Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
SABIC FI0644 Bimodal High Density Polyethylene for Blown Film Product Description: FI0644 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh.. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
SABIC FI0750 Bimodal High Density Polyethylene for Blown Film Product Description: FI0750 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh.. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
Polimeri Europa Greenflex® FF 45 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FF 45 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FF 45 show high toughness.Main Applications: Greenflex FF 45 is recommended for.. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
Polimeri Europa Greenflex® FL 25 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FL 25 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FL 25 show good optical properties and excellent sealability.Main Applications: .. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
Polimeri Europa Greenflex® HN 70 Ethylene Vinyl Acetate Copolymer - Compounding Greenflex HN 70 is an ethylene vinyl acetate copolymer (EVA) for compounding applications. Greenflex HN 70 is a medium fluidity grade with high tack.Main Applications: Greenflex HN 70 is recommend.. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
Polimeri Europa Greenflex® ML 21 Ethylene Vinyl Acetate Copolymer - Injection Molding Greenflex ML 21 is an ethylene vinyl acetate copolymer (EVA) for injection molding, when a good ESCR is required. Greenflex ML 21 contains additive waxes to obtain high production speed.Main Applic.. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
Polimeri Europa Greenflex® ML 31 Ethylene Vinyl Acetate Copolymer - Injection Molding & Profile Extrusion Greenflex ML 31 is an ethylene vinyl acetate copolymer (EVA) for injection molding applications and extrusion profile. Greenflex ML 31 contains additive waxes to obtain high production speed.Main A.. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
Polimeri Europa Greenflex® ML 50 Ethylene Vinyl Acetate Copolymer - Injection Molding, Compounding & Extrusion Greenflex ML 50 is an ethylene vinyl acetate copolymer (EVA) for injection molding, compounding and extrusion. Items produced with Greenflex ML 50 show high elasticity.Main Applications: Greenflex.. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
Polimeri Europa Greenflex® ML 60 Ethylene Vinyl Acetate Copolymer - Injection Molding, Compounding & Extrusion Greenflex ML 60 is an ethylene vinyl acetate copolymer (EVA) for injection molding, compounding and extrusion. Items produced with Greenflex ML 60 show very high elasticity.Main Applications: Gree.. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
Polimeri Europa Greenflex® MP 34 Ethylene Vinyl Acetate Copolymer - Injection Molding & Compounding Greenflex MP 34 is an ethylene vinyl acetate copolymer (EVA) for injection molding and compounding applications. Greenflex MP 34 combines high fluidity with high elasticity.Main Applications: Gree.. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
Polimeri Europa Greenflex® MP 35 Ethylene Vinyl Acetate Copolymer - Injection Molding & Extrusion Greenflex MP 35 is an ethylene vinyl acetate copolymer (EVA) for injection molding and extrusion. Greenflex MP 35 is an easy flowing material and provides a very high elasticity.Main Applications: .. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
Polimeri Europa Greenflex® MQ 40 Ethylene Vinyl Acetate Copolymer - Injection Molding & Compounding Greenflex MQ 40 is an ethylene vinyl acetate copolymer (EVA) for injection molding and compounding applications. Greenflex MQ 40 combines high fluidity and high elasticity.Main Applications: Green.. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
Polimeri Europa Greenflex® FD 23 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FD 23 is an ethylene vinyl acetate copolymer (EVA) suitable for blown film extrusion. Greenflex FD 23 is a version of Greenflex FD 20 with added slip and antiblocking agents. Films produ.. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
Polimeri Europa Greenflex® FD 53 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FD 53 is an ethylene vinyl acetate copolymer (EVA), containing antiblocking agent, for blown film extrusion. Films produced with Greenflex FD 53 exhibit good sealing properties, high flex.. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
Chevron Phillips Marlex® HMN 4550 High Density Polyethylene
(discontinued **) High Density PolyethyleneCustomer Benefits: This resin is a high density polyethylene copolymer with high stress crack resistance, outstanding impact strength, and good warpage resistance. It is us.. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
Chevron Phillips Marlex® HMN 55180 High Density Polyethylene
(discontinued **) High Density PolyethyleneCustomer Benefits: This resin is a narrow molecular weight distribution copolymer with easy processing characteristics and excellent toughness properties. This product disp.. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D 746 |
Total Finathene® 6450 HDPE film
(discontinued **) Applications: overwrap, food packaging, coextrusion, extrusion coatingInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lin.. |
|||
Brittleness Temperature | -80.0 °C | -112 °F | ASTM D746 |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with No Plasticizer MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Brittleness Temperature | -80.0 - -59.0 °C | -112 - -74.2 °F | Average value: -70.8 °C Grade Count:21 |
Overview of materials for High Density Polyethylene (HDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max.. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
LG Chemical LUTENE-H BE0400 HDPE Description: LUTENE - H BE0400 is an excellent materials for blow-molded articles with high density and rigidity. It has good flow characteristics and impact resistance.Applications: Blow molded con.. |
|||
Brittleness Temperature | >= -80.0 °C | >= -112 °F | ASTM D746-72 |
Iran Petrochemical (PCC) BL3 HF 4760 High Density Polyethylene BL3 is a high density polyethylene with 1-Butene as co monomer. It is high density and stiffness, good ESCR, high rigidity, good flowability and impact strength.Applications: small blow molding, bo.. |
|||
Brittleness Temperature | >= -80.0 °C | >= -112 °F | ASTM D746-72 |
Iran Petrochemical (PCC) EX 4 HM9455 F High Density Polyethylene EX4 is a high density polyethylene with 1-Butene as co monomer. It is high rigidity, low gel level, high drowdown, somewhat stiffer than EX 5.Applications: film extrusion, blending partner, refuse .. |
|||
Brittleness Temperature | >= -80.0 °C | >= -112 °F | ASTM D746-72 |
Iran Petrochemical (PCC) EX 6HT HM 9455 HT High Density Polyethylene EX 6HT is a high density polyethylene with 1-Butene as co monomer. It has good toughness, low gel level, good tear strength, high tenacity.Applications: film extrusion, blending partner, refuse ba.. |
|||
Brittleness Temperature | >= -80.0 °C | >= -112 °F | ASTM D746-72 |
Iran Petrochemical (PCC) EX 3 – 100S HM CRP 100 N High Density Polyethylene EX3-100S is a high density polyethylene with 1-Butene as co monomer. It is natural, outstanding ESCR, high impact strength, outstanding hydrostatic strength for PE 100 class.Applications: pipe extr.. |
|||
Brittleness Temperature | >= -80.0 °C | >= -112 °F | ASTM D746-72 |
Iran Petrochemical (PCC) EX 4HS HM 9455 F1 High Density Polyethylene EX 4HS is a high density polyethylene with 1-Butene as co monomer. It has high rigidity, low gel level, high drawdown, very high stiffness and good tenacity.Applications: film extrusion, blending .. |
|||
Brittleness Temperature | -80.0 °C | -112 °F | ASTM D746-79 |
Saint-Gobain Versilicâ„¢ SPX-50 High Strength Silicone Tubing Formulation Description: Versilicâ„¢ SPX-50: Peroxide-cured Versilicâ„¢ High-Strength Silicone Tubing is designed for use in applications where flexibility, resiliency and durability are required. Its s.. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
Teknor Apex Telcar® TL-8431 Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Electrical/Electronic Applications; Industrial Cable Jacketing;.. |
|||
Brittleness Temperature | -80.0 °C | -112 °F | ASTM D746 |
Total HDPE 6280 High Density Polyethylene, Injection Molding Resin Characteristics:Excellent stiffnessExcellent surface appearanceGood warp resistanceExcellent impact resistanceASTM D 1248 - Type III, Class A, Category 3FDA CompliantApplications:Dairy cratesPallets.. |
|||
Brittleness Temperature | -80.0 - -68.0 °C | -112 - -90.4 °F | Average value: -74.3 °C Grade Count:7 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Compounding Resin This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Compounding Resin". Each property range of values reported is m.. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
LyondellBasell Alathon® 9301 High Density Polyethylene ApplicationsALATHON 9301is a high density resin designed for sheet extrusion and thermoforming. It exhibits very low sag and high stiffness.Regulatory StatusALATHON 9301 meets the requirements of F.. |