Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | 0.125 in bar, Unannealed/Conditioned 48 hours; ASTM D648 |
Network Polymers NPP 808 C2WW Description: Polycarbonate AlloyInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP FARADEX AS003 ABS LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 - 106 °C | 172 - 222 °F | Average value: 90.0 °C Grade Count:24 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Sheet". Each property range of values reported is minimum and max.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | annealed; ASTM D648 |
Kleerdex Vinyloy™ 100 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Utility gradeApplications: Vinyloy 100 sheet is a fire retardant that can be used to substitute effectively for ABS and other utility grade thermoplastics.Features: Vinyloy 100 sheet is a recycled g.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C @Thickness 6.40 mm |
172 °F @Thickness 0.252 in |
ASTM D648 |
Kingfa FRHIPS-1162 Flame Retardant Polystyrene Features:UL 94 V-2 @ 1.6mm, V-2 @ 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingEl.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C @Thickness 6.40 mm |
172 °F @Thickness 0.252 in |
ASTM D648 |
Kingfa FRHIPS-8002 Flame Retardant Polystyrene Features:UL 94 V-2 @ 1.0mm, V-2 @ 3.2mmExcellent balancing properties, Non-DPOExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV and audio housingElec.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | |
Ineos Styrenics Polystyrene 145D (NAFTA) A high flow, general purpose polystyrene, offering exceptional processing characteristics for thin wall parts, multi-cavity tools, and complex designs.Information provided by BASF.Ineos Styrenics pu.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | annealed; ASTM D648 |
KYDEX® 6200 Thermoplastic Sheet Fire rated sheet for mass transitApplications: Dashboards, seatbacks, armrests, tray tables, window reveals, cabin linersFeatures: Kydex 6200 is a proprietary, high performance thermoplastic sheet. .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C @Thickness 6.40 mm |
172 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Prevex BJAX PPE+PS Foamable resin. All properties at 10% density reduction; 0.250" thick specimens; improved productivity.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA12 L N MB Availability: North AmericaForms: PelletsFeatures: Low ViscosityTPCI# 8807105Information provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C @Thickness 3.20 mm |
172 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP AR002XXH ABS LNP* THERMOCOMP AR002XXH is a compound based on ABS resin containing 10% Barium Sulfate. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS GN005 Availability: North AmericaForms: PelletsFeatures: General PurposeAppearance: GreenInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C @Thickness 6.40 mm |
172 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® EG-7000 ABS/PET, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® ABS SL2 Availability: North AmericaForms: PelletsAdditive: Silicone LubricantFeatures: General Purpose and LubricatedInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® ABS TL2 Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | ASTM D648 |
Supreme Petrochem SC 201LV General Purpose Polystyrene CharacteristicsHigh molecular weight grade Good flow properties along with good mechanical strength Easy process ability with good mold release propertiesProcessing Injection moldingApplicationsSuit.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | ISO 75-1/-2 |
Covestro Bayblend® FR 3005 Polycarbonate + ABS, Flame Retardant Grade Injection molding gradeeasy-flow gradeVicat/B 120 temperature = 95 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantglow wire test (GWFI): 960 °C (2.0 mm)no j.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | ASTM D648 |
Denka TE-10 Transparent Resin Polymer (MABS resin) ABS "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ABS 1501 Description: Injection Molding GradeInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ABS 2512 Description: Injection Molding Grade, Medium Impact, High FlowInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ABS 3002MC Description: Plating GradeInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | Unannealed; ASTM D648 |
Entec Hyrene® PS-HI 3/4 High Impact Polystyrene Available in North America Features: High Impact ResistanceRoHS Compliant Form: Pellets Information provided by Entec |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | |
Aclo Accutech Polypropylene Copolymer CP0437G5M25CL Glass/Mineral Reinforced Coupled |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | |
BASF Polystyrol® 475 K Impact Grade Polystyrene (Europe) Normal flowing, high-impact grade with particularly good creep strength.Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | |
BASF Polystyrol® 2710 Impact Grade Polystyrene (Europe) Special high-impact grade for refrigerators and the packaging sector. Particularly resistant to stress cracking.Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | ASTM D648 |
Ashley Polymers Ashlene® 990L Nylon 610 A general purpose, medium viscosity grade for injection molding and extrusion.Data provided by the manufacturer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | Annealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion L6256 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C @Thickness 6.40 mm |
172 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL FN170X PPE+PS Foamable resin. All properties at 10% density reduction; 0.250"" thick test specimens. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | annealed; ASTM D648 |
Kleerdex Kydex® 120 Acrylic/PVC Thermoplastic Sheet
(discontinued **) USDA approved thermoplastic sheetApplications: High impact resistant wallcovering, push plates and kick plates, equipment housings, splash and safety guardsFeatures: Kydex 120 meets class I/A fire c.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | ASTM D648 |
Supreme Petrochem SP6409 High Gloss Polystyrene Characteristics High gloss in co-extrusion Improved dart impact strength of co-extruded sheets Processing Co-extrusion cap layer Applications Gloss cap layer for refrigerator liner and other formin.. |