Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Greenflex® ML 50 Ethylene Vinyl Acetate Copolymer - Injection Molding, Compounding & Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Greenflex ML 50 is an ethylene vinyl acetate copolymer (EVA) for injection molding, compounding and extrusion. Items produced with Greenflex ML 50 show high elasticity.Main Applications: Greenflex ML 50 is recommended for the production of foamed and crosslinked sheets for shoes, dolls, shock absorbers and gaskets.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.941 g/cc
0.941 g/cc
ISO 1183
Vinyl Acetate Content 19 %
19 %
Internal Method
Melt Flow 2.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 89
89
ISO 868/A
Hardness, Shore D 36
36
ISO 868/A
Tensile Strength, Yield 4.50 MPa
653 psi
ISO 527
Flexural Modulus 0.0400 GPa
5.80 ksi
ISO 178
Thermal Properties Metric English Comments
Melting Point 83.0 °C
181 °F
Internal Method
Vicat Softening Point 58.0 °C

@Load 1.00 kg
136 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -80.0 °C
<= -112 °F
ASTM D746