| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 216 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
|
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS
High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 216 °F | 120°C/h; ISO 75/1 |
|
Polykemi AB SCANBLEND FS7 UV4 PC/ASA Blend with Improved Weather Resistance
Information provided by Polykemi AB
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 215 °F | ASTM D648 |
|
Polymer Resources AH-GP2-[color]-H Acetal Homopolymer, Medium Flow, General Purpose Molding, Heat Stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 216 °F | |
|
Plastcom SLOVALEN PH 56 T FRD 1 PP, flame retardant
FeaturesModified homopolymer PP for injection moulding with decreased flammability. Contains flame retardant on the halogen basis. Used in the electrical industry - terminals, coil forms, guides, co..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 216 °F | Unannealed; ASTM D648 |
|
Ravago Manufacturing Americas Hybrid B2026IU Polycarbonate + PBT Alloy
Available in North America UV Stabilizer Good Impact Resistance RoHS Compliant Form: Pellets Processing Method: Injection Molding Information provided by Ravago
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 215 °F | Unannealed; ASTM D648 |
|
Ravago Manufacturing Americas Hylac® FR134G10 ABS, 10% Glass Fiber Reinforced
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) |
102
°C <br>@Thickness 6.40 mm
|
216
°F <br>@Thickness 0.252 in
|
Unannealed; ASTM D648 |
|
LG Chemical LUPOS GP2206F ABS+GF20%, Flame Retardant
Feature: Injection Molding, ABS+GF20%, Flame RetardantApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7, 65997-17-3, 88497-56-7 and 1309-64-4Information provided b..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 216 °F | ISO 75A |
|
Lucite International Diakon® MH254 Acrylic Bead Polymer, High Transparency
PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 215 °F | |
|
MTI ThermoStran® TPU-50G Long Glass Fiber Compound
ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t..
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 215 °F | Unannealed; ASTM D648 |
|
Techmer ES Electrablend® HIPS
Availability: North AmericaForms: PelletsFeatures: ConductiveInformation provided by TP Composites, Inc.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 215 °F | unannealed, .125in; ASTM D648 |
|
Star Plastics ABSGF30 Molding Grade ABS With 30% Glass
Information provided by Star Plastics, Inc.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 216 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
|
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER
PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 216 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
|
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Europe-Africa-Middle East)
PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) |
102
°C <br>@Thickness 3.20 mm
|
216
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D648 |
|
SABIC Innovative Plastics LNP THERMOCOMP AF006XXZ ABS
LNP* THERMOCOMP* AF006XXZ is a compound based on ABS resin containing 30% Glass Fiber.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) |
102
°C <br>@Thickness 3.20 mm
|
216
°F <br>@Thickness 0.126 in
|
unannealed; ASTM D 648 |
|
SABIC Innovative Plastics LNP Thermocomp FF004 PE
LNP THERMOCOMP* FF004 is a compound based on Polyethylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) |
102
°C <br>@Thickness 6.40 mm
|
216
°F <br>@Thickness 0.252 in
|
ASTM D648 |
|
Samsung Cheil Industries Starex® GR-5020T SAN, 20% Glass Filled
Information provided by Samsung Cheil Industries.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) |
102
°C <br>@Thickness 6.40 mm
|
216
°F <br>@Thickness 0.252 in
|
ASTM D648 |
|
Samsung Cheil Industries Infino® HI-1001BP PC/ABS, Metal Plating Grade
PC/ABS material for platingInformation provided by Samsung Cheil Industries.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 216 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
|
SABIC Innovative Plastics LNP THERMOCOMP RB008 PA 66 (Asia Pacific)
LNP THERMOCOMP* RB008 is a compound based on Nylon 66 resin containing Glass Bead.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 215 °F | ASTM D648 |
|
Techmer ES Electrafil® J-1200/CF/30 ABS, 30% Carbon Fiber Reinforced |
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 215 °F | Unannealed; ASTM D648 |
|
Techmer ES Luriblend® POM HO TL20 Acetal
Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated and HomopolymerInformation provided by TP Composites, Inc.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 216 °F | ASTM D648 |
|
A. Schulman POLYFLAM™ FLP 3714 20% Glass Filled HDPE
DescriptionPolyfort® FLP 3714 is a 20% glass filled HDPE product. Information provided by A. Schulman.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 216 °F | ASTM D648 |
|
A. Schulman POLYFLAM™ FLP 3714 20% Glass Filled HDPE
DescriptionPolyfort® FLP 3714 is a 20% glass filled HDPE product. Information provided by A. Schulman.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 216 °F | Flatw 80x10x4, sp=64 mm; ISO 75/Af |
|
Eurostar Starflam PK0049 PA6, Mineral Fiber Filled, Flame Retardant, Injection Molded
Starflam PK0049 is a Free Flame Retardant Mineral Filled Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 216 °F | ISO 75 |
|
Eurotec® Tecolen® CP30 GR20 NL PPCP, 20% glass fiber reinforced, natural, high flow grade
Information provided by Eurotec®
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 216 °F | ASTM D648 |
|
PolyOne Lubri-Tech™ AT-000/02T Acetal - 2% PTFE
(discontinued **)
Data provided by PolyOne.
|
|||
| Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 216 °F | ASTM D648 |
|
Ashley Polymers Ashlene® R6041 Nylon 66, PTFE and Silicone Modified