |
|||
CTE, linear | 40.0 µm/m-°C @Temperature 20.0 °C |
22.2 µin/in-°F @Temperature 68.0 °F |
DIN 53752; ASTM D696 |
Kolon SPESIN® KP213G15HI Multi Reinforced PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
CTE, linear | 40.0 µm/m-°C @Temperature 20.0 °C |
22.2 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
LATI LARIL 13 G/20 20% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
CTE, linear | 40.0 µm/m-°C @Thickness 1.57 mm, Temperature 20.0 °C |
22.2 µin/in-°F @Thickness 0.0620 in, Temperature 68.0 °F |
x-axis; IPC-TM 650-2.4.24 |
Industrial Laminates/Norplex NP159 Synthetic Fabric
(discontinued **) Description: Woven aramid fiber fabric combined with high temperature phenolic resin. With a proper post baking procedure, NP159 will withstand continuous operation at 200° C. Material becomes brit.. |
|||
CTE, linear | 40.0 µm/m-°C | 22.2 µin/in-°F | ASTM D696 |
Kolon SPESIN® KP213G30SB3 Glass Fiber Reinforced PBT Compound Resin G/F 30% reinforcedApplications: Ignition coil bobbinsInformation provided by API-Kolon. |
|||
CTE, linear | 40.0 µm/m-°C | 22.2 µin/in-°F | ASTM D696 |
Kolon SPESIN® KP513UG PBT Alloy Resin Extrudable, delusteringApplications: Mono filamentInformation provided by API-Kolon. |
|||
CTE, linear | 40.0 µm/m-°C | 22.2 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1105-8001 PEEK, with glass spheres Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Reduced moment of inertia compared with metal parts.Chemical and hydrolysis resistance par.. |
|||
CTE, linear | 40.0 µm/m-°C | 22.2 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1200-7116-1 ABS, with carbon fiber Applications: Office communication.Reduced moment of inertia compared with metal parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Strong, stiff .. |
|||
CTE, linear | 40.0 µm/m-°C @Temperature 20.0 °C |
22.2 µin/in-°F @Temperature 68.0 °F |
DIN 53752; ASTM D696 |
Kolon KOPA® KN135HB40SIBL Multi Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
CTE, linear | 40.0 µm/m-°C @Temperature 20.0 °C |
22.2 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
Teijin Panlite® G-3120PH For Cameras, Glass Fiber Reinforced Polycarbonate Resin Reinforced with 30 % of special GF and improved appearance grade.Applications:Precision machinery, electric and electronic components that need dimensional accuracy and good appearance.Information p.. |
|||
CTE, linear | 40.0 - 60.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
22.2 - 33.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics NORYL GTX GTX870 PPE+PA6 (Asia Pacific) |
|||
CTE, linear | 40.0 - 45.0 µm/m-°C | 22.2 - 25.0 µin/in-°F | |
Master Bond EP21ARHT Two component epoxy adhesive, sealant, coating and encapsulating system Product Description: Master Bond EP21ARHT is a two component epoxy resin system for high performance bonding, sealing, coating and encapsulating. It has a convenient 100 to 50 mix ratio by weight an.. |
|||
CTE, linear | 40.0 - 45.0 µm/m-°C | 22.2 - 25.0 µin/in-°F | |
Master Bond EP21ARHTND Two component epoxy adhesive, sealant, coating and encapsulating system Product Description: Master Bond EP21ARHTND is a two component epoxy resin system for high performance bonding, sealing and coating. It has a convenient 100 to 50 mix ratio by weight and is formulat.. |
|||
CTE, linear | 40.0 - 45.0 µm/m-°C | 22.2 - 25.0 µin/in-°F | |
Master Bond EP46HT-2Med Two Component Heat Resistant Biocompatible Epoxy System Master Bond Polymer System EP46HT-2MED is a two component medical grade epoxy system for high performance structural bonding and casting suitable for applications where resistance to temperatures fr.. |
|||
CTE, linear | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-2 |
Unitika B2040G33 PA66, 33% Glass Fiber Reinforced, Conditioned Information provided by Unitika Ltd. |
|||
CTE, linear | 40.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
22.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duranex® 3105H Polybutylene Terephthalate (PBT), Standard, 15% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
CTE, linear | 40.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
22.2 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 53752 |
CP-Polymer-Technik Wellamid® 6600 CF10 HWCP 10% Carbon Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
CTE, linear | 40.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
22.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM Test |
BASF Ultramid® A34 01 PA66 (Dry) Ultramid A34 01 is an intermediate visosity, PA66 grade. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation "X Polyamide", 1.6.1998 or .. |
|||
CTE, linear | 40.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
22.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
Beijing Chemical Industry KAIFA® M109-G20 MPPO Resin 20% glass fiber reinforcedInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
CTE, linear | 40.0 µm/m-°C | 22.2 µin/in-°F | ASTM E831 |
Addiplast Addinyl A2 M20 V10 Nylon 66, Glass/Mineral Filled Mixed products with improved stiffness and good dimensional stability, low warpage.Information provided by Addiplast. |
|||
CTE, linear | 40.0 µm/m-°C @Temperature 20.0 °C |
22.2 µin/in-°F @Temperature 68.0 °F |
|
AIM CASTIN Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |
|||
CTE, linear | 40.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
22.2 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 53752 |
CP-Polymer-Technik Wellamid® 6000 CF 10 HWCP 10% Carbon Fiber Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
CTE, linear | 40.0 µm/m-°C | 22.2 µin/in-°F | ASTM E831 |
Addiplast Addinyl C2 M20 V10 Nylon 66/6, Glass/Mineral Filled Mixed products with improved stiffness and good dimensional stability, low warpage.Information provided by Addiplast. |
|||
CTE, linear | 40.0 µm/m-°C @Temperature 20.0 °C |
22.2 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Resinoid 2016P Phenolic Molding, Fabric Reinforced Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance |
|||
CTE, linear | 40.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
22.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics Valox® VGF4715 PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear | 40.0 µm/m-°C @Temperature 20.0 °C |
22.2 µin/in-°F @Temperature 68.0 °F |
DIN 53752; ASTM D696 |
Kolon KOPA® KN135G33HI Multi Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubric.. |
|||
CTE, linear | 40.0 µm/m-°C @Temperature 20.0 °C |
22.2 µin/in-°F @Temperature 68.0 °F |
DIN 53752; ASTM D696 |
Kolon Kopa® KN173MS Nylon 6 Resin KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c.. |