Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 213 °C | 415 °F | ASTM D-648 |
PlastiComp Complet® LGF40 - PA6 Nylon 6, 40% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 40% long glass fiber reinforcementInformation provided by PlastiComp, Inc.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 213 °C | 415 °F | ISO 75, ASTM D648 |
Nilit Nilamid B3 H G8 40% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G8 is a product that combines outstanding strength and stiffness with good moldability and good impact strength. It is widely used for structural applications.Key character.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 213 °C @Thickness 3.18 mm |
415 °F @Thickness 0.125 in |
Annealed; ASTM D648 |
PolyOne Edgetek® RA-10GF-10CF/000 HI Polyphenylsulfone (PPSU) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 213 °C | 415 °F | Annealed; ASTM D648 |
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 resin. .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 213 °C | 415 °F | Unannealed; ASTM D648 |
Solvay Specialty Polymers KetaSpire® KT-820 GF13 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 is a low flow, 13% glass fiber reinforced grade of polyetheretherketone (PEEK). The glass fiber content is optimized to provide a balance of strength and stiffness with toughness-re.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 213 °C | 415 °F | Annealed, 0.125 in bars; ASTM D648 |
PolyOne Edgetek® RA-20CF/000 Polyarylsulfone, Carbon Fiber Reinforced
(discontinued **) Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 213 °C | 415 °F | ASTM D648 |
Lavergne VYPET VNT 835 PET 35% Glass-Mineral Reinforced Vypet VNT 835 is a 35% mineral and fiberglass reinforced PET injection molding compound designed for structural applications.Features: High temperature performance; Low warp; Excellent dimensional s.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 213 °C | 415 °F | ISO 75-1/-2 |
Lanxess Durethan® BKV 50 H2.0 EF 900116 Nylon 6, 50% Glass Fiber PA 6, injection molding grade, 50% glass fibers, good heat-ageing resistance, low viscosity (easy flow)Application Examples: mirror baseplates |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 213 °C | 415 °F | Unannealed; ASTM D648 |
Techmer ES Elastoblend® PA6 GF30 IM L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedUL File N.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 213 °C | 415 °F | Unannealed; ASTM D648 |
Techmer ES Elastoblend® PA6 GF40 IM2 NAT 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedUL File Number: E157318Processing Meth.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 213 °C | 415 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 GF50 IM 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedProcessing Method: Injection MoldingIn.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 213 °C | 415 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PEI GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 213 °C | 415 °F | ASTM D648 |
Techmer ES Plaslube® J-3/30/TF/13/SI/2 Nylon 6, 30% GFR, 13% PTFE, 2% Silicone Plaslube glass fiber reinforced polytetrafluoroethylene (PTFE) lubricated nylon 612 grades offer a unique balance of excellent wear and friction performance with good dimensional stability and mecha.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 213 °C | 415 °F | ASTM D648 |
Techmer ES Plaslube® J-3/30/TF/15 Nylon 6, 30% GFR, 15% PTFE Plaslube glass fiber reinforced polytetrafluoroethylene (PTFE) lubricated nylon 612 grades offer a unique balance of excellent wear and friction performance with good dimensional stability and mecha.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 213 °C | 415 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP JF006E PES LNP* THERMOCOMP* JF006E is a compound based on Polyethersulfone resin containing 30% Glass Fiber. Added features of this material include: Easy Molding. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 213 °C | 415 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP RX07034 PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RX07034 is a compound based on PA 66 resin containing Glass Fiber. Added features include; Low Smoke, Easy Molding, Cross Linkable under Beta-or Gamma Radiation; Specially developed.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | >= 213 °C | >= 415 °F | ISO 75 Af |
Vyncolit A2710 Glass Fiber Reinforced Novolac Phenolic Vyncolit A2710 is a glass fiber reinforced phenolic molding compound with excellent mechanical and thermal properties.Information provided by Sumitomo Bak North America, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 213 °C | 415 °F | ASTM D648 |
Adell BT-37 Nylon 6, 35% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 213 °C | 415 °F | ASTM D648 |
Asahi Kasei Thermylon® NSG-440A 60% Ceramic and Glass Fiber Reinforced Information provided by Asahi Thermofil |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 213 °C | 415 °F | Annealed, 0.125 in bars; ASTM D648 |
PolyOne Edgetek® RA-30CF/000 Polyarylsulfone, Carbon Fiber Reinforced
(discontinued **) Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 213 °C | 415 °F | ASTM D648 |
PolyOne Stat-Tech™ RA-06CF-09GF/000 Polyarylsulfone - 9% Glass Fiber - 6% Carbon Fiber Reinforced - ESD Applications
&a Data provided by PolyOne. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 213 °C | 415 °F | Annealed, 0.125 in bars; ASTM D648 |
PolyOne Edgetek® PI-40GF/000 Polyetherimide (PEI), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |