| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.30 g/cc | 0.0470 lb/in³ | ASTM D792 |
| Water Absorption | 0.70 % | 0.70 % | 24 hour immersion; ASTM D570 |
| Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 87 | 87 | ASTM D785 |
| Hardness, Rockwell R | 120 | 120 | ASTM D785 |
| Tensile Strength, Ultimate | 141 MPa | 20500 psi | ASTM D638 |
| Elongation at Break | 3.5 % | 3.5 % | ASTM D638 |
| Flexural Strength | 207 MPa | 30000 psi | ASTM D790 |
| Flexural Modulus | 6.60 GPa | 957 ksi | ASTM D790 |
| Compressive Yield Strength | 172 MPa | 24900 psi | ASTM D695 |
| Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 213 °C | 415 °F | ASTM D789 |
| Deflection Temperature at 0.46 MPa (66 psi) | 218 °C | 424 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 213 °C | 415 °F | ASTM D648 |
| Flammability, UL94 | HB | HB |