Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Master Bond EP21ARHTND Two component epoxy adhesive, sealant, coating and encapsulating system

Category Polymer , Thermoset , Epoxy , Epoxy Encapsulant, Unreinforced
Manufacturer Master Bond Inc.
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Master Bond EP21ARHTND Two component epoxy adhesive, sealant, coating and encapsulating system.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: Master Bond EP21ARHTND is a two component epoxy resin system for high performance bonding, sealing and coating. It has a convenient 100 to 50 mix ratio by weight and is formulated to cure at ambient temperatures or more quickly at elevated temperatures. It has resistance to a wide array of chemicals, particularly to acids (a more detailed list appears below). It is resistant to sulfuric and hydrochloric acids. EP21ARHTND is 100% reactive and contains no solvents or diluents. It has very low linear shrinkage upon cure. Also, it has outstanding physical properties and electrical insulation values. EP21ARHTND can be used as an adhesive, sealant, coating, potting or encapsulating material. EP21ARHTND is especially useful for coating tanks and other vessels that may contain acids. It is serviceable over the wide temperature range of -60°F to +400°F. It adheres well to a wide variety of substrates including metals, glass, ceramics and many rubbers and plastics. EP21ARHTND is a smooth paste and is considered a non-drip type system. Parts A and B are amber. This epoxy compound is widely used in aerospace, electronic, electrical, chemical processing applications and in other applications where chemical resistance to acids is needed and a non-drip viscosity is helpful. Product Advantages: Smooth paste; contains no solvents or diluents Versatile cure schedules; ambient temperature cures or fast elevated temperature cures High bonding strength to both similar and dissimilar substrates Wide temperature service capability from -60°F to +400°F Good electrical insulator. Low viscosity. Ideal for potting and encapsulation Outstanding chemical resistance, particularly to acidsInformation provided by MasterBond®
Mechanical Properties Metric English Comments
Hardness, Shore D >= 75
>= 75
Tensile Strength at Break >= 62.1 MPa
<br>@Temperature 23.9 °C
>= 9000 psi
<br>@Temperature 75.0 °F
Shear Strength 17.2 MPa
2500 psi
Al/Al, Tensile lap
Thermal Properties Metric English Comments
CTE, linear 40.0 - 45.0 µm/m-°C
22.2 - 25.0 µin/in-°F
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
Dielectric Constant 3.8
<br>@Frequency 60.0 Hz,<br> Temperature 25.0 °C
3.8
<br>@Frequency 60.0 Hz,<br> Temperature 77.0 °F
Dielectric Strength 17.3 kV/mm
<br>@Thickness 3.17 mm
440 kV/in
<br>@Thickness 0.125 in
Processing Properties Metric English Comments
Cure Time 120 - 180 min
<br>@Temperature 93.3 °C
2.00 - 3.00 hour
<br>@Temperature 200 °F
120 - 180 min
<br>@Temperature 93.3 °C
2.00 - 3.00 hour
<br>@Temperature 200 °F
Overnight at 75°F followed by
1440 - 2880 min
<br>@Temperature 22.2 °C
24.0 - 48.0 hour
<br>@Temperature 72.0 °F
Pot Life 30 - 50 min
30 - 50 min
100 gram mass
Shelf Life 12.0 Month
<br>@Temperature 23.9 °C
12.0 Month
<br>@Temperature 75.0 °F
in original, unopened containers
Descriptive Properties Value Comments
Mixing Ratio (A to B) 100:50
by weight