Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 66.0 °C | 151 °F | ASTM D648 |
NYCOA 534 H High Viscosity, Heat Stabilized Nylon 6 Resin NYCOA 534 H is a high viscosity; heat stabilized, nucleated Nylon 6 resin. The high viscosity and fast set-up time make an excellent material for extrusion of tubing, rods, sheet and film. Because o.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.0 °C | 151 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYabs SN0 ABS Information provided by Polykemi AB |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.0 °C | 151 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PP CIP15015 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.0 °C | 151 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Konduit MT00EL PP LNP* Konduit* MT00EL is a Polypropylene base resin with thermal fillers. Characteristics of this grade are Thermal Conductivity and it is Low Extraactible.This data was supplied by SABIC-IP for th.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.0 °C | 151 °F | |
Eastman Eastar DN101 PCTG Copolyester
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.0 °C | 151 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PP CIP6015F VTUV Polypropylene, Mineral Reinforced, Heat and UV Stabilized Information provided by Polykemi AB |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.0 °C | 151 °F | ASTM D648 |
Ineos Barex® 218 E Acrylonitrile-Methyl Acrylate Copolymer Extrusion Grade. Barex® Resins are available in either natural or blue tint. Barex® 218E is most commonly used for thermoformed sheet applications in which high impact performance is require.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.0 °C | 151 °F | ISO 75A |
Lucite International Elvakon® 4494 Low Gloss Acrylic Capstock Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable pr.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.0 °C | 151 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP LUBRICOMP RP003 PA 66 LNP* LUBRICOMP* RP003 is a compound based on Nylon 66 resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.0 °C @Thickness 3.20 mm |
151 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP RX01514 PA 66 LNP* LUBRICOMP* RX01514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.0 °C | 151 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP LUBRICOMP RX93237 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RX93237 is a compound based on Nylon 66 resin containing PTFE, Silicone, MOS2. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.0 °C | 151 °F | ASTM D 648 |
Shakespeare Isocorâ„¢ SVP6105 medium viscosity PA-610 Isocorâ„¢ 6105 is a medium viscosity PA-610. This resin is specifically suited for applications requiring low moisture absorption and greater dimensional stability. Isocorâ„¢ 6105 is also .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.0 °C @Thickness 3.20 mm |
151 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON KEP33 Acetal (Asia Pacific) LNP STAT-KON* KEP33 is a compound based on Acetal resin containing Silicone, Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.0 °C @Thickness 3.20 mm |
151 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-LOY 93000LTH Acrylic LNP* STAT-LOY* 93000LTH is a compound based on Acrylic resin. Added features of this material include: Antistatic, Transparent and Formulation Locked. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.0 °C @Thickness 3.20 mm |
151 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-LOY A3000TXB ABS LNP* STAT-LOY* A3000TXB is a compound based on ABS resin. Added features of this material include: Antistatic, Transparent, Formulated with FDA Food Contact Additives and Bioassessed to ISO 10993... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.0 °C | 151 °F | ASTM Test |
Styrolution Styrolux 3G33 SBC Styrolux 3G33 is a thermoplastic styrene-butadiene block copolymer which is suitable for injection molding, extrusion and thermoforming. It offers an outstanding combination of crystal clarity and .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.0 °C | 151 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1182 Talc Fortified Impact Resistant Polypropylene DescriptionPolyfort® FPP 1182 is a 20% talc fortified impact resistant polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.0 °C | 151 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1182 Talc Fortified Impact Resistant Polypropylene DescriptionPolyfort® FPP 1182 is a 20% talc fortified impact resistant polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.0 °C | 151 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1182 Talc Fortified Impact Resistant Polypropylene DescriptionPolyfort® FPP 1182 is a 20% talc fortified impact resistant polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.0 °C | 151 °F | ASTM D648 |
A. Schulman POLYFORT™ FXP 2600-3120 CaC02 Filled Homopolymer Polypropylene DescriptionPolyfort® FXP 2600-3120 is a 20% GAC02 filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.0 °C | 151 °F | ISO 75 |
Eastman DuraStar DS2000 Polymer, Natural Durastar DS2000 polymer has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. DS2000 has ver.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.0 °C | 151 °F | |
Eastman Eastar DN004 PCTG Copolyester ISO data as provided by the manufacturer, Eastman Chemical |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.0 °C | 151 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® FG408L NC010 Nylon 66
(Unverified Data**) Unreinforced Toughened Polyamide 66 with Developed for Food Contact Applications Zytel FG408L NC010 is a general purpose lubricated impact modified polyamide 66 resin with superior toughness for inj.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.0 °C | 151 °F | Flatw 80x10x4, sp=64 mm; ISO 75/Af |
Eurostar Starpylen MB006SU PP, Glass Bead Filled, Injection Molding Resin Starpylen MB006SU is a Glass Bead Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.0 °C | 151 °F | ASTM D648 |
Ashley Polymers Ashlene® 525 Nylon 66 High impact Nylon 66 with good stiffness for injection molding.Data provided by the manufacturer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.0 °C | 151 °F | ASTM Test |
BASF Styroclear GH 62 SBC Styroclear GH 62 is a high flow thermoplastic styrene-butadiene block copolymer with excellent mold release properties. It has crystal clarity, good toughness, good stiffness and warpage resistance.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.0 °C | 151 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PPH TS15030 D Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.0 °C | 151 °F | ASTM D648 |
Ashley Polymers Ashlene® R3137 BK PC/PBT A thermoplastic alloy offering a high level of chemical resistance combined with high impact and excellent mechanical properties. Black.Data provided by the manufacturer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.0 °C | 151 °F | ASTM D648 |
Chevron Phillips K-Resin® BK13 Styrene-Butadiene Copolymer, Injection Molding Grade
(discontinued **) Styrene-Butadiene CopolymerBK13 is an SBC developed specifically to have enhanced flow capabilities and improved stiffness over the KR01 grade. BK13 molded parts give excellent detail on rapid prod.. |