Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | ASTM D648 |
Plaskolite Optix® CA-1000 IG Clear High Impact Acrylic Resin High impact acrylic resin, injection molding and extrusion gradeApplications: A premium impact acrylic resin particularly suited for medical and food uses. This resin offers the best impact resista.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | ASTM D648 |
Plaskolite West Optix® CA-1000 IG UC Clear High Impact Acrylic Resin High impact acrylic resin, injection molding and extrusion gradeApplications: A premium impact acrylic resin particularly suited for medical and food uses. This resin is suited for Gamma irradiatio.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | ASTM D648 |
Resirene Resirene® 6220 High Impact Polystyrene Features:Low FlowEasy ProcessingGood GlossHigh ElongationFDA Rating: 21 CFR 177.1640Mechanical StrengthApplications:Extrusion/ ThermoformingDisposablesGPPS/HIPS BlendsRefrigerator PartsInformation p.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Cycolac® EX58 ABS High impact ABS for sheet extrusion and blow molding applications. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | annealed; ASTM D648 |
Kleerdex Vinyloy™ 100 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Utility gradeApplications: Vinyloy 100 sheet is a fire retardant that can be used to substitute effectively for ABS and other utility grade thermoplastics.Features: Vinyloy 100 sheet is a recycled g.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | annealed; ASTM D648 |
Kleerdex Vinyloy™ 102 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Recycled capped FR sheetApplications: Vinyloy 102 sheet is capped sheet that can be used to substitute effectively for ABS and other grades of thermoplastic sheet for your thermoforming needs.Featur.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | ASTM D648 |
Albis Plastics Cellulose Acetate Propionate CP808 (FDA), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C @Thickness 6.40 mm |
172 °F @Thickness 0.252 in |
ASTM D648 |
Kingfa HIPS-5197 High Impact Polystyrene Features:UL 94 HB @ 1.6mmExcellent balance propertiesHigh mechanical strengthGood heat stabilityColor tailor-made for clientsApplications:Injection moldingGas assistant moldingTV & Audio housingElec.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | |
Ineos ABS Lustran® 1152 Key Features:UnfilledHigh impact or high impact modifiedSuitable processing methods:Sheet extrusionThermoforming |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP STAT-KON CD0001 PS LNP* STAT-KON* CD000I is a compound based on Polystyrene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Stat-loy A3000Z ABS LNP* Stat-loy* A3000Z is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for t.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics XYLEX X8300 PC+POLYESTER (Asia Pacific) PC+Polyester, UV Stabilized, Transparent |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | annealed; ASTM Test |
Styrolution Terlux® 2812 TR MABS Terlux 2812 TR is a transparent grade of MABS for injection molding with high flowability.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C @Thickness 6.40 mm |
172 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® EG-7000 ABS/PET, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | ASTM D648 |
Samyang Trimma® SD6320P PMMA, Translucent High scratch resistance; stability against weak acids, strong acids, weak alkalis and inorganic salts.Information provided by Samyang. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C @Thickness 3.20 mm |
172 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP TF006 PU LNP THERMOCOMP TF006 is a compound based on Polyurethane containing 30% Glass Fiber. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C @Thickness 3.20 mm |
172 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL N190X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. RTI Elec/Imp/Str 95/80/95. Dielectric strength. Suitable for E/E market applications. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | ASTM D648 |
Supreme Petrochem SC 208 General Purpose Polystyrene CharacteristicsHigh flow grade Easy processing Good clarity & shineProcessing Extrusion MoldingApplications Hand molding applications of novelty items, toys etc. Carrier for master batches, as a .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | ASTM D648 |
Supreme Petrochem SP 564 Flame Retardant Polystyrene Characteristics Very good flow properties Free of DBDPO, PBDE & TBBA, complies with ROHS directive of EU Processing MoldingApplications Large size T.V. Cabinets VCR cabinets Electrical boxes, ele.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | ASTM D648 |
Supreme Petrochem SP6415 High Gloss High Impact Polystyrene Characteristics Very good gloss with the retention of ESCR properties Good toughness Also available in various color shades Processing Injection moldingApplications Refrigerator end caps Refriger.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | Conditioned 4 hours @ 70°C (158°F); ASTM D648 |
Eastman Tenite Propionate 383A2R30009 Natural, Trsp Cellulose Acetate Propionate Plasticizer 9%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | ISO 75-1/-2 |
Covestro Bayblend® FR 3005 Polycarbonate + ABS, Flame Retardant Grade Injection molding gradeeasy-flow gradeVicat/B 120 temperature = 95 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantglow wire test (GWFI): 960 °C (2.0 mm)no j.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | 0.125";; ASTM D648 |
Diamond Polymers Centrex® 825 Sheet Extrusion Grade Centrex 825 resin is a high-gloss, high-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® FG133F1 NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66 with Developed for Food Contact Applications Zytel FG133F1 NC010 is a nucleated PA 66. It has been developed for consideration into applications such as parts for the food .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | unannealed; ISO 75 |
Chi Mei Polylac® PA-758R ABS - Transparent Transparent, Chemical Resistant |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | ASTM-D648 |
Braskem PCD 0440 HECO Polypropylene Heterophasic Copolymer PCD 0440 is a medium melt flow rate heterophasic copolymer with high impact strength. This resin is designed for steel pipe coating (SPC) and injection molding. Its applications include: automotive.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | ASTM D648 |
Ashley Polymers Ashlene® F242 ABS Flame retardant.Data provided by the manufacturer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | 0.25 inch; ASTM D648 |
PlastxWorld CEVIAN® A1700 PA/ABS Alloy, Conditioned Property data is for samples at equilibrium moisture (2.0%)Information provided by PlastxWorld Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | annealed; ASTM D648 |
Kleerdex Kydex® 550 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Weatherable monolithic sheetApplications: Housings for equipment, recreational vehicles and truck parts, safety equipment, building products, signageFeatures: Kydex 550 offers the properties of "Kyd.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Xenoy® X6320 PBT+PC X6320 is a mineral filled PBT/PC resin developed for automotive painted doorhandles. Key advantages are excellent surface finish, easy processing and paint quality.This data was supplied by SABIC-IP.. |