Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 960 °C @Thickness 2.00 mm |
1760 °F @Thickness 0.0787 in |
Flammability Index; IEC 60695-2-12 |
PolyOne OnFlex™ S HF 90A-3S1988 Thermoplastic Elastomer (TPE) OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu.. |
|||
Glow Wire Test | 960 °C @Thickness 3.20 mm |
1760 °F @Thickness 0.126 in |
Glow Wire Flammability Index; IEC 694-2-12 |
Nilit Nilamid A G5 FR PH1 25% Glass Fiber Reinforced, Flame Retardant PA66 Description: Nilamid A G5 FR PH1 combines flame retardancy with outstanding mechanical performance. This product has a complete yellow card, with RTI and CTI listings. The formulation has been optim.. |
|||
Glow Wire Test | 960 °C @Thickness 1.60 mm |
1760 °F @Thickness 0.0630 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® 920 PC (Europe-Africa-Middle East) LEXAN 920 is a low viscosity flame retardant grade, especially suitable for electrical applications. |
|||
Glow Wire Test | 960 °C @Thickness 1.00 mm |
1760 °F @Thickness 0.0394 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® 945ASR PC Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t.. |
|||
Glow Wire Test | 960 °C @Thickness 1.00 mm |
1760 °F @Thickness 0.0394 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® 955U PC Lexan* 955U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio.. |
|||
Glow Wire Test | 960 °C @Thickness 1.60 mm |
1760 °F @Thickness 0.0630 in |
Flammability Index; IEC 60695-2-12 |
PolyOne Bergamid™ A700 G20 HW UF Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Glow Wire Test | 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
IEC 60695-2-12 |
DuPont Performance Polymers Rynite® GW520CS NC010 PET
(Unverified Data**) Rynite® GW520CS NC010 is a 20% glass fiber reinforced, flame retardant, color stabilized, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
Glow Wire Test | 960 °C @Thickness 2.00 mm |
1760 °F @Thickness 0.0787 in |
IEC 695-2-1 |
LATI LASULF Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
Glow Wire Test | 960 °C @Thickness 1.50 mm |
1760 °F @Thickness 0.0591 in |
DAM; IEC 60695-2-12 |
DuPont Performance Polymers Zytel® 103FHS BKB038 Nylon 66
(Unverified Data**) Zytel® 103FHS BKB038 is a heat stabilized, lubricated, PA 66 resin for fast cycling.Information provided by DuPont Performance Polymers |
|||
Glow Wire Test | 960 °C @Thickness 1.00 mm |
1760 °F @Thickness 0.0394 in |
DAM; IEC 60695-2-12 |
DuPont Performance Polymers Zytel® FR70M30V0 BK010 Nylon 66
(Unverified Data**) Zytel® FR70M30V0 BK010 is a 30% mineral reinforced, flame retardant, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Glow Wire Test | 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
Mitsubishi Xantar® FC 22 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
Mitsubishi Xantar® G2F 23 UR Polycarbonate-10% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 960 °C @Thickness 0.750 mm |
1760 °F @Thickness 0.0295 in |
IEC 60695-2-12 |
Lanxess Durethan® AKV 15 FN 00 000000 Nylon 66, 12% Glass Fiber PA 66, 12% glass fiber, injection molding, halogen free flame retardantInformation provided by LANXESS. |
|||
Glow Wire Test | 960 °C @Diameter 3.00 mm |
1760 °F @Diameter 0.118 in |
GWFI; IEC 60695-2-12 |
Lanxess Durethan® B 30 S FN30 000000 Nylon 6, Flame Retardant PA 6, non-reinforced, injection molding, halogen free flame retardant, heat-aging resistanceInformation provided by LANXESS. |
|||
Glow Wire Test | 960 °C @Thickness 2.00 mm |
1760 °F @Thickness 0.0787 in |
GWFI/GWT |
LATI Kelon® B FR H2 CEG/500-V0CT3 PA 6, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion co.. |
|||
Glow Wire Test | 960 °C @Thickness 2.00 mm |
1760 °F @Thickness 0.0787 in |
GWFI/GWT |
LATI Latene® 7H2W-V0 PP Homopolymer, Heat Stabilized, Flame Retardant Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Low smoke density and low toxicity i.. |
|||
Glow Wire Test | 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
Mitsubishi Xantar® F 25 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
Mitsubishi Xantar® FC 23 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 960 °C @Thickness 1.00 mm |
1760 °F @Thickness 0.0394 in |
GWFI/GWT |
LATI Latamid 6 H2 G/20-V2HF PA 6, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Euro.. |
|||
Glow Wire Test | 960 °C @Thickness 1.00 mm |
1760 °F @Thickness 0.0394 in |
GWFI/GWT |
LATI Latamid 66 H2 G/25-V0KB PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |
|||
Glow Wire Test | 960 °C @Thickness 2.00 mm |
1760 °F @Thickness 0.0787 in |
GWFI/GWT |
LATI Latilon 30D G/10-V0 PC, 10% Glass Fiber Reinforced, Flame Retardant Polycarbonate (PC) based compound. Glass fibers. UL94 V-0 classified, brominated and chlorinated halogens-based flame retardants free. Low smoke density and low toxicity index. High dimensional stab.. |
|||
Glow Wire Test | 960 °C @Thickness 3.20 mm |
1760 °F @Thickness 0.126 in |
VDE 0471/P2-4, IEC 695 |
EPICHEM Epilon G2-PC 10% GF Polycarbonate, 10% Glass Fiber Characteristics: 10% glass fibre filled, good mechanical properties |
|||
Glow Wire Test | 960 °C @Thickness 3.20 mm |
1760 °F @Thickness 0.126 in |
VDE 0471/P2-4, IEC 695 |
EPICHEM Epiryl PPO V0 Polyphenylene oxide Characteristics: self-extinguishing V0 at 1,6 mm |
|||
Glow Wire Test | 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
BK, Glow-Wire Ignition; IEC 60695-2-12 |
Eurostar Starflam RF0097P PA66/6, 45% Glass Filled, Injection Molded Starflam RF0097P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1009Z270EM)Information provided by Polym.. |
|||
Glow Wire Test | 960 °C @Thickness 2.00 mm |
1760 °F @Thickness 0.0787 in |
GWFI; IEC 60695 |
Eurotec® Tecomid® NT40 GR30 NL XA60 PPA, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural Information provided by Eurotec® |
|||
Glow Wire Test | 960 °C @Thickness 2.00 mm |
1760 °F @Thickness 0.0787 in |
GWFI; IEC 60695 |
Eurotec® Tecopet® PT70 GR30 NL100 XD70 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), long-term heat stabilized, natural Information provided by Eurotec® |
|||
Glow Wire Test | 960 °C @Thickness 0.750 mm |
1760 °F @Thickness 0.0295 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® ECO315 BK13 Nylon 66, Flame Retardant, DAM Vydyne® ECO366 BK13 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for m.. |
|||
Glow Wire Test | 960 °C @Thickness 0.750 mm |
1760 °F @Thickness 0.0295 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® ECO366 Nylon 66, Flame-retardant, DAM Vydyne® ECO366 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for machin.. |
|||
Glow Wire Test | 960 °C @Thickness 1.50 mm |
1760 °F @Thickness 0.0591 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® ML6230 PC Copolymer (Asia Pacific) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colors.This data was supplied by SABIC-IP for the Asia Pacific region. |