Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 215 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
215 °F
ASTM D648
Polymer Resources AH-GP1-[color]-H Acetal Homopolymer, Low Flow, High Melt Strength, Heat Stabilized
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
215 °F
ASTM D648
Polymer Resources AH-GP2-[color]-H Acetal Homopolymer, Medium Flow, General Purpose Molding, Heat Stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
215 °F
ASTM D648
Polymer Resources NY66-GP2-[color]-H General Purpose Nylon 66, Nucleated, Heat Stabilized
General Purpose Nylon 66, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grade..
Deflection Temperature at 1.8 MPa (264 psi) 102 - 110 °C
215 - 230 °F
Average value: 106 °C Grade Count:7
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled". Specific grades with carbon fiber conte..
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
215 °F
Unannealed; ASTM D648
Ravago Manufacturing Americas Hylac® FR134G10 ABS, 10% Glass Fiber Reinforced
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
215 °F
Unannealed; ASTM D648
Ravago Manufacturing Americas Hylon® N1000NL2 Nylon 6/6 (DAM)
Information provided by Ravago.
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
215 °F
Unannealed; ASTM D648
Techmer ES Electrablend® HIPS
Availability: North AmericaForms: PelletsFeatures: ConductiveInformation provided by TP Composites, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
215 °F
unannealed, .125in; ASTM D648
Star Plastics ABSGF30 Molding Grade ABS With 30% Glass
Information provided by Star Plastics, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
215 °F
Unannealed; ASTM D648
Techmer ES HiFill® PP GF/M30 CC BK 30% Glass/Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 30% Filler by WeightFeatures: Chemically Coupled and CopolymerAppearance: BlackInformation provided by TP Composites, In..
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
215 °F
Unannealed; ASTM D648
Techmer ES Luriblend® PA6/6 TS18 Nylon 66
Availability: North AmericaForms: PelletsAdditive: PTFE + Silicone Lubricant (18%)Features: LubricatedInformation provided by TP Composites, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
215 °F
Unannealed; ASTM D648
Techmer ES Statiblend® ABS E AS
Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: AntistaticInformation provided by TP Composites, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
215 °F
ASTM Test
Styrolution Terblend® N NG-04 20% Glass Filled ABS/PA6 (Dry)
Terblend N NG-04 is a glass fibre reinforced ABS/PA6 blend with excellent dimensional stability, low mold shrinkage and high heat resistance.Information provided by STYROLUTION, which is a joint ven..
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
215 °F
ASTM D648
Techmer ES Electrafil® J-1200/CF/30 ABS, 30% Carbon Fiber Reinforced
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
215 °F
Unannealed; ASTM D648
Techmer ES Luriblend® POM HO TL20 Acetal
Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated and HomopolymerInformation provided by TP Composites, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
215 °F
Unannealed; ASTM D648
Chase Plastics CP Pryme® A120 ABS, 20% Glass Fiber Reinforced
Features: Glass fiber reinforcementInjection moldingForm: PelletsInformation provided by Chase Plastics.
Deflection Temperature at 1.8 MPa (264 psi) 102 °C

@Thickness 3.17 mm
215 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Chase Plastics CP Pryme® A220G ABS Molding Resin, 20% Glass Fiber Reinforced
Information provided by Chase Plastics.
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
215 °F
Unannealed; ASTM D648
Chase Plastics CP Pryme® APC300 ABS Polycarbonate Alloy, Recycled Content
Features: Recycled contentForm: PelletsInformation provided by Chase Plastics.
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
215 °F
Unannealed; ASTM D648
Techmer ES Luriblend® POM HO TL20 BK Acetal
Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated and HomopolymerAppearance: BlackInformation provided by TP Composites, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
215 °F
ASTM D648
Chase Plastics CP Pryme® PCA300 General Purpose Polycarbonate/ABS Alloy (Utility Grade)
Information provided by Chase Plastics.
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
215 °F
ASTM D648
Polymer Resources PPX-FR5 Modified PPO, UL 94 V-0 with HDT of 225 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.