| Category | Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled |
| Manufacturer | Techmer ES |
| Trade Name | Electrafil® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Techmer ES Electrafil® J-1200/CF/30 ABS, 30% Carbon Fiber Reinforced.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.20 g/cc | 0.0434 lb/in³ | ASTM D792 |
| Water Absorption | 0.20 % | 0.20 % | 24 hrs. ASTM D570 |
| Linear Mold Shrinkage | 0.00050 cm/cm @Thickness 3.17 mm |
0.00050 in/in @Thickness 0.125 in |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 103 MPa | 15000 psi | ASTM D638 |
| Elongation at Break | 1.0 % | 1.0 % | ASTM D638 |
| Flexural Yield Strength | 145 MPa | 21000 psi | ASTM D790 |
| Flexural Modulus | 12.8 GPa | 1850 ksi | ASTM D790 |
| Izod Impact, Notched | 0.427 J/cm @Thickness 3.17 mm |
0.800 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Izod Impact, Unnotched | 2.14 J/cm @Thickness 3.17 mm |
4.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 104 °C | 220 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 215 °F | ASTM D648 |
| Flammability, UL94 | HB @Thickness 1.59 mm |
HB @Thickness 0.0625 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 50 ohm | 50 ohm | ASTM D257 |