Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 82.8 °C @Thickness 6.35 mm |
181 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne LubriOne™ 5209 FPL 20 Natural Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 82.8 °C @Thickness 6.35 mm |
181 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne LubriOne™ AT-000/20T Black Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 82.8 °C | 181 °F | 0.125 inch bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Network Polymers SBN 150 Styrene Butadiene Acrylonitrile Terpolymer Description: Styrene Butadiene Acrylonitrile TerpolymerInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 82.8 °C | 181 °F | Unannealed; ASTM D648 |
M. Holland Company GS410WC Polystyrene
(discontinued **) Features: High Clarity, High FlowUses: Household Goods, LabwareApprovals: FDA 21 CFR 177.1640 Processing Method: Injection MoldingInformation provided by M. Holland. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 82.8 °C | 181 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS 8015 CL Availability: North AmericaForms: PelletsFeatures: CopolymerAppearance: Clear/TransparentInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 82.8 °C @Thickness 3.20 mm |
181 °F @Thickness 0.126 in |
Unannealed; ASTM D648 |
Styron MAGNUMâ„¢ 3325 MT Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 3325 MT is a resin with excellent processing characteristics and matt surface finish. The mass (continuous process) ABS technology of Styron ensures an ABS resin that combines.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 82.8 °C | 181 °F | Unannealed; ASTM Data |
Styron Magnum™ 344CC ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 82.8 °C | 181 °F | Unannealed; ASTM D648 |
Styron XU 73120.00 Polycarbonate Resin Overview: XU 73120.00 Experimental Polycarbonate Resin is a high flow ignition resistant PC blend that contains no chlorinated or brominated additives. This resin is specifically designed to offer e.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 82.8 °C | 181 °F | Unannealed; ASTM Data |
Styron Magnum™ 344HP ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 82.8 °C | 181 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ABS 3003MC Black 1722 Description: BlackInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 82.8 °C | 181 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ABS 3500 Description: Natural, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 82.8 °C | 181 °F | 0.125 in bar Annealed 4 hours at 80°C; ASTM D648 |
Diamond Polymers ABS VP-12 Description: Flame Retardant with UVInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 82.8 °C | 181 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ASA S150 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 82.8 °C | 181 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ASA S510 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 82.8 °C | 181 °F | 0.125 in bar Annealed 4 hours at 80°C; ASTM D648 |
Diamond Polymers TR 5000 AS/P Description: Transparent ABS, Antistatic GradeInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 82.8 °C | 181 °F | ASTM D648 |
Americas Styrenics STYRON® 404 High Impact Polystyrene Product CharacteristicsAdditive FreeTypical ApplicationsCompounding and masterbatchesInformation provided by AmericasStyrenics LLC. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 82.8 °C | 181 °F | |
Aclo Accutech Polypropylene Copolymer HP0335W40L Wollastonite Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 82.8 °C | 181 °F | |
Aclo Accutech Polypropylene Homopolymer HP0339M40CL Mica Reinforced Coupled |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 82.8 °C | 181 °F | ASTM D648 |
Americas Styrenics STYRON® 498 High Impact Polystyrene Product CharacteristicsHigh glossHigh impactFood Contact CompliantUL Classification 94HBTypical ApplicationsAppliancesMedicalHousewaresConsumer electronicsInformation provided by AmericasStyrenics L.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 82.8 °C | 181 °F | Unannealed (0.250"); ASTM D648 |
LTL Color Compounds ColorFast® GPA300 ABS Super-tough ABS with our highest impact strength, injection moldingAll information provided by LTL Color Compounders, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 82.8 °C | 181 °F | Unannealed (0.250"); ASTM D648 |
LTL Color Compounds ColorFast® GPA300X ABS Extrusion grade, high impact, high gloss ABSAll information provided by LTL Color Compounders, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 82.8 °C | 181 °F | |
Aclo Accucomp ABS ABS801V Automotive Approved Grade |